JPS5648270A - Formation of paint film for preventing bill - Google Patents
Formation of paint film for preventing billInfo
- Publication number
- JPS5648270A JPS5648270A JP12459279A JP12459279A JPS5648270A JP S5648270 A JPS5648270 A JP S5648270A JP 12459279 A JP12459279 A JP 12459279A JP 12459279 A JP12459279 A JP 12459279A JP S5648270 A JPS5648270 A JP S5648270A
- Authority
- JP
- Japan
- Prior art keywords
- film
- bill
- forming
- applying
- preventing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
PURPOSE: To form a paint film for preventing a building structure etc. from being sticked with bills, by applying painting material for forming thick film to the surface of the building structure, by forming irregular patterns on the film with a pattern roller, then by applying top coat of a specific composition to the film.
CONSTITUTION: A bill-preventing film is formed on the electric-light pole, fence, or wall of building etc., the film which makes it difficult to stick a bill or makes the bill peel off easily even if it is stuck. The surface ground of the electric-light pole etc. is adjusted by applying under coat to the surface at need. Then painting material of 100W500 poise viscosity at 25°C, for forming thick film, which contains 20W 70% aggregate such as silica etc. having a ratio of under 200 mesh: 30W150 mesh in the range 30W100:100W30, and epoxy resin and solvent, is applied to the undercoat. Then irregular pattern is formed using a pattern roller 4 attached with nap 2 having separated holes 3 1W20mm in depth, 5W100mm in length, 2W50mm in breadth. Finally, top coat composed of 100pts. film-forming resin, 5W80pts. silicone oil, and diluent is painted.
COPYRIGHT: (C)1981,JPO&Japio
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12459279A JPS5648270A (en) | 1979-09-27 | 1979-09-27 | Formation of paint film for preventing bill |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12459279A JPS5648270A (en) | 1979-09-27 | 1979-09-27 | Formation of paint film for preventing bill |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5648270A true JPS5648270A (en) | 1981-05-01 |
JPS6132076B2 JPS6132076B2 (en) | 1986-07-24 |
Family
ID=14889261
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP12459279A Granted JPS5648270A (en) | 1979-09-27 | 1979-09-27 | Formation of paint film for preventing bill |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5648270A (en) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63113641U (en) * | 1987-01-19 | 1988-07-21 | ||
JP2009263425A (en) * | 2008-04-22 | 2009-11-12 | Aica Kogyo Co Ltd | Aqueous coating composition |
KR102184648B1 (en) * | 2020-04-09 | 2020-11-30 | 김소중 | Waterproofing method with asphalt shingles prevention function |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63165850U (en) * | 1987-04-17 | 1988-10-28 | ||
KR102540158B1 (en) * | 2022-02-14 | 2023-06-05 | 주식회사 부일건화 | Waterproof method for concrete structure |
Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55132662A (en) * | 1979-04-04 | 1980-10-15 | Dainippon Toryo Co Ltd | Method for formation of bill-preventing paint film |
-
1979
- 1979-09-27 JP JP12459279A patent/JPS5648270A/en active Granted
Patent Citations (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS55132662A (en) * | 1979-04-04 | 1980-10-15 | Dainippon Toryo Co Ltd | Method for formation of bill-preventing paint film |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63113641U (en) * | 1987-01-19 | 1988-07-21 | ||
JP2009263425A (en) * | 2008-04-22 | 2009-11-12 | Aica Kogyo Co Ltd | Aqueous coating composition |
KR102184648B1 (en) * | 2020-04-09 | 2020-11-30 | 김소중 | Waterproofing method with asphalt shingles prevention function |
Also Published As
Publication number | Publication date |
---|---|
JPS6132076B2 (en) | 1986-07-24 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5648270A (en) | Formation of paint film for preventing bill | |
JPS5727177A (en) | Method for finishing ornamental wall representing pattern of natural stone | |
JPS55132662A (en) | Method for formation of bill-preventing paint film | |
JPS56150465A (en) | Decorative board | |
JPS5431447A (en) | Method of coating film of fluorine resin | |
JPS56129061A (en) | Coating of bricklike rugged decorative sheet | |
JPS5689876A (en) | Manufacture of decorative laminated material with unevenness pattern | |
JPS5719058A (en) | Patterning method | |
JPS5778977A (en) | Formation of two color finish painting surface | |
JPS55116468A (en) | Preparing enamel-pattern-like coated decorative board | |
JPS5481348A (en) | Production of decorative sheet | |
JPS54112938A (en) | Method of preventing paper sticking | |
SU670598A1 (en) | Powder polymeric ink | |
JPS54152576A (en) | Preparation of color board with three-dimensional pattern | |
JPS5455034A (en) | Crack pattern finish | |
JPS5775175A (en) | Anti-slip coating method for paint | |
JPS5567365A (en) | Decoration of sheet material | |
JPS5520650A (en) | Pattern forming method | |
JPS5631473A (en) | Preparation of building panel with brick pattern | |
JPS5473833A (en) | Roller coating | |
JPS5665663A (en) | Preparation of embossed patterns on decorative board | |
JPS5534154A (en) | Coating method of inorganic substrate | |
JPS5648273A (en) | Manufacture of decorative laminated panel | |
JPS567665A (en) | Preparation of decorative material | |
JPS5549171A (en) | Forming method of glued paper preventive paint film |