Nothing Special   »   [go: up one dir, main page]

CN101920292A - Riveting method - Google Patents

Riveting method Download PDF

Info

Publication number
CN101920292A
CN101920292A CN201010158395XA CN201010158395A CN101920292A CN 101920292 A CN101920292 A CN 101920292A CN 201010158395X A CN201010158395X A CN 201010158395XA CN 201010158395 A CN201010158395 A CN 201010158395A CN 101920292 A CN101920292 A CN 101920292A
Authority
CN
China
Prior art keywords
riveted
boss
riveting
hardwares
metal elements
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201010158395XA
Other languages
Chinese (zh)
Inventor
李殷德
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201010158395XA priority Critical patent/CN101920292A/en
Publication of CN101920292A publication Critical patent/CN101920292A/en
Pending legal-status Critical Current

Abstract

The invention relates to a riveting method comprising the following steps of: firstly preprocessing two metal elements to be riveted by utilizing the traditional mechanical processing method for punching or lathe processing to form gaps at the riveting points of the two metal elements to be riveted; and then pressing the riveting points of the two metal elements to be riveted by utilizing combined type punch riveting to make the two metal elements extrude with each other and fill the gaps, thereby forming firm connection. Based on the adoption of a two-step method combining the traditional mechanical processing method for preprocessing and cavity angle-expanded filling, in the riveting method, certain shape preprocessing is firstly carried out to the metal elements to be riveted with each other by adopting the traditional mechanical processing mode for punching or lathe processing to form convenient riveting points, and then the two metal elements which have cavities before combination are punched by adopting combined type punch riveting to extrude with each other and fill the cavities for forming a partially filling-in or fully filling-in inversed hanging lock structure, thereby achieving the purpose of firm riveting.

Description

A kind of clinching method
Technical field
The invention belongs to the Machining Technology field, be specifically related to the clinching method between the hardware of tool definite shape.
Background technology
For the permanent riveting process of metal that need satisfy outward appearance and fixing requirement simultaneously, always there is very high difficulty.Existing traditional handicraft adopts the riveting of rising of means of spot welds or straight shape, and not only complex technical process, production efficiency are low, and firm weak effect, electroplates riveted joint position, back appearance poor.
Summary of the invention
The objective of the invention is at the deficiencies in the prior art, a kind of firm and reliable connection, production efficiency height are provided, can effectively cut down the consumption of energy and the rise clinching method at angle of hole economical with materials, that be particularly suitable for loudspeaker rear plate manufacturing in the electron trade.
The objective of the invention is to be achieved through the following technical solutions:
A kind of clinching method is characterized in may further comprise the steps:
Utilize traditional machining process of punching press or machined into that two hardwares to be riveted are carried out preliminary treatment earlier, riveting point at two hardwares to be riveted forms the space, at this moment, described preliminary treatment is to adopt the method for car system to make boss and make subtended angle in the both sides of boss in riveting point, metal cartridge to be riveted bottom to form the upside down funnel shape boss with subtended angle and get out through hole therebetween, on metal base plate to be riveted, utilize again the cooperation of upper die and lower die stamp out up-small and down-big have subtended angle and with the corresponding flared hole of upside down funnel shape boss of metal cartridge bottom; Exert pressure and make the extruding and fill the space and form firm connection mutually of two hardwares in the riveting point that is riveted on two hardwares to be riveted by combined pressing again, this moment exerts pressure and makes the extruding and fill the space to form firm connection be to utilize the cooperation of the boss of metal cartridge and metal base plate and flared hole both to be combined and put into mould to carry out knockdown punching press riveted joint mutually of two hardwares in the described riveting point that is riveted on two hardwares to be riveted by combined pressing, this moment, the boss of metal cartridge produced crimp because of pressurized, deformation direction is the center line that deviates from boss, this boss is subjected to the obstruction of metal base plate when crimp simultaneously, forces its deflection to be filled in the space between the boss of metal base plate flared hole and metal cartridge and the reversal of the natural order of things locking structure that the formation gap is filled up or all filled up.
The present invention fills the clinching method of the two step method that combines owing to adopt traditional machining process to carry out preliminary treatment and the hole angle of rising, earlier the hardware that will rivet is mutually carried out the preliminary treatment of definite shape by the machining mode of utilizing traditional punching press or machined into, form behind the riveting point easily again and to make two hardwares that have the hole before the combination be subjected to punching press to influence mutual extrusion packing hole by the combined pressing riveted joint to form the reversal of the natural order of things locking structure that part is filled up or all filled up, reach the purpose of firm riveted joint.And processing and making process is simple, and whole process can realize automatic continuous production, the production efficiency height, and can effectively cut down the consumption of energy and economical with materials, directly reduced manufacturing cost, be particularly suitable for the making of loudspeaker rear plate in the electron trade.
Describe work implementation procedure of the present invention in detail below in conjunction with accompanying drawing.
Description of drawings
Fig. 1 is the realization flow figure of embodiment of the present invention.
The specific embodiment
As shown in Figure 1, clinching method of the present invention may further comprise the steps: utilize traditional machining process of punching press or machined into that two hardwares to be riveted are carried out preliminary treatment earlier, form space 3 in the riveting point of two hardwares to be riveted, exert pressure and make the extruding and fill space 3 and form firmly and connect mutually of two hardwares in the riveting point that is riveted on two hardwares to be riveted by combined pressing again.Wherein according to the shape of hardware to be riveted and preliminary treatment that characteristic is carried out and the appearance performance requirement after the combination punching press riveted joint, the present invention includes but be not limited to following this embodiment, as shown in Figure 1, above-mentioned clinching method can be may further comprise the steps: adopt the method for car system or forge hot or cold forging to make boss 15 and make subtended angle in the both sides of boss 15 in 1 riveting point, metal cartridge bottom to be riveted earlier to form the upside down funnel shape boss 15 with subtended angle and get out through hole 16 therebetween, on metal base plate to be riveted 2, utilize again the cooperation of patrix 51 and counterdie 52 stamp out up-small and down-big have subtended angle and with the upside down funnel shape boss 15 corresponding flared hole 25 of metal cartridge 1 bottom, utilize the cooperation of the boss 15 of metal cartridge 1 and metal base plate 2 and flared hole 25 both to be combined and put into mould then and carry out knockdown punching press riveted joint, this moment, the boss 15 of metal cartridge 1 produced crimp because of pressurized, deformation direction is the center line that deviates from boss 15, this boss 15 is subjected to the obstruction of metal base plate 2 when crimp simultaneously, forces its deflection to be filled in the space 3 between the boss 15 of metal base plate 2 flared hole 25 and metal cartridge 1 and the reversal of the natural order of things locking structure that formation space 3 parts are filled up or all filled up.

