Nothing Special   »   [go: up one dir, main page]

JP6274574B2 - Laminated glass, glass with heating mechanism and vehicle - Google Patents

Laminated glass, glass with heating mechanism and vehicle Download PDF

Info

Publication number
JP6274574B2
JP6274574B2 JP2014190395A JP2014190395A JP6274574B2 JP 6274574 B2 JP6274574 B2 JP 6274574B2 JP 2014190395 A JP2014190395 A JP 2014190395A JP 2014190395 A JP2014190395 A JP 2014190395A JP 6274574 B2 JP6274574 B2 JP 6274574B2
Authority
JP
Japan
Prior art keywords
conductive
mesh
glass
laminated glass
base material
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
JP2014190395A
Other languages
Japanese (ja)
Other versions
JP2016060668A (en
Inventor
川 晃次郎 大
川 晃次郎 大
倉 哲 夫 松
倉 哲 夫 松
上 功 井
上 功 井
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Dai Nippon Printing Co Ltd
Original Assignee
Dai Nippon Printing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dai Nippon Printing Co Ltd filed Critical Dai Nippon Printing Co Ltd
Priority to JP2014190395A priority Critical patent/JP6274574B2/en
Publication of JP2016060668A publication Critical patent/JP2016060668A/en
Application granted granted Critical
Publication of JP6274574B2 publication Critical patent/JP6274574B2/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Description

本発明は、メッシュシートを有する合わせガラス、合わせガラスを有する加熱機構付きガラス、並びに、合わせガラスを有する乗り物に関する。   The present invention relates to a laminated glass having a mesh sheet, a glass with a heating mechanism having a laminated glass, and a vehicle having the laminated glass.

従来、車両のフロントウィンドウやリアウィンドウ等の窓ガラスに用いるデフロスタ装置として、窓ガラス全体にタングステン線等からなる電熱線を配置したものが知られている(例えば、特許文献1、特許文献2を参照)。この従来技術では、窓ガラス全体に配置された電熱線に通電し、その抵抗加熱により窓ガラスを昇温させて、窓ガラスの曇りを取り除いて、又は、窓ガラスに付着した雪や氷を溶かして、乗員の視界を確保することができる。   2. Description of the Related Art Conventionally, as a defroster device used for a window glass such as a front window or a rear window of a vehicle, an apparatus in which a heating wire made of tungsten wire or the like is arranged on the entire window glass is known (for example, Patent Document 1 and Patent Document 2). reference). In this prior art, a heating wire arranged on the entire window glass is energized, and the window glass is heated by resistance heating to remove fogging of the window glass or to melt snow and ice attached to the window glass. The occupant's field of view can be secured.

特開2013−173402号公報JP 2013-173402 A 特開平8−72674号公報JP-A-8-72674

従来技術のデフロスタ装置では、一対のガラス板の間に、接合層及び電熱線を挟み込んで加熱圧着し、合わせガラスとしていた。また、電熱線としては、別工程で製造されたタングステン線等からなるものを用いていた。しかし、別工程で製造された電熱線を配置する方法では、電熱線の配置パターンは直線や波線等の簡単な形状に限られ、複雑な形状に配置することは難しかった。また、断面形状が矩形状等の電熱線は、ガラス板上又は樹脂層上に、その向きを合わせて適切に配置することが困難である。したがって、電熱線としては、断面形状が円形のものを用いるしかなかった。   In a conventional defroster device, a bonding layer and a heating wire are sandwiched between a pair of glass plates and thermocompression bonded to form a laminated glass. Moreover, as a heating wire, what consists of the tungsten wire etc. which were manufactured at another process was used. However, in the method of arranging heating wires manufactured in a separate process, the arrangement pattern of heating wires is limited to simple shapes such as straight lines and wavy lines, and it is difficult to arrange them in a complicated shape. In addition, it is difficult to properly arrange heating wires having a rectangular cross-sectional shape on the glass plate or the resin layer in the same direction. Therefore, the heating wire has only to have a circular cross-sectional shape.

一方、配線の形成方法として、ベース基材上に、フォトリソグラフィー技術を用いたパターニングにより導電配線を形成する方法が知られている。この方法は、まず、平板状のベース基材上に、銅箔等の金属箔の貼着、めっき、スパッタリング等により導電性金属層を形成する。次に、導電性金属層上にフォトリソグラフィー技術を用いてレジストパターンを形成する。そして、このレジストパターンをマスクとして、導電性金属層をエッチングする。このエッチングにより、導電性金属層がレジストパターンと略同一のパターンにパターニングされる。この方法は、複雑な配置パターンや断面形状の導電配線であっても簡単に形成できるという利点がある。   On the other hand, as a wiring forming method, a method of forming a conductive wiring on a base substrate by patterning using a photolithography technique is known. In this method, first, a conductive metal layer is formed on a flat base substrate by attaching a metal foil such as a copper foil, plating, sputtering, or the like. Next, a resist pattern is formed on the conductive metal layer using a photolithography technique. Then, the conductive metal layer is etched using this resist pattern as a mask. By this etching, the conductive metal layer is patterned into a pattern substantially the same as the resist pattern. This method has an advantage that even a conductive wiring having a complicated arrangement pattern or cross-sectional shape can be easily formed.

ところで、車両のフロントウィンドウやリアウィンドウ等の窓ガラスには、空気抵抗の低減や意匠性の向上等のために、湾曲しているものが多い。そして、この湾曲した窓ガラスに電熱線を備えたデフロスタ装置を設ける場合、一対の湾曲したガラス板の間に、電熱線を挟み込んで合わせガラスとする必要がある。   By the way, many window glasses such as a front window and a rear window of a vehicle are curved in order to reduce air resistance and improve design. And when providing the defroster apparatus provided with the heating wire in this curved window glass, it is necessary to insert | stack a heating wire between a pair of curved glass plates to make a laminated glass.

しかし、湾曲した一対のガラス板の間に、平板状の部材を挟み込もうとすると、平板状の部材がガラス板の湾曲に追従しきれず、平板状の部材にしわが発生する問題がある。したがって、デフロスタ装置を備えた合わせガラスにおける電熱線の形成の際に、上述の、ベース基材上に、フォトリソグラフィー技術を用いたパターニングにより導電配線を形成する技術を採用することはできなかった。   However, if a flat plate member is sandwiched between a pair of curved glass plates, there is a problem that the flat plate member cannot follow the curve of the glass plate and wrinkles occur in the flat plate member. Therefore, when the heating wire is formed in the laminated glass provided with the defroster device, it has not been possible to employ the above-described technology for forming the conductive wiring on the base substrate by patterning using the photolithography technology.

本発明は、以上の点を考慮してなされたものであり、基材上に導電性メッシュを形成したメッシュシートを、一対の湾曲したガラス板の間に挟み込んだ際に、メッシュシートへのしわの発生を適切に抑制することを目的とする。   The present invention has been made in consideration of the above points, and when a mesh sheet in which a conductive mesh is formed on a substrate is sandwiched between a pair of curved glass plates, wrinkles are generated on the mesh sheet. It aims at suppressing appropriately.

本発明による合わせガラスは、
一対の湾曲したガラスと、
前記一対の湾曲したガラスの間に配置されたメッシュシートと、
前記各ガラスと前記メッシュシートとの間に配置され且つ当該ガラスと前記メッシュシートとを接合する接合層と、を備え、
前記メッシュシートは、無延伸樹脂基材と、前記無延伸樹脂基材上に形成された導電性メッシュと、を有する。
The laminated glass according to the present invention is
A pair of curved glasses;
A mesh sheet disposed between the pair of curved glasses;
A bonding layer disposed between each glass and the mesh sheet and bonding the glass and the mesh sheet;
The mesh sheet has an unstretched resin base material and a conductive mesh formed on the unstretched resin base material.

本発明による合わせガラスにおいて、導電性メッシュは、導電細線を用いて形成され、導電細線の幅は、メッシュシートの法線方向に沿って無延伸樹脂基材から離間するにつれて狭くなるように変化してもよい。   In the laminated glass according to the present invention, the conductive mesh is formed using a conductive fine wire, and the width of the conductive fine wire changes so as to become narrower as the distance from the unstretched resin base material increases along the normal direction of the mesh sheet. May be.

