Prior art keywords
riveted
boss
hardwares
riveting
tubaeform
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010101583733A
Other languages
Chinese (zh)
Inventor
李殷德
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010101583733A priority Critical patent/CN101875086A/en
Publication of CN101875086A publication Critical patent/CN101875086A/en
Pending legal-status Critical Current

Links

Landscapes

  • Insertion Pins And Rivets (AREA)

Abstract

The invention relates to a riveting method. The riveting method comprises the following steps of: preprocessing two metal elements to be riveted by the conventional machining method such as stamping or lathe machining; forming a gap at the riveted point of the two metal elements to be riveted; and then applying pressure at the riveted point of the two metal elements to be riveted by combined stamping and riveting to make the two metal elements extrude each other and filling the gap to form a firm connection. Due to the riveting method, which is a two-step method combining preprocessing by adopting the conventional machining method and cavity angle-expanding filling, the metal elements to be mutually riveted are preprocessed in a certain shape by utilizing the conventional machining method such as stamping or lathe machining to form a convenient riveting point; the two metal elements with the cavity before combination are stamped to extrude each other and fill the cavity to form a partially filled or fully filled inverted locking structure by adopting the combined stamping and riveting; and therefore, the aim of firm riveting is fulfilled.

Description

A kind of clinching method
Technical field
The invention belongs to the Machining Technology field, be specifically related to the clinching method between the hardware of tool definite shape.
Background technology
For the permanent riveting process of metal that need satisfy outward appearance and fixing requirement simultaneously, always there is very high difficulty.Existing traditional handicraft adopts the riveting of rising of means of spot welds or straight shape, and not only complex technical process, production efficiency are low, and firm weak effect, electroplates riveted joint position, back appearance poor.
Summary of the invention
The objective of the invention is at the deficiencies in the prior art, a kind of firm and reliable connection, production efficiency height are provided, can effectively cut down the consumption of energy and the rise clinching method at angle of hole economical with materials, that be particularly suitable for loudspeaker rear plate manufacturing in the electron trade.
The objective of the invention is to be achieved through the following technical solutions:
A kind of clinching method is characterized in may further comprise the steps:
Utilize traditional machining process of punching press or machined into that two hardwares to be riveted are carried out preliminary treatment earlier, riveting point at two hardwares to be riveted forms the space, at this moment, described preliminary treatment is to adopt the method for car system or forge hot or cold forging to make boss in riveting point, metal cartridge to be riveted bottom, on metal base plate to be riveted, utilize again the cooperation of upper die and lower die stamp out up-small and down-big have subtended angle and with the corresponding tubaeform blind hole of metal cartridge bottom boss; Exert pressure and make the extruding and fill the space and form firm connection mutually of two hardwares in the riveting point that is riveted on two hardwares to be riveted by combined pressing again, this moment exerts pressure and makes the extruding and fill the space to form firm connection be to utilize the cooperation of the boss of metal cartridge and metal base plate and tubaeform blind hole both to be combined and put into mould to carry out knockdown punching press riveted joint mutually of two hardwares in the described riveting point that is riveted on two hardwares to be riveted by combined pressing, this moment, the boss of metal cartridge produced crimp because of pressurized, deformation direction is the center line that deviates from tubaeform blind hole, this boss is subjected to the obstruction of metal base plate when crimp simultaneously, forces its deflection to be filled in the space between the boss of the tubaeform blind hole of metal base plate and metal cartridge and the reversal of the natural order of things locking structure that the formation gap is filled up or all filled up.
The present invention fills the clinching method of the two step method that combines owing to adopt traditional machining process to carry out preliminary treatment and the hole angle of rising, earlier the hardware that will rivet is mutually carried out the preliminary treatment of definite shape by the machining mode of utilizing traditional punching press or machined into, form behind the riveting point easily again and to make two hardwares that have the hole before the combination be subjected to punching press to influence mutual extrusion packing hole by the combined pressing riveted joint to form the reversal of the natural order of things locking structure that part is filled up or all filled up, reach the purpose of firm riveted joint.And processing and making process is simple, and whole process can realize automatic continuous production, the production efficiency height, and can effectively cut down the consumption of energy and economical with materials, directly reduced manufacturing cost, be particularly suitable for the making of loudspeaker rear plate in the electron trade.
Describe work implementation procedure of the present invention in detail below in conjunction with accompanying drawing.
Description of drawings
Fig. 1 is the realization flow figure of embodiment of the present invention.
The specific embodiment
As shown in Figure 1, clinching method of the present invention may further comprise the steps: utilize traditional machining process of punching press or machined into that two hardwares to be riveted are carried out preliminary treatment earlier, form space 3 in the riveting point of two hardwares to be riveted, exert pressure and make the extruding and fill space 3 and form firmly and connect mutually of two hardwares in the riveting point that is riveted on two hardwares to be riveted by combined pressing again.Wherein according to the shape of hardware to be riveted and preliminary treatment that characteristic is carried out and the appearance performance requirement after the combination punching press riveted joint, the present invention includes but be not limited to following this embodiment, as shown in Figure 1, above-mentioned clinching method can be may further comprise the steps: adopt the method for car system or forge hot or cold forging to make boss 17 earlier in riveting point, metal cartridge to be riveted 1 bottom, on metal base plate to be riveted 2, utilize again the cooperation of patrix 51 and counterdie 52 stamp out up-small and down-big have subtended angle and with metal cartridge 1 bottom boss 17 corresponding tubaeform blind holes 26, utilize the cooperation of the boss 17 of metal cartridge 1 and metal base plate 2 and tubaeform blind hole 26 both to be combined and put into mould then and carry out knockdown punching press riveted joint, this moment, the boss 17 of metal cartridge produced crimp because of pressurized, deformation direction is the center line that deviates from tubaeform blind hole 26, this boss 17 is subjected to the obstruction of metal base plate 2 when crimp simultaneously, forces its deflection to be filled in the space 3 between the boss 17 of metal base plate 2 tubaeform blind holes 26 and metal cartridge 1 and the reversal of the natural order of things locking structure that formation space 3 parts are filled up or all filled up.

