Okamoto et al., 2013 - Google Patents
Compression deformability of Γ and ζ Fe–Zn intermetallics to mitigate detachment of brittle intermetallic coating of galvannealed steelsOkamoto et al., 2013
View PDF- Document ID
- 12058059731383692199
- Author
- Okamoto N
- Kashioka D
- Inomoto M
- Inui H
- Takebayashi H
- Yamaguchi S
- Publication year
- Publication venue
- Scripta Materialia
External Links
Snippet
Micropillar compression tests on each of the five intermetallic phases of the Fe–Zn system, which constitute the coating of galvannealed steels, have revealed that the Γ phase formed in direct contact with the steel substrate and the ζ phase formed on the outermost surface are …
- 229910000831 Steel 0 title abstract description 29
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/04—Ferrous alloys, e.g. steel alloys containing manganese
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
- C22C38/18—Ferrous alloys, e.g. steel alloys containing chromium
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Okamoto et al. | Compression deformability of Γ and ζ Fe–Zn intermetallics to mitigate detachment of brittle intermetallic coating of galvannealed steels | |
Yang et al. | Tensile deformation of low density duplex Fe–Mn–Al–C steel | |
Inoue et al. | Fracture elongation of brittle/ductile multilayered steel composites with a strong interface | |
Fan et al. | The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel | |
Chu et al. | Bendable bulk metallic glass: Effects of a thin, adhesive, strong, and ductile coating | |
Lee et al. | Liquid-metal-induced embrittlement of Zn-coated hot stamping steel | |
Kaijalainen et al. | Effect of austenite grain structure on the strength and toughness of direct-quenched martensite | |
Zheng et al. | Plastic instability mechanisms in bimetallic nanolayered composites | |
Reumont et al. | The effects of an Fe–Zn intermetallic-containing coating on the stress corrosion cracking behavior of a hot-dip galvanized steel | |
Kim et al. | Tensile and compressive behavior of tungsten, molybdenum, tantalum and niobium at the nanoscale | |
Gui et al. | Cracking and interfacial debonding of the Al–Si coating in hot stamping of pre-coated boron steel | |
Dieudonné et al. | Role of copper and aluminum additions on the hydrogen embrittlement susceptibility of austenitic Fe–Mn–C TWIP steels | |
He et al. | Improving ductility by increasing fraction of interfacial zone in low C steel/304 SS laminates | |
Wu et al. | ZrCu-based bulk metallic glass composites with large strain-hardening capability | |
Wang et al. | The effect of martensite volume and distribution on shear fracture propagation of 600–1000 MPa dual phase sheet steels in the process of deep drawing | |
Kim et al. | Energy-based approach to predict the fatigue life behavior of pre-strained Fe–18Mn TWIP steel | |
Lhuissier et al. | Strain field in a brittle/ductile multilayered steel composite | |
Golem et al. | Influence of austenitizing parameters on microstructure and mechanical properties of Al-Si coated press hardened steel | |
Deng et al. | Influence of coating thickness and temperature on mechanical properties of steel deposited with Co-based alloy hardfacing coating | |
Llanos et al. | Hot deformation and static softening behavior of vanadium microalloyed high manganese austenitic steels | |
Pierce et al. | Hot deformation behavior of an industrially cast large grained low density austenitic steel | |
Han et al. | Effect of carbon content on cracking phenomenon occurring during cold rolling of three light-weight steel plates | |
Yu et al. | Revealing extraordinary strength and toughness of multilayer TWIP/Maraging steels | |
Dymáček et al. | Tensile, creep and fracture testing of prospective Fe-Al-based alloys using miniature specimens | |
Mehner et al. | Hydrogen embrittlement of a quenching and partitioning steel during corrosion and zinc electroplating |