本発明による合わせガラスにおいて、導電性メッシュは、導電細線を用いて形成され、導電細線は、導電性金属層と、導電性金属層の表面の少なくとも一部分を覆う暗色層と、を有してもよい。   In the laminated glass according to the present invention, the conductive mesh is formed using a conductive fine wire, and the conductive fine wire may include a conductive metal layer and a dark color layer covering at least a part of the surface of the conductive metal layer. Good.

本発明による加熱機構付きガラスは、上述の合わせガラスと、合わせガラスの導電性メッシュに接続された電源と、を備える。   The glass with a heating mechanism according to the present invention includes the laminated glass described above and a power source connected to the conductive mesh of the laminated glass.

本発明による乗り物は、上述の合わせガラスを備える。   A vehicle according to the present invention includes the laminated glass described above.

本発明によれば、ベース基材上に電熱線を形成したシートを、一対の湾曲したガラス板の間に挟み込んだ際に、シートにおけるしわの発生を適切に抑制することができる。   ADVANTAGE OF THE INVENTION According to this invention, when the sheet | seat which formed the heating wire on the base base material is pinched | interposed between a pair of curved glass plates, generation | occurrence | production of a wrinkle in a sheet | seat can be suppressed appropriately.

図1は、本発明による一実施の形態を説明するための図であって、合わせガラスを備えた乗り物を概略的に示す斜視図である。特に図1では、乗り物の例として合わせガラスを備えた自動車を概略的に示している。FIG. 1 is a diagram for explaining an embodiment according to the present invention, and is a perspective view schematically showing a vehicle provided with a laminated glass. In particular, FIG. 1 schematically shows an automobile with laminated glass as an example of a vehicle. 図2は、合わせガラスをその板面の法線方向から見た図である。FIG. 2 is a view of the laminated glass as viewed from the normal direction of the plate surface. 図3は、図2の合わせガラスの横断面図である。FIG. 3 is a cross-sectional view of the laminated glass of FIG. 図4は、図3の合わせガラスを構成する各部材の積層前の状態を示す図である。FIG. 4 is a view showing a state before lamination of each member constituting the laminated glass of FIG. 図5は、メッシュシートをそのシート面の法線方向から見た平面図であって、導電性メッシュのパターンの一例を示す平面図である。FIG. 5 is a plan view of the mesh sheet as seen from the normal direction of the sheet surface, and is a plan view showing an example of a conductive mesh pattern. 図6は、図5のA−A線に対応する断面図であって、導電細線の断面形状の一例を示す図である。FIG. 6 is a cross-sectional view corresponding to the line AA in FIG. 5, and is a diagram illustrating an example of a cross-sectional shape of the conductive thin wire. 図7は、図5のA−A線に対応する断面図であって、導電細線の断面形状の他の例を示す図である。FIG. 7 is a cross-sectional view corresponding to the line AA in FIG. 5 and is a diagram illustrating another example of the cross-sectional shape of the conductive thin wire. 図8は、合わせガラスの製造方法の一例を説明するための図である。FIG. 8 is a diagram for explaining an example of a method for producing laminated glass. 図9は、合わせガラスの製造方法の一例を説明するための図である。FIG. 9 is a diagram for explaining an example of a method for producing laminated glass. 図10は、合わせガラスの製造方法の一例を説明するための図である。FIG. 10 is a diagram for explaining an example of a method for producing laminated glass. 図11は、合わせガラスの製造方法の一例を説明するための図である。FIG. 11 is a diagram for explaining an example of a method for producing laminated glass. 図12は、合わせガラスの製造方法の一例を説明するための図である。FIG. 12 is a diagram for explaining an example of a method for producing laminated glass. 図13は、合わせガラスの製造方法の一例を説明するための図である。FIG. 13 is a diagram for explaining an example of a method for producing laminated glass. 図14は、合わせガラスの製造方法の一例を説明するための図である。FIG. 14 is a diagram for explaining an example of a method for producing laminated glass. 図15は、合わせガラスの製造方法の一例を説明するための図である。FIG. 15 is a diagram for explaining an example of a method for manufacturing a laminated glass.

以下、図面を参照して本発明の一実施の形態について説明する。なお、本件明細書に添付する図面においては、図示と理解のしやすさの便宜上、適宜縮尺および縦横の寸法比等を、実物のそれらから変更し誇張してある。   Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the drawings attached to the present specification, for the sake of illustration and ease of understanding, the scale, the vertical / horizontal dimension ratio, and the like are appropriately changed and exaggerated from those of the actual product.

なお、本明細書において、「板」、「シート」、「フィルム」の用語は、呼称の違いのみに基づいて、互いから区別されるものではない。例えば、「メッシュシート」は板やフィルムと呼ばれ得るような部材をも含む概念であり、したがって、「メッシュシート」は、「メッシュ板(基板)」や「メッシュフィルム」と呼ばれる部材と、呼称の違いのみにおいて区別され得ない。   In the present specification, the terms “plate”, “sheet”, and “film” are not distinguished from each other only based on the difference in names. For example, “mesh sheet” is a concept that includes a member that can be called a plate or a film. Therefore, “mesh sheet” is a member called “mesh plate (substrate)” or “mesh film”. It cannot be distinguished only by the difference.

また、「シート面(板面、フィルム面)」とは、対象となるシート状(板状、フィルム状)の部材を全体的かつ大局的に見た場合において対象となるシート状部材(板状部材、フィルム状部材)の平面方向と一致する面のことを指す。   In addition, “sheet surface (plate surface, film surface)” means a target sheet-like member (plate-like) when the target sheet-like (plate-like, film-like) member is viewed as a whole and globally. It refers to the surface that coincides with the plane direction of the member or film-like member.

さらに、本明細書において用いる、形状や幾何学的条件並びにそれらの程度を特定する、例えば、「平行」、「直交」、「同一」等の用語や長さや角度の値等については、厳密な意味に縛られることなく、同様の機能を期待し得る程度の範囲を含めて解釈することとする。   Furthermore, as used in this specification, the shape and geometric conditions and the degree thereof are specified. For example, terms such as “parallel”, “orthogonal”, “identical”, length and angle values, etc. Without being bound by meaning, it should be interpreted including the extent to which similar functions can be expected.

図1〜図15は、本発明による一実施の形態を説明するための図である。このうち図1は、合わせガラスを備えた自動車を概略的に示す図であり、図2は、合わせガラスをその板面の法線方向から見た図であり、図3は、図2の合わせガラスの横断面図であり、図4は、図3の合わせガラスを構成する各部材の積層前の状態を示す図である。   1 to 15 are diagrams for explaining an embodiment according to the present invention. Among these, FIG. 1 is a diagram schematically showing an automobile equipped with a laminated glass, FIG. 2 is a diagram of the laminated glass viewed from the normal direction of the plate surface, and FIG. 3 is a diagram of FIG. FIG. 4 is a cross-sectional view of the glass, and FIG. 4 is a diagram showing a state before lamination of each member constituting the laminated glass of FIG.

図1に示されているように、乗り物の一例としての自動車1は、フロントウィンドウ、リアウィンドウ、サイドウィンドウ等の窓ガラスを有している。ここでは、フロントウィンドウ5が合わせガラス10で構成されている例を説明する。また、自動車1はバッテリー等の電源7を有している。   As shown in FIG. 1, an automobile 1 as an example of a vehicle has window glasses such as a front window, a rear window, and a side window. Here, an example in which the front window 5 is formed of a laminated glass 10 will be described. The automobile 1 has a power source 7 such as a battery.

この合わせガラス10をその板面の法線方向から見たものを図2に示す。また、図2の合わせガラス10のIII−III線に対応する横断面図を図3に示す。合わせガラス10は、一対の湾曲したガラス板11,12と、一対の湾曲したガラス板11,12の間に配置されたメッシュシート20と、ガラス板11,12とメッシュシート20とを接合する接合層13,14とを有している。   FIG. 2 shows the laminated glass 10 viewed from the normal direction of the plate surface. Moreover, the cross-sectional view corresponding to the III-III line of the laminated glass 10 of FIG. 2 is shown in FIG. The laminated glass 10 includes a pair of curved glass plates 11 and 12, a mesh sheet 20 disposed between the pair of curved glass plates 11 and 12, and a joint that joins the glass plates 11 and 12 and the mesh sheet 20. Layers 13 and 14.