Claims (1)

1. clinching method, it is characterized in that described clinching method may further comprise the steps: utilize traditional machining process of punching press or machined into that two hardwares to be riveted are carried out preliminary treatment earlier, riveting point at two hardwares to be riveted forms space (3), at this moment, described preliminary treatment is to adopt the method for car system to make boss (15) in riveting point, metal cartridge to be riveted (1) bottom and make subtended angle in the both sides of boss (15) to form the upside down funnel shape boss (15) with subtended angle and get out through hole (16) therebetween, utilizes the cooperation of patrix (51) and counterdie (52) to stamp out up-small and down-big have a subtended angle and the corresponding flared hole of upside down funnel shape boss (15) (25) bottom metal cartridge (1) again on metal base plate to be riveted (2); Exert pressure and make the extruding and fill space (3) and form firmly and connect mutually of two hardwares in the riveting point that is riveted on two hardwares to be riveted by combined pressing again, this moment exerts pressure and makes the extruding and fill space (3) and form that firmly to connect be to utilize the cooperation of the boss (15) of metal cartridge (1) and metal base plate (2) and flared hole (25) both to be combined and put into mould to carry out knockdown punching press and rivet mutually of two hardwares in the described riveting point that is riveted on two hardwares to be riveted by combined pressing, the boss (15) of metal cartridge this moment (1) produces crimp because of pressurized, the center line of deformation direction for deviating from boss (15), this boss (15) is subjected to the obstruction of metal base plate (2) when crimp simultaneously, forces its deflection to be filled in the space (3) between the boss (15) of metal base plate (2) flared hole (25) and metal cartridge (1) and forms the reversal of the natural order of things locking structure that space (3) is partly filled up or all filled up.
CN201010158395XA 2008-12-11 2008-12-11 Riveting method Pending CN101920292A (en)