CN103846633A - 一种变速箱用的惰轮轴的锻造方法 - Google Patents
一种变速箱用的惰轮轴的锻造方法 Download PDFInfo
- Publication number
- CN103846633A CN103846633A CN201410047511.9A CN201410047511A CN103846633A CN 103846633 A CN103846633 A CN 103846633A CN 201410047511 A CN201410047511 A CN 201410047511A CN 103846633 A CN103846633 A CN 103846633A
- Authority
- CN
- China
- Prior art keywords
- temperature
- heating
- idler shaft
- forging
- jackshaft
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种变速箱用的惰轮轴的锻造方法,包括以下步骤:浇注圆柱形坯料步骤,圆柱形坯料中化学成分重量百分比为:C0.27-0.42%,Mn1.2-2.4%,Si0.5-1.2,Mg0.07-0.15%,Cr0.5-1.2%,W0.42-0.8%,Ti0.4-1.0%,Cu痕量~0.050%,P≤0.040%、S≤0.030%,余量为Fe及不可避免的夹杂质;浇注成型的坯体温度降至250℃,再加热至600-700℃,保温3-5小时,炉冷至200℃,保温4小时,再加热至550-600℃,保温2-4小时,以30℃/小时冷却至200℃,再以20℃/小时,冷却常温;本发明使其利于大批量的工业化的生产,并减少了锻造过程中出现夹污、充不满的现象,产品的力学性能进一步改善,节约了产品用料,提高了产品的模具寿命。
Description
技术领域
本发明涉及一种变速箱用的惰轮轴的锻造方法。
背景技术
惰轮轴是汽车上的关键零件,由于其形状的特殊性及其使用性能的重要性,因而增加了其锻造成型的困难,在料的分配及工艺的选择上都需要慎重考虑。为此,开发该类锻件的合理锻造方法也颇受国内外关注。
目前,国内的惰轮轴常规的工艺流程为:加热、预锻、终锻、精整。该方案的缺点为:需要大吨位压力机,能耗大、材料利用率低,造成锻件成本高。以该方案的工艺流程所产生的锻件容易出现夹污、充不满等,缺陷废品率达5%,而且原料利用率只有20-30%,由于飞边过大等原因,模具的寿命也只有在5000-6000件左右。
发明内容
本发明的目的是提供一种变速箱用的惰轮轴的锻造方法,使其利于大批量的工业化的生产,并减少了锻造过程中出现夹污、充不满的现象,产品的力学性能进一步改善,节约了产品用料,提高了产品的模具寿命。
本发明的技术方案如下:
一种变速箱用的惰轮轴的锻造方法,包括以下步骤:
a、浇注圆柱形坯料步骤
圆柱形坯料中化学成分重量百分比为:C 0.27-0.42%,Mn 1.2-2.4%,Si 0.5-1.2,Mg 0.07-0.15%, Cr 0.5-1.2%, W 0.42-0.8%,Ti 0.4-1.0%, Cu 痕量~0.050%,P≤0.040%、S≤0.030%,余量为Fe及不可避免的夹杂质;浇注成型的坯体温度降至250℃,再加热至600-700℃,保温3-5小时,炉冷至200℃,保温4小时,再加热至550-600℃,保温2-4小时,以30℃/小时冷却至200℃,再以20℃/小时,冷却常温;
b、锻造步骤
1、毛坯件放入中频加热炉加热,加热温度1120-1180℃,保持加热时间3.6min;再放入冲床进行镦粗,镦粗厚度40±1mm,将工件中的镦粗端进行压方,使得长60mm,宽40mm;
2、将压方后的工件放入摩压机中安装的成型模具上,利用成型模具热锻工件;温度900℃,压力400T;
c、热处理
将锻造成型的惰轮轴置于第一设定温度的淬火炉中,第一设定温度为850℃-900℃,保持淬火炉内温度对中间轴实施淬火,保温时间范围为2.5-3.5小时,将淬火加热后的中间轴出炉冷却至温度≤100℃;