Claims (1)

1. clinching method, it is characterized in that described clinching method may further comprise the steps: utilize traditional machining process of punching press or machined into that two hardwares to be riveted are carried out preliminary treatment earlier, riveting point at two hardwares to be riveted forms space (3), at this moment, described preliminary treatment is to adopt the method for car system or forge hot or cold forging to make boss (17) in riveting point, metal cartridge to be riveted (1) bottom, on metal base plate to be riveted (2), utilize again the cooperation of patrix (51) and counterdie (52) stamp out up-small and down-big have subtended angle and bottom metal cartridge (1) boss (17) corresponding tubaeform blind holes (26); Exert pressure and make the extruding and fill space (3) and form firmly and connect mutually of two hardwares in the riveting point that is riveted on two hardwares to be riveted by combined pressing again, this moment exerts pressure and makes the extruding and fill space (3) and form that firmly to connect be to utilize the cooperation of the boss (17) of metal cartridge (1) and metal base plate (2) and tubaeform blind hole (26) both to be combined and put into mould to carry out knockdown punching press and rivet mutually of two hardwares in the described riveting point that is riveted on two hardwares to be riveted by combined pressing, the boss (17) of metal cartridge this moment (1) produces crimp because of pressurized, the center line of deformation direction for deviating from tubaeform blind hole (26), this boss (17) is subjected to the obstruction of metal base plate (2) when crimp simultaneously, forces its deflection to be filled in the space (3) between the boss (17) of tubaeform blind hole of metal base plate (2) (26) and metal cartridge (1) and forms the reversal of the natural order of things locking structure that space (3) is partly filled up or all filled up.
CN2010101583733A 2008-12-11 2008-12-11 Riveting method Pending CN101875086A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2010101583733A CN101875086A (en) 2008-12-11 2008-12-11 Riveting method

