JPS56130432A - Improvement for residual stress of pipe - Google Patents
Improvement for residual stress of pipeInfo
- Publication number
- JPS56130432A JPS56130432A JP3161980A JP3161980A JPS56130432A JP S56130432 A JPS56130432 A JP S56130432A JP 3161980 A JP3161980 A JP 3161980A JP 3161980 A JP3161980 A JP 3161980A JP S56130432 A JPS56130432 A JP S56130432A
- Authority
- JP
- Japan
- Prior art keywords
- pipe
- weld zone
- cooling
- compressive stress
- quenching
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
PURPOSE:To improve a corrosion resistance and a fatigue endurance in a weld zone of a pipe by laying residual compressive stress on inner and outer surfaces of a weld zone through quenching an outer surface immediately after heating while cooling an inner surface thereof. CONSTITUTION:In pipe materials 1, 1' welded at a weld zone 2, a cooling water flows inside the pipe to cool, and at the same time a heating coil 3 of ring shape provided outside the weld zone 2 heats up the pipe locally by high frequency current from a high frequency heating device 5, rendering a residual compressive stress to an inner surface of the pipe and a residual tensile stress to an outer surface of it. Next, a cooling device 6 is arranged around an outer surface of the weld zone 2 and cooling medium 9 is made gushed out by opening a valve 8, quenching an outer surface of the pipe including the weld zone. In the outer surface of the pipe, a tensile yield is generated at the time of quenching, but a residual compressive stress is inversely generated with a complete cooling, thus the pipe in a state of residual compressive stress in both inner and outer surfaces is obtained, so that there is no decreases in a corrosion resistance and a fatigue endurance based on a residual tensile stress in the pipe.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3161980A JPS56130432A (en) | 1980-03-14 | 1980-03-14 | Improvement for residual stress of pipe |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3161980A JPS56130432A (en) | 1980-03-14 | 1980-03-14 | Improvement for residual stress of pipe |
Publications (1)
Publication Number | Publication Date |
---|---|
JPS56130432A true JPS56130432A (en) | 1981-10-13 |
Family
ID=12336223
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP3161980A Pending JPS56130432A (en) | 1980-03-14 | 1980-03-14 | Improvement for residual stress of pipe |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS56130432A (en) |
Cited By (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58221692A (en) * | 1982-06-17 | 1983-12-23 | Mitsubishi Heavy Ind Ltd | Correction method of welding strain |
JPS5933095A (en) * | 1982-08-19 | 1984-02-22 | Mitsubishi Heavy Ind Ltd | Method for relieving weld stress |
WO2011035780A1 (en) * | 2009-09-23 | 2011-03-31 | Acument Gmbh & Co Ohg | Parts welded in a rotationally symmetrical manner |
EP4375383A1 (en) * | 2022-11-28 | 2024-05-29 | MAHLE International GmbH | Method for introducing compressive stress in at least one target region |
-
1980
- 1980-03-14 JP JP3161980A patent/JPS56130432A/en active Pending
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS58221692A (en) * | 1982-06-17 | 1983-12-23 | Mitsubishi Heavy Ind Ltd | Correction method of welding strain |
JPS5933095A (en) * | 1982-08-19 | 1984-02-22 | Mitsubishi Heavy Ind Ltd | Method for relieving weld stress |
WO2011035780A1 (en) * | 2009-09-23 | 2011-03-31 | Acument Gmbh & Co Ohg | Parts welded in a rotationally symmetrical manner |
US9289863B2 (en) | 2009-09-23 | 2016-03-22 | Ruia Global Fasteners Ag | Parts welded in a rotationally symmetrical manner |
EP4375383A1 (en) * | 2022-11-28 | 2024-05-29 | MAHLE International GmbH | Method for introducing compressive stress in at least one target region |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3025596A (en) | Braze bonding of concentric tubes and shells and the like | |
US4348041A (en) | Butt welded tubular structure of austenite stainless steel | |
US3101404A (en) | Welding method employing ultrasonic energy | |
US2542393A (en) | Apparatus for welding | |
US2730599A (en) | Pressure welding by induction heating | |
JPS56130432A (en) | Improvement for residual stress of pipe | |
JPH0512274Y2 (en) | ||
SE8403928L (en) | HEAT TREATMENT PROCEDURE FOR A PIPE PIPE | |
JPS55146211A (en) | Manufacture of push rod for driving valve of internal combustion engine | |
JPS5617199A (en) | Method of improving stress corrosion cracking resistance of weld zone of austenite stainless steel pipe | |
JPS58210123A (en) | Heat treatment of clad steel pipe | |
JP3694365B2 (en) | Induction heating diffusion bonding method | |
JPS5770095A (en) | Method for improving residual stress of weld zone of pipe | |
JPS5414347A (en) | Heat treating method for welded joint | |
JPS55113836A (en) | High frequency surface hardening method of gear | |
JPS5494415A (en) | Heat treatment method of pipes | |
JPS56119664A (en) | Brazing method | |
JPS558462A (en) | Heat treating apparatus | |
JPS57203765A (en) | Damage resistant and abrasion resistant roll for continuous casting | |
JPS5762886A (en) | Improving method of residual stress in tube joint weld zone | |
JPS53130242A (en) | Welding method for manufacture of thick-walled large diameter welded steel pipe | |
JPS5762885A (en) | Inprovement of residual stress for welded part of pipe joint | |
Korzan et al. | Preferential Estimation of Parameters of Welding Pipes With High-Frequency Current Heating | |
JPS55158224A (en) | Hardening method for inner surface of pipe | |
JPH0147527B2 (en) |