将冷却后的惰轮轴置于第二设定温度的回火炉中,第二设定温度为500℃-600℃,保持回火炉内温度对中间轴实施回火,保温时间范围为3.0-4.0小时,将回火加热后的中间轴出炉冷却;
d、磷化处理,对惰轮轴进行表面高温磷化处理:在90-100℃的温度下进行,磷酸盐溶液的游离酸度于总酸度的比值为1∶7-9,处理时间为45-50分钟。
本发明使其利于大批量的工业化的生产,并减少了锻造过程中出现夹污、充不满的现象,产品的力学性能进一步改善,节约了产品用料,提高了产品的模具寿命。
本发明的力学性能检测数据如下:
抗拉强度 σb (MPa):≥1045
屈服强度 σs (MPa):≥930
伸长率 δ5 (%):≥12
断面收缩率 ψ (%):≥54
冲击功 Akv (J):≥65
冲击韧性值 αkv (J/cm2):≥75
硬度 :≤223HB。
具体实施方式
一种变速箱用的惰轮轴的锻造方法,包括以下步骤:
a、浇注圆柱形坯料步骤
圆柱形坯料中化学成分重量百分比为:C 0.27-0.42%,Mn 1.2-2.4%,Si 0.5-1.2,Mg 0.07-0.15%, Cr 0.5-1.2%, W 0.42-0.8%,Ti 0.4-1.0%, Cu 痕量~0.050%,P≤0.040%、S≤0.030%,余量为Fe及不可避免的夹杂质;浇注成型的坯体温度降至250℃,再加热至600-700℃,保温3-5小时,炉冷至200℃,保温4小时,再加热至550-600℃,保温2-4小时,以30℃/小时冷却至200℃,再以20℃/小时,冷却常温;
b、锻造步骤
3、毛坯件放入中频加热炉加热,加热温度1120-1180℃,保持加热时间3.6min;再放入冲床进行镦粗,镦粗厚度40±1mm,将工件中的镦粗端进行压方,使得长60mm,宽40mm;
4、将压方后的工件放入摩压机中安装的成型模具上,利用成型模具热锻工件;温度900℃,压力400T;
c、热处理
将锻造成型的惰轮轴置于第一设定温度的淬火炉中,第一设定温度为850℃-900℃,保持淬火炉内温度对中间轴实施淬火,保温时间范围为2.5-3.5小时,将淬火加热后的中间轴出炉冷却至温度≤100℃;
将冷却后的惰轮轴置于第二设定温度的回火炉中,第二设定温度为500℃-600℃,保持回火炉内温度对中间轴实施回火,保温时间范围为3.0-4.0小时,将回火加热后的中间轴出炉冷却;
d、磷化处理,对惰轮轴进行表面高温磷化处理:在90-100℃的温度下进行,磷酸盐溶液的游离酸度于总酸度的比值为1∶7-9,处理时间为45-50分钟。
Claims (1)
1.一种变速箱用的惰轮轴的锻造方法,其特征在于,包括以下步骤:
a、浇注圆柱形坯料步骤
圆柱形坯料中化学成分重量百分比为:C 0.27-0.42%,Mn 1.2-2.4%,Si 0.5-1.2,Mg 0.07-0.15%, Cr 0.5-1.2%, W 0.42-0.8%,Ti 0.4-1.0%, Cu 痕量~0.050%,P≤0.040%、S≤0.030%,余量为Fe及不可避免的夹杂质;浇注成型的坯体温度降至250℃,再加热至600-700℃,保温3-5小时,炉冷至200℃,保温4小时,再加热至550-600℃,保温2-4小时,以30℃/小时冷却至200℃,再以20℃/小时,冷却常温;
b、锻造步骤
毛坯件放入中频加热炉加热,加热温度1120-1180℃,保持加热时间3.6min;再放入冲床进行镦粗,镦粗厚度40±1mm,将工件中的镦粗端进行压方,使得长60mm,宽40mm;
将压方后的工件放入摩压机中安装的成型模具上,利用成型模具热锻工件;温度900℃,压力400T;
c、热处理
将锻造成型的惰轮轴置于第一设定温度的淬火炉中,第一设定温度为850℃-900℃,保持淬火炉内温度对中间轴实施淬火,保温时间范围为2.5-3.5小时,将淬火加热后的中间轴出炉冷却至温度≤100℃;
将冷却后的惰轮轴置于第二设定温度的回火炉中,第二设定温度为500℃-600℃,保持回火炉内温度对中间轴实施回火,保温时间范围为3.0-4.0小时,将回火加热后的中间轴出炉冷却;
d、磷化处理,对惰轮轴进行表面高温磷化处理:在90-100℃的温度下进行,磷酸盐溶液的游离酸度于总酸度的比值为1∶7-9,处理时间为45-50分钟。