JPH05205771A - Wrapping process for plate - Google Patents
Wrapping process for plateInfo
- Publication number
- JPH05205771A JPH05205771A JP4034544A JP3454492A JPH05205771A JP H05205771 A JPH05205771 A JP H05205771A JP 4034544 A JP4034544 A JP 4034544A JP 3454492 A JP3454492 A JP 3454492A JP H05205771 A JPH05205771 A JP H05205771A
- Authority
- JP
- Japan
- Prior art keywords
- separator
- electrode plate
- plate
- separators
- welded
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Description
【0001】[0001]
【産業上の利用分野】本発明は、ペースト式極板をセパ
レータで包装する方法に関するものである。BACKGROUND OF THE INVENTION 1. Field of the Invention The present invention relates to a method of packaging a paste type electrode plate with a separator.
【0002】[0002]
【従来の技術】従来、角形ニッケルカドミウム電池の陽
極板をセパレータで連続して包装する場合、図4に示す
ように、インデックステーブル1が90°回転する毎
に、極板ガイド2を通して2つ折りされたセパレータ3
の中に極板4が挿入されていた。そして、その場でセパ
レータ3の重なり部分3aが超音波等で溶着され、一定
間隔毎に移動するフィーダーで次工程へ移動し、極板4
をセパレータ3の折り曲げ部分までエアシリンダ5にて
押し込んでいた。2. Description of the Related Art Conventionally, when an anode plate of a prismatic nickel-cadmium battery is continuously packed with a separator, as shown in FIG. 4, every time the index table 1 is rotated by 90 °, it is folded in two through an electrode plate guide 2. Separator 3
The electrode plate 4 was inserted in the inside. Then, the overlapping portion 3a of the separator 3 is welded on the spot by ultrasonic waves or the like, and moved to the next step by a feeder that moves at regular intervals, and the electrode plate 4 is moved.
Was pushed by the air cylinder 5 to the bent portion of the separator 3.
【0003】[0003]
【発明が解決しようとする課題】従来の技術で述べた方
法は、極板4をエアシリンダ5でセパレータ3の間へ押
し込む時、極板4の表面がセパレータ3に引っ掛り、セ
パレータ3が損傷することがあった。特に、ニッケルマ
ットにペースト状活物質を塗り付けて乾燥させたペース
ト式極板は、セパレータ3の上での滑りが悪く、上記問
題点が顕著であり、連続して包装することができなかっ
た。In the method described in the prior art, when the electrode plate 4 is pushed into the space between the separators 3 by the air cylinder 5, the surface of the electrode plate 4 is caught by the separator 3 and the separator 3 is damaged. There was something to do. In particular, the paste-type electrode plate obtained by applying the paste-like active material to the nickel mat and drying it has a poor sliding property on the separator 3 and the above problems are prominent, so that it cannot be continuously packaged. ..
【0004】本発明は、上記問題点に鑑みてなされたも
のであって、その目的とするところは、セパレータを損
傷することなく、ペースト式極板を連続して包装する方
法を提供することにある。The present invention has been made in view of the above problems, and an object of the present invention is to provide a method for continuously packaging paste-type electrode plates without damaging the separator. is there.
【0005】[0005]
【課題を解決するための手段】上記目的を達成するため
に、本発明は、2つ折りしたセパレータ(3)を一定間
隔毎に移動させながら、極板(4)を該セパレータ
(3)で包装する方法において、前記セパレータ(3)
の間に極板(4)を挿入して、該セパレータ(3)の重
なり部分(3a)の一部を仮溶着する工程と、前記重な
り部分(3a)全体を溶着する工程とを有することを特
徴とするものである。[Means for Solving the Problems] In order to achieve the above object, the present invention wraps an electrode plate (4) with the separator (3) while moving the separator (3) folded in two at regular intervals. In the method, the separator (3)
And a step of inserting an electrode plate (4) between them to temporarily weld a part of the overlapping part (3a) of the separator (3) and a step of welding the entire overlapping part (3a). It is a feature.
【0006】[0006]
【作用】セパレータの間に極板を挿入する工程でセパレ
ータの折り目まで極板を挿入して、セパレータの重なり
部分の一部を仮溶着すると、セパレータ上で極板をずら
す必要がなく、極板が固定されるので次工程への移動中
に極板が位置ずれしない。[Operation] When the electrode plate is inserted between the separators and the electrode plate is inserted up to the fold of the separator and part of the overlapping portion of the separator is temporarily welded, it is not necessary to shift the electrode plate on the separator Is fixed, the electrode plate is not displaced during the movement to the next process.
【0007】[0007]
【実施例】本発明の実施例を図面を参照して説明する。
図1は、本発明の実施例を示す説明図で、1はインデッ
クステーブルでクランプ1aで陽極板4を把持して90
°毎に回転する。2は極板ガイドで2つ折りされたセパ
レータ3の間に極板4が挿入され易いようにしている。
尚、セパレータ3は一定間隔(図の矢印の間隔)毎に移
動するフィーダー(図示せず)に載置されている。Embodiments of the present invention will be described with reference to the drawings.