メッシュシート20は、基材30と、基材30上に形成された導電性メッシュ40と、導電性メッシュ40に通電するための配線部15と、導電性メッシュ40と配線部15とを接続する接続部16とを有している。   The mesh sheet 20 connects the base material 30, the conductive mesh 40 formed on the base material 30, the wiring part 15 for energizing the conductive mesh 40, and the conductive mesh 40 and the wiring part 15. And a connecting portion 16.

図2及び図3に示した例では、バッテリー等の電源7から、配線部15及び接続部16を介して導電性メッシュ40に通電し、導電性メッシュ40を抵抗加熱により発熱させる。導電性メッシュ40で発生した熱は接合層13,14を介してガラス板11,12に伝わり、ガラス板11,12が温められる。これにより、ガラス板11,12に付着した結露による曇りを取り除くことができる。また、ガラス板11,12に雪や氷が付着している場合には、この雪や氷を溶かすことができる。したがって、乗員の視界が良好に確保される。   In the example shown in FIGS. 2 and 3, the conductive mesh 40 is energized from the power source 7 such as a battery through the wiring portion 15 and the connection portion 16, and the conductive mesh 40 is heated by resistance heating. The heat generated in the conductive mesh 40 is transmitted to the glass plates 11 and 12 through the bonding layers 13 and 14, and the glass plates 11 and 12 are warmed. Thereby, the cloudiness by the dew condensation adhering to the glass plates 11 and 12 can be removed. Moreover, when snow and ice adhere to the glass plates 11 and 12, this snow and ice can be melted. Therefore, a passenger | crew's visual field is ensured favorable.

この合わせガラス10を作成するには、図4に示すように、湾曲したガラス板11、接合層13、メッシュシート20、接合層14、湾曲したガラス板12をこの順に重ね合わせ、加熱・加圧することで、湾曲したガラス板11、メッシュシート20及び湾曲したガラス板12が、接合層13,14により接合される。   In order to produce this laminated glass 10, as shown in FIG. 4, the curved glass plate 11, the bonding layer 13, the mesh sheet 20, the bonding layer 14, and the curved glass plate 12 are superposed in this order, and heated and pressurized. Thus, the curved glass plate 11, the mesh sheet 20, and the curved glass plate 12 are bonded by the bonding layers 13 and 14.

この際、湾曲したガラス板11,12の間に平板状のメッシュシート20が挟み込まれるが、メッシュシート20の基材30として、無延伸樹脂基材30を用いることにより、メッシュシート20へのしわの発生を適切に抑制することができる。この基材30の詳細については後述する。   At this time, the flat mesh sheet 20 is sandwiched between the curved glass plates 11 and 12, but by using the unstretched resin base material 30 as the base material 30 of the mesh sheet 20, wrinkles to the mesh sheet 20 are achieved. Can be appropriately suppressed. Details of the substrate 30 will be described later.

ガラス板11,12は、特にフロントウィンドウに用いる場合、乗員の視界を妨げないよう可視光透過率が高いものを用いることが好ましい。このようなガラス板11,12の材質としては、ソーダライムガラス、青板ガラス等が例示できる。ガラス板11,12は、可視光領域における透過率が90%以上であることが好ましい。ここで、ガラス板11,12の可視光透過率は、分光光度計((株)島津製作所製「UV−3100PC」、JISK0115準拠品)を用いて測定波長380nm〜780nmの範囲内で測定したときの、各波長における透過率の平均値として特定される。なお、ガラス板11,12の一部または全体に着色するなどして、可視光透過率を低くしてもよい。この場合、太陽光の直射を遮ったり、車外から車内を視認しにくくしたりすることができる。   In particular, when the glass plates 11 and 12 are used for a front window, it is preferable to use a glass plate having a high visible light transmittance so as not to obstruct the occupant's field of view. Examples of the material of the glass plates 11 and 12 include soda lime glass and blue plate glass. The glass plates 11 and 12 preferably have a transmittance in the visible light region of 90% or more. Here, the visible light transmittance of the glass plates 11 and 12 is measured within a measurement wavelength range of 380 nm to 780 nm using a spectrophotometer (“UV-3100PC” manufactured by Shimadzu Corporation, JISK0115 compliant product). Of the transmittance at each wavelength. The visible light transmittance may be lowered by coloring a part or the whole of the glass plates 11 and 12. In this case, it is possible to block direct sunlight and to make it difficult to visually recognize the inside of the vehicle from outside the vehicle.

また、ガラス板11,12は、1mm以上5mm以下の厚みを有していることが好ましい。このような厚みであると、強度及び光学特性に優れたガラス板11,12を得ることができる。   Moreover, it is preferable that the glass plates 11 and 12 have a thickness of 1 mm or more and 5 mm or less. With such a thickness, the glass plates 11 and 12 excellent in strength and optical characteristics can be obtained.

ガラス板11,12とメッシュシート20とは、それぞれ接合層13,14を介して接合されている。このような接合層13,14としては、種々の接着性または粘着性を有した材料からなる層を用いることができる。また、接合層13,14は、可視光透過率が高いものを用いることが好ましい。典型的な接合層としては、ポリビニルブチラール(PVB)からなる層を例示することができる。接合層13,14の厚みは、それぞれ0.15mm以上0.7mm以下であることが好ましい。   The glass plates 11 and 12 and the mesh sheet 20 are bonded via bonding layers 13 and 14, respectively. As the bonding layers 13 and 14, layers made of materials having various adhesiveness or tackiness can be used. The bonding layers 13 and 14 preferably have a high visible light transmittance. As a typical joining layer, the layer which consists of polyvinyl butyral (PVB) can be illustrated. The thickness of the bonding layers 13 and 14 is preferably 0.15 mm or more and 0.7 mm or less, respectively.

なお、合わせガラス10には、図示された例に限られず、特定の機能を発揮することを期待されたその他の機能層が設けられても良い。また、一つの機能層が二以上の機能を発揮するようにしてもよいし、例えば、合わせガラス10のガラス板11,12、接合層13,14や、後述するメッシュシート20の基材30の少なくとも1つに機能を付与するようにしてもよい。合わせガラス10に付与され得る機能としては、一例として、反射防止(AR)機能、耐擦傷性を有したハードコート(HC)機能、赤外線遮蔽(反射)機能、紫外線遮蔽(反射)機能、偏光機能、防汚機能等を例示することができる。   The laminated glass 10 is not limited to the illustrated example, and may be provided with other functional layers expected to exhibit a specific function. Moreover, you may make it one functional layer exhibit two or more functions, for example, the glass plates 11 and 12 of the laminated glass 10, the joining layers 13 and 14, and the base material 30 of the mesh sheet 20 mentioned later You may make it provide a function to at least one. Examples of functions that can be imparted to the laminated glass 10 include antireflection (AR) function, hard coat (HC) function having scratch resistance, infrared shielding (reflection) function, ultraviolet shielding (reflection) function, and polarization function. An antifouling function and the like can be exemplified.

次に、メッシュシート20について説明する。メッシュシート20は、基材30と、基材30上に設けられた導電性メッシュ40と、導電性メッシュ40に通電するための配線部15と、導電性メッシュ40と配線部15とを接続する接続部16とを有している。メッシュシート20は、ガラス板11,12と略同一の平面寸法を有して、合わせガラス10の全体にわたって配置されてもよいし、運転席の正面部分等、合わせガラス10の一部にのみ配置されてもよい。   Next, the mesh sheet 20 will be described. The mesh sheet 20 connects the base material 30, the conductive mesh 40 provided on the base material 30, the wiring part 15 for energizing the conductive mesh 40, and the conductive mesh 40 and the wiring part 15. And a connecting portion 16. The mesh sheet 20 has substantially the same plane dimensions as the glass plates 11 and 12, and may be disposed over the entire laminated glass 10, or only on a part of the laminated glass 10 such as a front portion of a driver's seat. May be.