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2010101583733A CN101875086A (en) 2008-12-11 2008-12-11 Riveting method

Related Parent Applications (1)

Application Number Title Priority Date Filing Date
CN2008102198469A Division CN101433934B (en) 2008-12-11 2008-12-11 Riveting method

Publications (1)

Publication Number Publication Date
CN101875086A true CN101875086A (en) 2010-11-03

Family

ID=43017828

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2010101583733A Pending CN101875086A (en) 2008-12-11 2008-12-11 Riveting method

Country Status (1)

Country Link
CN (1) CN101875086A (en)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102829449A (en) * 2012-08-17 2012-12-19 深圳市华星光电技术有限公司 Back plate component and liquid crystal display
CN103573767A (en) * 2013-09-27 2014-02-12 王福慧 Connection plate riveting structure and method thereof
CN103928815A (en) * 2014-04-28 2014-07-16 佛山市新基德电子厂有限公司 Cold stamping connection method of two electric conductors
CN104635889A (en) * 2013-11-15 2015-05-20 升业科技股份有限公司 Method for manufacturing heat dissipating base plate
CN108309544A (en) * 2018-03-05 2018-07-24 辽宁爱母医疗科技有限公司 A kind of intrauterine device holder

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102829449A (en) * 2012-08-17 2012-12-19 深圳市华星光电技术有限公司 Back plate component and liquid crystal display
CN103573767A (en) * 2013-09-27 2014-02-12 王福慧 Connection plate riveting structure and method thereof
CN104635889A (en) * 2013-11-15 2015-05-20 升业科技股份有限公司 Method for manufacturing heat dissipating base plate
CN104635889B (en) * 2013-11-15 2018-01-19 升业科技股份有限公司 The manufacture method of radiating bottom plate
CN103928815A (en) * 2014-04-28 2014-07-16 佛山市新基德电子厂有限公司 Cold stamping connection method of two electric conductors
CN108309544A (en) * 2018-03-05 2018-07-24 辽宁爱母医疗科技有限公司 A kind of intrauterine device holder

Similar Documents

Publication Publication Date Title
CN101433934B (en) Riveting method
CN101214526B (en) 7A04 aluminum alloy casing body parts multi-functional die forging technique and mold
CN105728575B (en) The flat no riveting plastic joining technique of the compound multiple degrees of freedom of double punches of aluminium alloy sheet
CN102784841B (en) Combined type precision sheet metal stamping and riveting mould
CN101875086A (en) Riveting method
CN109433988B (en) Continuous stamping and forging forming process and die for conical counter bore
CN102921802A (en) Method for forming car rear shaft support assembly cross beam
CN201693114U (en) Oil cylinder support forging finishing forming mould
CN202290949U (en) Mould for forming and processing end head of pipe fitting of carriage of motorcycle
CN101341634A (en) Clamp body for electrical connector clamps
CN101920292A (en) Riveting method
CN107433312B (en) High-pressure common rail pipe blank making mold and blank making method
CN101829735B (en) Riveting method
CN101829734B (en) Riveting method
CN202367058U (en) Main structure shape bending die for miniature motor junction box
CN202037252U (en) Steel pipe forming mould
CN102172767B (en) Large roller or gear forge piece forming device and using method
CN214556813U (en) Riveting die without rivet
CN110421110A (en) Fluting axle nut one-step moulding method
CN105414437A (en) Plate connecting method capable of using prepressing holes of soft rivet column and riveting compounding
CN202239183U (en) Motorcycle frame pipe fitting end head forming and preprocessing die
CN202861291U (en) T-shaped blank forging processing device
CN101992257B (en) Method for forging cup part with flange in outside diameter center
CN205217772U (en) Punching a hole of braking oil pipe support baffle, impression mould
CN201473164U (en) Connection structure of step tripod and main axle seat

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C12 Rejection of a patent application after its publication
RJ01 Rejection of invention patent application after publication

Open date: 20101103