FIG. 1 is an explanatory view showing an embodiment of the present invention, in which an index table 1 is a clamp 1a for holding an anode plate 4 and is 90
Rotate every °. Reference numeral 2 makes it easy for the electrode plate 4 to be inserted between the separators 3 folded in two by the electrode plate guide.
The separator 3 is placed on a feeder (not shown) that moves at regular intervals (intervals indicated by arrows in the figure).
【0008】次に、本発明の製造方法を説明する。図1
のように、インデックステーブル1のクランプ1aで把
持された陽極板4を90°回転し、セパレータ3の折り
曲げ部分まで挿入する。この時の図1のA−A’断面図
を図2に示す。この際陽極板4の回転部分に位置するセ
パレータ3の間には、内側が鏡面仕上げされた極板ガイ
ド2が配置され、陽極板4がセパレータ3の間にスムー
ズに挿入され易い様にしている。そして、陽極板4が把
持されたままで該陽極板4の両側のセパレータ3が重な
りあった部分3aの上下2点ずつを超音波により仮溶着
する。極板ガイドには、図3の拡大図で示すように、仮
溶着できるように切込み2aを入れてある。Next, the manufacturing method of the present invention will be described. Figure 1
As described above, the anode plate 4 gripped by the clamp 1a of the index table 1 is rotated by 90 ° and is inserted up to the bent portion of the separator 3. FIG. 2 is a sectional view taken along the line AA ′ of FIG. 1 at this time. At this time, an electrode plate guide 2 whose inside is mirror-finished is arranged between the separators 3 located at the rotating portion of the anode plate 4 so that the anode plate 4 can be smoothly inserted between the separators 3. . Then, while the anode plate 4 is being held, the upper and lower two points of the overlapping portion 3a of the separators 3 on both sides of the anode plate 4 are temporarily welded by ultrasonic waves. As shown in the enlarged view of FIG. 3, the electrode plate guide is provided with a cut 2a for temporary welding.
【0009】仮溶着が終了するとクランプ1aから陽極
板4を解除して、インデックステーブル1を90°回転
すると共にセパレータ3をフィーダーにより一定間隔移
動する。この時陽極板4は両側の上下2点ずつ計4点で
固定されているためセパレータ3の間でずれることがな
い。こうして一定間隔ずつ陽極板4入りのセパレータ3
を次工程へ送り、次工程で前記セパレータ3の重なり部
分3a全体を超音波溶着して、該溶着部分の中央を切断
して、袋状のセパレータに入った陽極板を1枚ずつ製作
する。When the temporary welding is completed, the anode plate 4 is released from the clamp 1a, the index table 1 is rotated by 90 °, and the separator 3 is moved by a constant distance by the feeder. At this time, since the anode plate 4 is fixed at a total of four points on each of the upper and lower two points, there is no displacement between the separators 3. Thus, the separator 3 containing the anode plate 4 at regular intervals
Is sent to the next step, and in the next step, the entire overlapping portion 3a of the separator 3 is ultrasonically welded, the center of the welded portion is cut, and one anode plate in each bag-shaped separator is manufactured.
【0010】[0010]
【発明の効果】本発明は、上述のとおり構成されている
ので、次に記載する効果を奏する。 (1)極板がセパレータの上をずれることがないので、
セパレータが損傷しない。 (2)極板の挿入工程からセパレータの溶着工程までの
移動中に極板が位置ずれしない。Since the present invention is configured as described above, it has the following effects. (1) Since the electrode plate does not shift on the separator,
The separator is not damaged. (2) The electrode plate is not displaced during the movement from the electrode plate inserting step to the separator welding step.
【図1】本発明の実施例を示す説明図である。FIG. 1 is an explanatory diagram showing an embodiment of the present invention.
【図2】図1のA−A’部断面図である。FIG. 2 is a sectional view taken along the line A-A ′ in FIG.
【図3】図1のB部拡大図である。FIG. 3 is an enlarged view of part B in FIG.
【図4】従来の方法を示す説明図である。FIG. 4 is an explanatory diagram showing a conventional method.
3 セパレータ 3a セパレータの重なり部分 4 極板 3 Separator 3a Overlapping part of separator 4 Electrode plate
Claims (1)
隔毎に移動させながら、極板(4)を該セパレータ
(3)で包装する方法において、 前記セパレータ(3)の間に極板(4)を挿入して、該
セパレータ(3)の重なり部分(3a)の一部を仮溶着
する工程と、 前記重なり部分(3a)全体を溶着する工程とを有する
ことを特徴とする、 極板の包装方法。1. A method of wrapping an electrode plate (4) with the separator (3) while moving the separator (3) folded in two at regular intervals, wherein the electrode plate (4) is placed between the separators (3). ) Is inserted to temporarily weld a part of the overlapping portion (3a) of the separator (3) and a step of welding the entire overlapping portion (3a) to each other. Packaging method.