基材30は、導電性メッシュ40を支持する基材として機能する。基材30は、可視光線波長帯域の波長(380nm〜780nm)を透過する一般に言うところの透明である電気絶縁性の基板であって、その製造工程において実質的に延伸を行っていない、すなわち無延伸の樹脂基材である。   The base material 30 functions as a base material that supports the conductive mesh 40. The base material 30 is a transparent and electrically insulating substrate that generally transmits a wavelength in the visible light wavelength band (380 nm to 780 nm), and is not substantially stretched in its manufacturing process. It is a stretched resin substrate.

基材30は、押出法、カレンダー法、キャスティング法等の、延伸工程を含まない公知の方法により作製することができる。ここで、基材となるシートの製造工程中または製造工程後の巻き取り工程において、このシートが引っ張られ、場合によってはわずかに延伸することがあるが、これは「延伸」には含まない。言い換えると、シートを適切に巻き取るために不可避の延伸が生じたとしても、実質的な延伸工程を含んでいない限り、その工程で製造されたシートは、「無延伸」のシートに含まれる。   The base material 30 can be produced by a known method that does not include a stretching step, such as an extrusion method, a calendar method, or a casting method. Here, in the winding process after the manufacturing process or after the manufacturing process of the sheet as the base material, the sheet is pulled and may be slightly stretched in some cases, but this is not included in “stretching”. In other words, even if unavoidable stretching occurs in order to properly wind the sheet, the sheet produced in that process is included in the “unstretched” sheet unless it includes a substantial stretching process.

基材30に含まれる樹脂としては、可視光を透過する樹脂であればいかなる樹脂でもよいが、好ましくは熱可塑性樹脂を用いることができる。この熱可塑性樹脂としては、例えば、ポリメチルメタクリレート等のアクリル樹脂、ポリ塩化ビニル、ポリエチレンテレフタレート、アモルファスポリエチレンテレフタレート(A−PET)等のポリエステル樹脂、ポリエチレン樹脂、ポリプロピレン等のポリオレフィン樹脂、トリアセチルセルロース(三酢酸セルロース)等のセルロース系樹脂、ポリスチレン、ポリカーボネート樹脂、AS樹脂等を挙げることができる。とりわけ、アクリル樹脂やポリ塩化ビニルは、エッチング耐性、耐候性、耐光性に優れており、好ましい。   The resin contained in the base material 30 may be any resin as long as it transmits visible light, but a thermoplastic resin can be preferably used. Examples of the thermoplastic resin include acrylic resins such as polymethyl methacrylate, polyester resins such as polyvinyl chloride, polyethylene terephthalate, and amorphous polyethylene terephthalate (A-PET), polyolefin resins such as polyethylene resin and polypropylene, triacetyl cellulose ( Cellulose resins such as cellulose triacetate), polystyrene, polycarbonate resin, AS resin, and the like. In particular, acrylic resin and polyvinyl chloride are preferable because they are excellent in etching resistance, weather resistance, and light resistance.

また、基材30は、導電性メッシュ40の保持性や、光透過性等を考慮すると、0.03mm以上0.15mm以下の厚みを有していることが好ましい。   Moreover, it is preferable that the base material 30 has a thickness of 0.03 mm or more and 0.15 mm or less in consideration of retainability of the conductive mesh 40, light transmittance, and the like.

図5〜図7を参照して、導電性メッシュ40について説明する。図5は、メッシュシート20をそのシート面の法線方向から見た平面図であって、導電性メッシュ40の配置パターンの一例を示す図である。   The conductive mesh 40 will be described with reference to FIGS. FIG. 5 is a plan view of the mesh sheet 20 as viewed from the normal direction of the sheet surface, and is a diagram illustrating an example of an arrangement pattern of the conductive mesh 40.

導電性メッシュ40は、バッテリー等の電源7から、配線部15及び接続部16を介して通電され、抵抗加熱により発熱する。そして、この熱が接合層13,14を介してガラス板11,12に伝わることで、ガラス板11,12が温められる。   The conductive mesh 40 is energized from the power source 7 such as a battery through the wiring portion 15 and the connection portion 16 and generates heat by resistance heating. And when this heat | fever is transmitted to the glass plates 11 and 12 through the joining layers 13 and 14, the glass plates 11 and 12 are warmed.

図5に示されているように、導電性メッシュ40は、多数の開口43を画成するメッシュ状の部材である。導電性メッシュ40は、2つの分岐点42の間を延びて、開口43を画成する複数の導電細線41を含んでいる。すなわち、導電性メッシュ40は、両端において分岐点42を形成する多数の導電細線41の集まりとして構成されている。とりわけ図示された例では、分岐点42において、3つの導電細線41が等角度で接続されることにより、6つの導電細線41で囲まれた同一形状のハニカム状の開口43が多数画成されている。   As shown in FIG. 5, the conductive mesh 40 is a mesh member that defines a large number of openings 43. The conductive mesh 40 includes a plurality of conductive thin wires 41 extending between the two branch points 42 and defining the openings 43. That is, the conductive mesh 40 is configured as a collection of a large number of thin conductive wires 41 that form branch points 42 at both ends. In particular, in the illustrated example, at the branch point 42, three conductive thin wires 41 are connected at an equal angle, so that a large number of honeycomb-shaped openings 43 of the same shape surrounded by the six conductive thin wires 41 are defined. Yes.

図示された例では、導電性メッシュ40は、同一形状のハニカム状の開口43が規則的に配置されたメッシュパターンを有しているが、このようなメッシュパターンに限られず、三角形、矩形等の同一形状の開口43が規則的に配置されたメッシュパターン、異形状の開口43が規則的に配置されたメッシュパターン、ボロノイメッシュのような、異形状の開口43が不規則的に配置されたメッシュパターン等、種々のメッシュパターンを用いることができる。   In the illustrated example, the conductive mesh 40 has a mesh pattern in which honeycomb-shaped openings 43 having the same shape are regularly arranged. However, the conductive mesh 40 is not limited to such a mesh pattern, and may be a triangle, a rectangle, or the like. Mesh pattern in which irregularly shaped openings 43 are irregularly arranged, such as a mesh pattern in which openings 43 of the same shape are regularly arranged, a mesh pattern in which irregularly shaped openings 43 are regularly arranged, and a Voronoi mesh Various mesh patterns such as patterns can be used.

このような導電性メッシュ40を構成するための材料としては、例えば、金、銀、銅、白金、アルミニウム、クロム、モリブデン、ニッケル、チタン、パラジウム、インジウム、タングステン、及び、これらの合金の一以上を例示することができる。   Examples of the material for forming the conductive mesh 40 include one or more of gold, silver, copper, platinum, aluminum, chromium, molybdenum, nickel, titanium, palladium, indium, tungsten, and alloys thereof. Can be illustrated.

図6は、図5のA−A線に対応する断面図であって、導電細線の断面形状の一例を示す図である。基材30上に、導電性メッシュ40をなす複数の導電細線41が形成されている。図示された例では、導電細線41は、基材30側の面41a、基材30の反対側の面41b及び側面41c,41dを有し、全体として略長方形の断面を有している。導電細線41の幅W、すなわち、基材30のシート面に沿った幅Wは2μm以上20μm以下とし、高さ(厚さ)H、すなわち、基材30のシート面への法線方向に沿った高さ(厚さ)Hは1μm以上60μm以下とすることが好ましい。このような寸法の導電細線41によれば、その導電細線41が十分に細線化されているので、導電性メッシュ40を効果的に不可視化することができる。   FIG. 6 is a cross-sectional view corresponding to the line AA in FIG. 5, and is a diagram illustrating an example of a cross-sectional shape of the conductive thin wire. A plurality of thin conductive wires 41 forming the conductive mesh 40 are formed on the base material 30. In the illustrated example, the conductive thin wire 41 has a surface 41 a on the base material 30 side, a surface 41 b on the opposite side of the base material 30, and side surfaces 41 c and 41 d, and has a substantially rectangular cross section as a whole. The width W of the thin conductive wire 41, that is, the width W along the sheet surface of the substrate 30 is 2 μm or more and 20 μm or less, and the height (thickness) H, that is, along the normal direction to the sheet surface of the substrate 30. The height (thickness) H is preferably 1 μm or more and 60 μm or less. According to the conductive thin wire 41 having such a dimension, since the conductive thin wire 41 is sufficiently thinned, the conductive mesh 40 can be effectively invisible.

