JPS5635372A - Preparation of thermal battery - Google Patents
Preparation of thermal batteryInfo
- Publication number
- JPS5635372A JPS5635372A JP11092379A JP11092379A JPS5635372A JP S5635372 A JPS5635372 A JP S5635372A JP 11092379 A JP11092379 A JP 11092379A JP 11092379 A JP11092379 A JP 11092379A JP S5635372 A JPS5635372 A JP S5635372A
- Authority
- JP
- Japan
- Prior art keywords
- electrolyte
- powder
- mixture
- heat
- desired size
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE:To obtain a battery with reduced scattering of the performance and high reliability by press molding a mixture of electrolyte holding material powder and electrolyte powder, heat-treating, crushing to a desired size, and remolding it to form an electrolyte layer. CONSTITUTION:In a ball mill, 35wt% of an electrolyte holding material powder comprising an inorganic adsorbent such as kaolin or alumina and 65wt% of LiCl- KCl electrolyte powder are mixed homogeneously. The mixture is prepress molded, heat-treated, for example, at 700 deg.C for 20min, ground into prticles of a desired size suitable for the next process, and then the powder is remolded to form an electrolyte layer 3. Another way, in which a positive active material powder and an electrolyte powder are mixed homogeneously, the mixture is premolded, heat- treated, ground into particles with desired size, and remolded, may be used to form a positive active material layer 4. Thus a battery with reduced scattering of the performance and high reliability can be obtained.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11092379A JPS5635372A (en) | 1979-08-29 | 1979-08-29 | Preparation of thermal battery |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP11092379A JPS5635372A (en) | 1979-08-29 | 1979-08-29 | Preparation of thermal battery |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5635372A true JPS5635372A (en) | 1981-04-08 |
JPS6122424B2 JPS6122424B2 (en) | 1986-05-31 |
Family
ID=14548043
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP11092379A Granted JPS5635372A (en) | 1979-08-29 | 1979-08-29 | Preparation of thermal battery |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5635372A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2005347028A (en) * | 2004-06-01 | 2005-12-15 | Matsushita Electric Ind Co Ltd | Thermal battery |
JP2008141160A (en) * | 2006-11-10 | 2008-06-19 | Doshisha | Thermally initiated molten salt capacitor |
CN109011696A (en) * | 2018-07-25 | 2018-12-18 | 中国科学院上海应用物理研究所 | The purification method of insoluble impurities in a kind of fused salt |
-
1979
- 1979-08-29 JP JP11092379A patent/JPS5635372A/en active Granted
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2005347028A (en) * | 2004-06-01 | 2005-12-15 | Matsushita Electric Ind Co Ltd | Thermal battery |
JP2008141160A (en) * | 2006-11-10 | 2008-06-19 | Doshisha | Thermally initiated molten salt capacitor |
CN109011696A (en) * | 2018-07-25 | 2018-12-18 | 中国科学院上海应用物理研究所 | The purification method of insoluble impurities in a kind of fused salt |
Also Published As
Publication number | Publication date |
---|---|
JPS6122424B2 (en) | 1986-05-31 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
IL56252A0 (en) | Pressure-ressistant polyurethane-polyurea particles for the encapsulation of active ingredients and process for their manufacture | |
JPS566376A (en) | Enclosed cell | |
JPS5635372A (en) | Preparation of thermal battery | |
GB1061817A (en) | Improvements in or relating to abrasive tumbling media | |
JPS5527673A (en) | Piezoelectric ceramics | |
JPS53145099A (en) | Preparing piezo-electric rubber | |
JPS5295598A (en) | Production of sepiolite moldings | |
JPS6489486A (en) | Manufacture of porous piezo-electric ceramic material | |
JPS56130082A (en) | Organic solvent battery | |
JPS57111956A (en) | Silver-oxide secondary battery | |
JPS55137669A (en) | Nonaqueous electrolyte battery | |
JPS5744697A (en) | Preparation of carbonaceous material | |
GB937435A (en) | Improvements relating to carbon electrodes for electrolytic aluminium furnaces and to electrode paste for producing such electrodes | |
JPS5595272A (en) | Granulation method of lead powder for clad type plate | |
JPS5588273A (en) | Method for preparing air electrode of cell | |
JPS55146880A (en) | Production method for positive pole mix of organic electrolyte battery | |
SU487667A1 (en) | Method for producing high molecular weight polyoxyethylene powder | |
JP2874783B2 (en) | Method for producing glass powder | |
JPS54139098A (en) | Porcelain composite of high dielectric constant system | |
JPS56106376A (en) | Manufacture of matrix for fuel cell | |
JPS5761258A (en) | Nonaqueous-electrolyte battery | |
JPS5556883A (en) | Electrode for calcium ion water producer | |
Kamagai et al. | Ceramic Sintered Body | |
JPH0479170A (en) | Lithium cell | |
DE4142072A1 (en) | METHOD FOR PRODUCING ACTIVE DIMENSION FROM ACTIVE DIMENSION ISOLATED FROM WASTE LEAD ACCUMULATORS |