また、導電細線41は、基材30上に設けられた第1の暗色層46、第1の暗色層46上に設けられた導電性金属層45、及び、導電性金属層45上に設けられた第2の暗色層47を含んでいる。言い換えると、導電性金属層45の表面のうち、基材30側の面を第1の暗色層46が覆っており、導電性金属層45の表面のうち、基材30と反対側の面及び両側面を第2の暗色層47が覆っている。   The conductive thin wire 41 is provided on the first dark color layer 46 provided on the base material 30, the conductive metal layer 45 provided on the first dark color layer 46, and the conductive metal layer 45. The second dark color layer 47 is included. In other words, the surface on the base material 30 side of the surface of the conductive metal layer 45 is covered with the first dark color layer 46, and the surface on the opposite side of the base material 30 among the surface of the conductive metal layer 45 and The second dark color layer 47 covers both side surfaces.

金属材料からなる導電性金属層45は、比較的高い反射率を呈する。そして、導電性メッシュ40の導電細線41をなす導電性金属層45によって光が反射されると、その反射した光が視認されるようになり、乗員の視界を妨げる場合がある。また、外部から導電性金属層45が視認されると、意匠性が低下する場合がある。そこで、暗色層46,47が、導電性金属層45の表面の少なくとも一部分に配置されている。暗色層46,47は、導電性金属層45よりも可視光の反射率が低い層であればよく、例えば黒色等の暗色の層である。この暗色層46,47によって、導電性金属層45が視認されづらくなり、乗員の視界を良好に確保することができる。また、外部から見たときの意匠性の低下を防ぐことができる。   The conductive metal layer 45 made of a metal material exhibits a relatively high reflectance. When the light is reflected by the conductive metal layer 45 that forms the conductive thin wires 41 of the conductive mesh 40, the reflected light is visually recognized and may hinder the occupant's field of view. Further, when the conductive metal layer 45 is visually recognized from the outside, the designability may be deteriorated. Therefore, the dark color layers 46 and 47 are disposed on at least a part of the surface of the conductive metal layer 45. The dark color layers 46 and 47 may be layers having a visible light reflectance lower than that of the conductive metal layer 45, and are dark color layers such as black. The dark color layers 46 and 47 make it difficult for the conductive metal layer 45 to be visually recognized, so that the occupant's field of view can be favorably secured. Moreover, the fall of the designability when seen from the outside can be prevented.

図7は、図5のA−A線に対応する断面図であって、導電細線の断面形状の他の例を示す図である。図示された例では、導電細線41は、基材30側の面41a、基材30の反対側の面41b及び側面41c,41dを有している。基材30側の面41aと基材30の反対側の面41bは平行をなしている。側面41cは、メッシュシート20のシート面の法線方向に沿って基材30から離間するにつれて側面41dに近づくようなテーパ面をなしている。側面41dも、メッシュシート20のシート面の法線方向に沿って基材30から離間するにつれて側面41cに近づくようなテーパ面をなしている。導電細線41は、全体として略台形の断面を有している。すなわち、導電細線41の幅は、メッシュシート20の法線方向に沿って基材30から離間するにつれて狭くなるように変化している。また、図6に示した例と同様、導電性金属層45の表面のうち、基材30側の面を第1の暗色層46が覆っており、導電性金属層45の表面のうち、基材30と反対側の面及び両側面を第2の暗色層47が覆っている。   FIG. 7 is a cross-sectional view corresponding to the line AA in FIG. 5 and is a diagram illustrating another example of the cross-sectional shape of the conductive thin wire. In the illustrated example, the conductive thin wire 41 has a surface 41a on the base material 30 side, a surface 41b on the opposite side of the base material 30, and side surfaces 41c and 41d. The surface 41a on the substrate 30 side and the surface 41b on the opposite side of the substrate 30 are parallel. The side surface 41 c has a tapered surface that approaches the side surface 41 d as the distance from the base material 30 increases along the normal direction of the sheet surface of the mesh sheet 20. The side surface 41d also has a tapered surface that approaches the side surface 41c as the distance from the base material 30 increases along the normal direction of the sheet surface of the mesh sheet 20. The thin conductive wire 41 has a substantially trapezoidal cross section as a whole. That is, the width of the thin conductive wire 41 changes so as to become narrower as the distance from the base material 30 increases along the normal direction of the mesh sheet 20. Similarly to the example shown in FIG. 6, the first dark color layer 46 covers the surface on the base material 30 side of the surface of the conductive metal layer 45. A second dark color layer 47 covers the surface opposite to the material 30 and both side surfaces.

なお、図7には、導電細線41が全体として略台形の断面を有して、導電細線41の幅が、メッシュシート20の法線方向に沿って基材30から離間するにつれて狭くなるように変化しているものを示したが、これに限らず、側面41c,41dが曲線で構成されていたり、多段状となっていたりしてもよい。また、メッシュシート20の法線方向に沿って基材30から離間するにつれて、部分的に導電細線41の幅が広くなる箇所があってもよい。すなわち、導電細線41の断面を全体的かつ大局的に見た場合において、導電細線41の幅が、メッシュシート20の法線方向に沿って基材30から離間するにつれて狭くなるように変化しているものであればよい。   In FIG. 7, the conductive thin wire 41 has a substantially trapezoidal cross section as a whole, and the width of the conductive thin wire 41 becomes narrower as it is separated from the base material 30 along the normal direction of the mesh sheet 20. Although what is changing was shown, it is not restricted to this, The side surfaces 41c and 41d may be comprised by the curve, or may be multistage shape. Further, there may be a portion where the width of the conductive thin wire 41 is partially increased as the distance from the base material 30 is increased along the normal direction of the mesh sheet 20. That is, when the cross section of the thin conductive wire 41 is viewed as a whole and globally, the width of the thin conductive wire 41 changes so as to become narrower as it is separated from the base material 30 along the normal direction of the mesh sheet 20. If it is,

図7に示した例では、導電細線41の幅が、メッシュシート20の法線方向に沿って基材30から離間するにつれて狭くなるように変化するように構成されているので、ガラス板11,12、接合層13,14及びメッシュシート20を積層する際に、導電性メッシュ40を確実に接合層13に埋め込むことができ、導電性メッシュ40と接合層13との界面に気泡が残留することを抑制することができる。   In the example illustrated in FIG. 7, the width of the conductive thin wire 41 is configured to change so as to become narrower as it is separated from the base material 30 along the normal line direction of the mesh sheet 20. 12. When laminating the bonding layers 13 and 14 and the mesh sheet 20, the conductive mesh 40 can be reliably embedded in the bonding layer 13, and bubbles remain at the interface between the conductive mesh 40 and the bonding layer 13. Can be suppressed.

次に、図8〜図15を参照して、メッシュシート20の製造方法の一例について説明する。図8〜図15は、メッシュシート20の製造方法の一例を順に示す断面図である。   Next, an example of a method for manufacturing the mesh sheet 20 will be described with reference to FIGS. 8-15 is sectional drawing which shows an example of the manufacturing method of the mesh sheet 20 in order.

まず、図8に示すように、基材30を準備する。基材30は、可視光線波長帯域の波長(380nm〜780nm)を透過する一般に言うところの透明である電気絶縁性の無延伸樹脂基材である。   First, as shown in FIG. 8, a base material 30 is prepared. The base material 30 is a transparent, electrically insulating, unstretched resin base material that is generally transparent and transmits a wavelength in the visible light wavelength band (380 nm to 780 nm).

次に、図9に示すように、基材30上に第1の暗色層46を設ける。例えば、電界めっき及び無電界めっきを含むめっき法、スパッタリング法、CVD法、PVD法、イオンプレーティング法、又はこれらの二以上を組み合わせた方法により、基材30上に第1の暗色層46を設けることができる。なお、第1の暗色層46の材料としては、種々の公知のものを用いることができる。例えば窒化銅、酸化銅、窒化ニッケル等が例示できる。   Next, as shown in FIG. 9, a first dark color layer 46 is provided on the substrate 30. For example, the first dark color layer 46 is formed on the substrate 30 by a plating method including electroplating and electroless plating, a sputtering method, a CVD method, a PVD method, an ion plating method, or a combination of these two or more. Can be provided. Various known materials can be used as the material for the first dark color layer 46. For example, copper nitride, copper oxide, nickel nitride and the like can be exemplified.

次に、図10に示すように、第1の暗色層46上に導電性金属層45を設ける。導電性金属層45は、上述したように、金、銀、銅、白金、アルミニウム、クロム、モリブデン、ニッケル、チタン、パラジウム、インジウム、タングステン、及び、これらの合金の一以上からなる層である。導電性金属層45は、公知の方法で形成され得る。例えば、銅箔等の金属箔を耐候性接着剤等を用いて貼着する方法、電界めっき及び無電界めっきを含むめっき法、スパッタリング法、CVD法、PVD法、イオンプレーティング法、又はこれらの二以上を組み合わせた方法を採用することができる。   Next, as shown in FIG. 10, a conductive metal layer 45 is provided on the first dark color layer 46. As described above, the conductive metal layer 45 is a layer made of one or more of gold, silver, copper, platinum, aluminum, chromium, molybdenum, nickel, titanium, palladium, indium, tungsten, and alloys thereof. The conductive metal layer 45 can be formed by a known method. For example, a method of attaching a metal foil such as copper foil using a weather resistant adhesive, a plating method including electroplating and electroless plating, a sputtering method, a CVD method, a PVD method, an ion plating method, or these A method of combining two or more can be employed.

次に、図11に示すように、導電性金属層45上に、レジスト層48を設ける。レジスト層48は、例えば特定波長域の光、例えば紫外線に対する感光性を有する樹脂層である。この樹脂層は、樹脂フィルムを貼着して形成してもよいし、流動性の樹脂をコーティングすることにより形成してもよい。また、レジスト層48の具体的な感光特性は特に限られない。例えば、レジスト層48として、光硬化型の感光材が用いられてもよく、若しくは、光溶解型の感光材が用いられてもよい。   Next, as shown in FIG. 11, a resist layer 48 is provided on the conductive metal layer 45. The resist layer 48 is a resin layer having photosensitivity to, for example, light in a specific wavelength range, for example, ultraviolet rays. This resin layer may be formed by sticking a resin film, or may be formed by coating a fluid resin. The specific photosensitive characteristics of the resist layer 48 are not particularly limited. For example, as the resist layer 48, a photocurable photosensitive material may be used, or a photodissolvable photosensitive material may be used.

その後、図12に示すように、レジスト層48をパターニングして、レジストパターン49を形成する。レジスト層48をパターニングする方法としては、公知の種々の方法が採用することができるが、この例では、レジスト層48として、特定波長域の光、例えば紫外線に対する感光性を有する樹脂層を用い、公知のフォトリソグラフィー技術を用いてパターニングしている。まず、レジスト層48上に、パターン化したい部分を開口したマスク、又は、パターン化したい部分を遮蔽したマスクを配置し、このマスクを介してレジスト層48に紫外線を照射する。その後、紫外線がマスクにより遮蔽された部分、又は、紫外線が照射された部分を現像等の手段により除去する。これにより、パターニングされたレジストパターン49を形成することができる。   Thereafter, as shown in FIG. 12, the resist layer 48 is patterned to form a resist pattern 49. As a method of patterning the resist layer 48, various known methods can be employed. In this example, a resin layer having photosensitivity to light in a specific wavelength region, for example, ultraviolet rays, is used as the resist layer 48. Patterning is performed using a known photolithography technique. First, a mask in which a portion to be patterned is opened or a mask in which a portion to be patterned is shielded is disposed on the resist layer 48, and the resist layer 48 is irradiated with ultraviolet rays through this mask. Thereafter, the portion where the ultraviolet rays are shielded by the mask or the portion irradiated with the ultraviolet rays is removed by means such as development. Thereby, the patterned resist pattern 49 can be formed.

次に、図13に示すように、レジストパターン49をマスクとして、導電性金属層45及び第1の暗色層46をエッチングする。このエッチングにより、導電性金属層45及び第1の暗色層46がレジストパターン49と略同一のパターンにパターニングされる。エッチング方法は特に限られることはなく、公知の方法が採用できる。公知の方法としては、例えば、エッチング液を用いるウェットエッチングや、プラズマエッチングなどが挙げられる。その後、図14に示すように、レジストパターン49を除去する。   Next, as shown in FIG. 13, the conductive metal layer 45 and the first dark color layer 46 are etched using the resist pattern 49 as a mask. By this etching, the conductive metal layer 45 and the first dark color layer 46 are patterned into a pattern substantially the same as the resist pattern 49. The etching method is not particularly limited, and a known method can be employed. Known methods include, for example, wet etching using an etchant, plasma etching, and the like. Thereafter, as shown in FIG. 14, the resist pattern 49 is removed.

最後に、導電性金属層45の基材30の反対側の面41b及び側面41c,41dに第2の暗色層47を形成する。第2の暗色層47は、例えば導電性金属層45をなす材料の一部分に暗色化処理(黒化処理)を施して、導電性金属層45をなしていた一部分から、金属酸化物や金属硫化物からなる第2の暗色層47を形成することができる。また、暗色材料の塗膜や、ニッケルやクロム等のめっき層等のように、導電性金属層45の表面に第2の暗色層47を設けるようにしてもよい。また、導電性金属層45の表面を粗化して第2の暗色層47を設けるようにしてもよい。   Finally, the second dark color layer 47 is formed on the surface 41b and the side surfaces 41c and 41d on the opposite side of the base material 30 of the conductive metal layer 45. For example, the second dark color layer 47 is subjected to a darkening process (blackening process) on a part of the material forming the conductive metal layer 45, and the metal oxide or metal sulfide is formed from a part of the conductive metal layer 45. A second dark color layer 47 made of a material can be formed. Alternatively, the second dark color layer 47 may be provided on the surface of the conductive metal layer 45, such as a coating film of dark color material or a plating layer of nickel or chromium. Alternatively, the second dark color layer 47 may be provided by roughening the surface of the conductive metal layer 45.

この例では、導電性金属層45の基材30の反対側の面41b及び側面41c,41dに第2の暗色層47を形成したが、これに限られず、導電性金属層45の基材30の反対側の面41bのみ、又は、導電性金属層45の側面41c,41dのみに第2の暗色層47を形成してもよい。   In this example, the second dark color layer 47 is formed on the surface 41b and the side surfaces 41c and 41d opposite to the base material 30 of the conductive metal layer 45. However, the present invention is not limited to this, and the base material 30 of the conductive metal layer 45 is not limited thereto. The second dark color layer 47 may be formed only on the opposite surface 41 b or only on the side surfaces 41 c and 41 d of the conductive metal layer 45.

導電性金属層45の基材30の反対側の面41bのみに第2の暗色層47を形成する場合は、例えば、図10に示した工程の後に、導電性金属層45上に第2の暗色層47及びレジスト層48をこの順に設け、レジスト層48をパターニングしてレジストパターン49を形成する。その後、レジストパターン49をマスクとして、第2の暗色層47、導電性金属層45及び第1の暗色層46をエッチングすればよい。   In the case where the second dark color layer 47 is formed only on the surface 41b on the opposite side of the base material 30 of the conductive metal layer 45, for example, the second metal layer 45 is formed on the conductive metal layer 45 after the step shown in FIG. A dark color layer 47 and a resist layer 48 are provided in this order, and the resist layer 48 is patterned to form a resist pattern 49. Thereafter, the second dark color layer 47, the conductive metal layer 45, and the first dark color layer 46 may be etched using the resist pattern 49 as a mask.

また、導電性金属層45の側面41c,41dのみに第2の暗色層47を形成する場合は、例えば、図13に示した工程の後に、レジストパターン49を除去せずに第2の暗色層47を形成し、その後、レジストパターン49を除去すればよい。   When the second dark color layer 47 is formed only on the side surfaces 41c and 41d of the conductive metal layer 45, for example, the second dark color layer without removing the resist pattern 49 after the step shown in FIG. 47 is formed, and then the resist pattern 49 is removed.

なお、第1の暗色層46が必要ない場合には、図9に示した、基材30上に第1の暗色層46を設ける工程を省略すればよい。   If the first dark color layer 46 is not necessary, the step of providing the first dark color layer 46 on the substrate 30 shown in FIG. 9 may be omitted.

以上のように、本実施の形態における合わせガラス10は、一対の湾曲したガラス板11,12と、一対の湾曲したガラス板11,12の間に配置されたメッシュシート20と、各ガラス板11,12とメッシュシート20との間に配置され且つガラス板11,12と前記メッシュシート20とを接合する接合層13,14と、を備えている。前記メッシュシート20は、基材30と、前記基材30上に形成された導電性メッシュ40と、を有している。導電性メッシュ40は、上述したパターニング方法のように、種々の材料および種々の方法を用いて基材30上に作製することができ、さらに、所望のパターンを高精度に付与することもできる。したがって、例えば優れた光学特性を有する合わせガラス10を作製することも可能となる。   As described above, the laminated glass 10 in the present embodiment includes the pair of curved glass plates 11 and 12, the mesh sheet 20 disposed between the pair of curved glass plates 11 and 12, and each glass plate 11. , 12 and the mesh sheet 20 and bonding layers 13 and 14 for bonding the glass plates 11 and 12 and the mesh sheet 20 to each other. The mesh sheet 20 includes a base material 30 and a conductive mesh 40 formed on the base material 30. As in the patterning method described above, the conductive mesh 40 can be produced on the base material 30 using various materials and various methods, and a desired pattern can be imparted with high accuracy. Therefore, for example, the laminated glass 10 having excellent optical characteristics can be produced.

その一方で、この合わせガラスは、接合層を介してメッシュシートをガラス板間で加熱および加圧することによって製造され得る。ただし、加熱加圧後に冷却した状態での合わせガラスにおいて、基材へしわが発生するといった不具合が生じ得ることを、本件発明者らは知見した。基材へのしわの発生は、合わせガラスの湾曲した箇所に発生しており、また、合わせガラスの湾曲の程度にあわせてしわの程度も変化する。   On the other hand, this laminated glass can be manufactured by heating and pressurizing a mesh sheet between glass plates via a bonding layer. However, the present inventors have found that in the laminated glass in a cooled state after heating and pressurization, there may be a problem that wrinkles are generated on the base material. Generation | occurrence | production of the wrinkle to a base material has generate | occur | produced in the curved location of a laminated glass, and the grade of a wrinkle changes according to the grade of the curvature of a laminated glass.

一般に、製造工程で延伸されたシート(延伸シート)は、延伸工程でシートに残留応力が生じ、このシートを融点またはガラス転移点付近まで加熱すると、この残留応力によりシートが大きく収縮する。一方、製造工程で延伸されていないシート(無延伸シート)では、延伸工程による残留応力が生じないので、シートを加熱した際のシートの収縮が抑制され得る。したがって、メッシュシート20の基材30として無延伸樹脂基材を用いることにより、基材30として延伸された基材を用いた場合に比べて、メッシュシート20へのしわの発生が効果的に防止される。   In general, in a sheet stretched in the production process (stretched sheet), a residual stress is generated in the sheet in the stretching process, and when the sheet is heated to the vicinity of the melting point or the glass transition point, the sheet is largely contracted by the residual stress. On the other hand, in a sheet that has not been stretched in the manufacturing process (non-stretched sheet), the residual stress due to the stretching process does not occur, and thus the shrinkage of the sheet when the sheet is heated can be suppressed. Therefore, by using an unstretched resin base material as the base material 30 of the mesh sheet 20, the generation of wrinkles on the mesh sheet 20 can be effectively prevented as compared with the case where a base material stretched as the base material 30 is used. Is done.

なお、このシートの収縮の程度は、加熱収縮率の絶対値の大きさで評価することができる。加熱収縮率は、JIS C 2151に規定される寸法変化率であり、所定の大きさの試験片を100℃で15分間加熱し、室温まで冷却した後の寸法変化率として定義される。加熱前の寸法をL、加熱・冷却後の寸法をLとすると、加熱収縮率S(%)は、
S=(L−L)/L×100
で表せる。
The degree of shrinkage of the sheet can be evaluated by the absolute value of the heat shrinkage rate. The heat shrinkage rate is a dimensional change rate defined in JIS C 2151, and is defined as a dimensional change rate after a test piece having a predetermined size is heated at 100 ° C. for 15 minutes and cooled to room temperature. If the dimension before heating is L 0 and the dimension after heating / cooling is L, the heat shrinkage S (%) is
S = (L 0 −L) / L 0 × 100
It can be expressed as

製造工程で延伸されていない無延伸シートの加熱収縮率の絶対値は、製造工程で延伸された延伸シートの加熱収縮率の絶対値よりも小さくなる。典型的には、無延伸シートの面内の各方向での加熱収縮率の絶対値の最大値は10%以下であり、しわの発生を確実に抑制する観点から、5%以下であることが好ましい。   The absolute value of the heat shrinkage rate of the non-stretched sheet that has not been stretched in the manufacturing process is smaller than the absolute value of the heat shrinkage rate of the stretched sheet that has been stretched in the manufacturing process. Typically, the maximum absolute value of the heat shrinkage rate in each direction in the plane of the unstretched sheet is 10% or less, and 5% or less from the viewpoint of reliably suppressing the occurrence of wrinkles. preferable.

なお、上述した実施の形態に対して様々な変更を加えることが可能である。   Note that various modifications can be made to the above-described embodiment.

例えば、メッシュシート20の導電性メッシュ40は、基材30のガラス板11側の面上ではなく、ガラス板12側の面上に設けてもよい。また、基材30のガラス板11側及びガラス板12側の両面に設けてもよい。   For example, the conductive mesh 40 of the mesh sheet 20 may be provided not on the glass plate 11 side surface of the substrate 30 but on the glass plate 12 side surface. Moreover, you may provide in the both surfaces of the glass plate 11 side and the glass plate 12 side of the base material 30. FIG.

合わせガラス10は、自動車1のリアウィンドウ、サイドウィンドウやサンルーフに用いてもよい。また、自動車以外の、鉄道、航空機、船舶、宇宙船等の乗り物の窓に用いてもよい。   The laminated glass 10 may be used for a rear window, a side window, or a sunroof of the automobile 1. Moreover, you may use for windows of vehicles other than a motor vehicle, such as a railway, an aircraft, a ship, and a spacecraft.

さらに、合わせガラス10は、乗り物以外にも、特に室内と室外とを区画する箇所、例えばビルや店舗、住宅の窓等に使用することもできる。   Furthermore, the laminated glass 10 can also be used in places other than the vehicle, in particular, in places that divide the room from the outdoors, such as buildings, stores, and house windows.

なお、以上において上述した実施の形態に対するいくつかの変形例を説明してきたが、当然に、複数の変形例を適宜組み合わせて適用することも可能である。   In addition, although the some modification with respect to embodiment mentioned above was demonstrated above, naturally, it is also possible to apply combining several modifications suitably.

以下、実施例を用いて本発明をより詳細に説明するが、本発明はこの実施例に限定されるものではない。   EXAMPLES Hereinafter, although this invention is demonstrated in detail using an Example, this invention is not limited to this Example.

以下に説明する実施例1〜3、比較例に係る合わせガラスを実際に作製して、しわの発生を確認した。合わせガラスは、上述の実施の形態で説明した合わせガラスと同様に、第1のガラス板、第1の接合層、メッシュシート、第2の接合層、及び、第2のガラス板を、この順で含むようにした。各合わせガラスにおいて、第1及び第2のガラス板、第1及び第2の接合層は、同一のものを採用した。具体的には、第1及び第2のガラス板として、縦100mm、横100mm、厚さ2mmの湾曲した青板ガラス板を用いた。第1及び第2の接合層として、縦100mm、横100mm、厚さ0.4mmのポリビニルブチラール(PVB)からなる層を利用した。   The laminated glass which concerns on Examples 1-3 and the comparative example demonstrated below was produced actually, and generation | occurrence | production of wrinkles was confirmed. The laminated glass is composed of the first glass plate, the first bonding layer, the mesh sheet, the second bonding layer, and the second glass plate in this order in the same manner as the laminated glass described in the above embodiment. I included it. In each laminated glass, the same thing was employ | adopted for the 1st and 2nd glass plate and the 1st and 2nd joining layer. Specifically, curved blue plate glass plates having a length of 100 mm, a width of 100 mm, and a thickness of 2 mm were used as the first and second glass plates. As the first and second bonding layers, layers made of polyvinyl butyral (PVB) having a length of 100 mm, a width of 100 mm, and a thickness of 0.4 mm were used.

メッシュシートは、基材と、基材上に形成されたハニカム状の導電性メッシュと、を有するようにした。導電性メッシュは、上述したフォトリソグラフィー技術により、銅箔をパターニングすることにより、作製した。導電性メッシュの導電細線は、幅10μm、高さ(厚さ)10μmとした。導電性メッシュの開口率は、80%とした。メッシュシートの導電性メッシュは、各合わせガラスの間で、共通とした。その一方で、メッシュシートの基材は、各合わせガラスの間で、次のように異なる樹脂フィルムを用いた。   The mesh sheet had a base material and a honeycomb-like conductive mesh formed on the base material. The conductive mesh was produced by patterning a copper foil by the photolithography technique described above. The conductive fine wire of the conductive mesh had a width of 10 μm and a height (thickness) of 10 μm. The opening ratio of the conductive mesh was 80%. The conductive mesh of the mesh sheet was common among the laminated glasses. On the other hand, as the base material of the mesh sheet, different resin films were used between the laminated glasses as follows.

(実施例1)
実施例1では、メッシュシートの基材として、縦110mm、横110mm、厚さ0.1mmの無延伸アクリル樹脂フィルムを用いた。面内の各方向での加熱収縮率の絶対値の最大値は、5%であった。
Example 1
In Example 1, an unstretched acrylic resin film having a length of 110 mm, a width of 110 mm, and a thickness of 0.1 mm was used as the base material of the mesh sheet. The maximum absolute value of the heat shrinkage rate in each direction in the plane was 5%.

(実施例2)
実施例2では、メッシュシートの基材として、縦110mm、横110mm、厚さ0.1mmの無延伸アモルファスポリエチレンテレフタレートを用いた。面内の各方向での加熱収縮率の絶対値の最大値は、5%であった。
(Example 2)
In Example 2, unstretched amorphous polyethylene terephthalate having a length of 110 mm, a width of 110 mm, and a thickness of 0.1 mm was used as the base material of the mesh sheet. The maximum absolute value of the heat shrinkage rate in each direction in the plane was 5%.

(実施例3)
実施例3では、メッシュシートの基材として、縦110mm、横110mm、厚さ0.1mmの無延伸ポリ塩化ビニルを用いた。面内の各方向での加熱収縮率の絶対値の最大値は、8%であった。
(Example 3)
In Example 3, unstretched polyvinyl chloride having a length of 110 mm, a width of 110 mm, and a thickness of 0.1 mm was used as the base material of the mesh sheet. The maximum absolute value of the heat shrinkage rate in each direction in the plane was 8%.

(比較例)
比較例では、メッシュシートの基材として、縦110mm、横110mm、厚さ0.025mmの一軸延伸ポリエチレンテレフタレートフィルムを用いた。面内の各方向での加熱収縮率の絶対値の最大値は、20%であった。
(Comparative example)
In the comparative example, a uniaxially stretched polyethylene terephthalate film having a length of 110 mm, a width of 110 mm, and a thickness of 0.025 mm was used as the base material of the mesh sheet. The maximum absolute value of the heat shrinkage rate in each direction in the plane was 20%.

各合わせガラスは、共通する次の方法にて作製した。上述の第1のガラス板、第1の接合層、メッシュシート、第2の接合層、及び、第2のガラス板を、大気圧中で、この順に重ね、オートクレーブ装置へ搬入した。次に、オートクレーブ装置内を減圧した後、150℃、10atmで60分間加熱・加圧した。その後、大気圧中に取り出し、室温まで冷却して合わせガラスを作製した。   Each laminated glass was produced by the following common method. The first glass plate, the first bonding layer, the mesh sheet, the second bonding layer, and the second glass plate described above were stacked in this order in the atmospheric pressure and carried into the autoclave apparatus. Next, after reducing the pressure inside the autoclave, it was heated and pressurized at 150 ° C. and 10 atm for 60 minutes. Then, it took out in atmospheric pressure, cooled to room temperature, and produced the laminated glass.

作製した実施例1〜3に係る合わせガラス、及び、比較例に係る合わせガラスについて、目視でしわの有無を判定した。実施例1〜3に係る合わせガラスについては、注意深く観察しても、しわの存在は確認できなかった。一方、比較例に係る合わせガラスについては、目視で確認できるしわが多数存在していた。   About the laminated glass which concerns on the produced Examples 1-3 and the laminated glass which concerns on a comparative example, the presence or absence of wrinkles was determined visually. Even when carefully observing the laminated glasses according to Examples 1 to 3, the presence of wrinkles could not be confirmed. On the other hand, the laminated glass according to the comparative example had many wrinkles that could be visually confirmed.

1 自動車
5 フロントウィンドウ
7 電源
10 合わせガラス
11 ガラス板
12 ガラス板
13 接合層
14 接合層
15 接続部
16 配線部
20 メッシュシート
30 基材(無延伸樹脂基材)
40 導電性メッシュ
41 導電細線
42 分岐点
43 開口
45 導電性金属層
46 第1の暗色層
47 第2の暗色層
48 レジスト層
49 レジストパターン
DESCRIPTION OF SYMBOLS 1 Car 5 Front window 7 Power supply 10 Laminated glass 11 Glass plate 12 Glass plate 13 Joining layer 14 Joining layer 15 Connection part 16 Wiring part 20 Mesh sheet 30 Base material (non-stretched resin base material)
40 conductive mesh 41 conductive thin wire 42 branch point 43 opening 45 conductive metal layer 46 first dark color layer 47 second dark color layer 48 resist layer 49 resist pattern

Claims (5)

一対の湾曲したガラス板と、
前記一対の湾曲したガラス板の間に配置されたメッシュシートと、
各ガラス板と前記メッシュシートとの間に配置され且つ当該ガラス板と前記メッシュシートとを接合する接合層と、を備え、
前記メッシュシートは、無延伸樹脂基材と、前記無延伸樹脂基材上に形成された導電性メッシュと、を有する、合わせガラス。
A pair of curved glass plates;
A mesh sheet disposed between the pair of curved glass plates;
A bonding layer disposed between each glass plate and the mesh sheet and bonding the glass plate and the mesh sheet; and
The mesh sheet is a laminated glass having an unstretched resin substrate and a conductive mesh formed on the unstretched resin substrate.
前記導電性メッシュは、導電細線を用いて形成され、
前記導電細線の幅は、前記メッシュシートの法線方向に沿って前記無延伸樹脂基材から離間するにつれて狭くなるように変化する、請求項1に記載の合わせガラス。
The conductive mesh is formed using a thin conductive wire,
2. The laminated glass according to claim 1, wherein a width of the conductive thin wire changes so as to become narrower as it is separated from the unstretched resin base material along a normal direction of the mesh sheet.
前記導電性メッシュは、導電細線を用いて形成され、
前記導電細線は、導電性金属層と、前記金属層の表面の少なくとも一部分を覆う暗色層と、を有する、請求項1または2に記載の合わせガラス。
The conductive mesh is formed using a thin conductive wire,
The laminated glass according to claim 1 or 2, wherein the thin conductive wire has a conductive metal layer and a dark color layer covering at least a part of the surface of the metal layer.
請求項1〜3のいずれか一項に記載された合わせガラスと、
前記合わせガラスの前記導電性メッシュに接続された電源と、を備える、加熱機構付きガラス。
Laminated glass according to any one of claims 1 to 3,
And a power source connected to the conductive mesh of the laminated glass.
請求項1〜3のいずれか一項に記載された合わせガラスまたは請求項4の加熱機構付きガラスを備えた乗り物。   The vehicle provided with the laminated glass as described in any one of Claims 1-3, or the glass with a heating mechanism of Claim 4.
JP2014190395A 2014-09-18 2014-09-18 Laminated glass, glass with heating mechanism and vehicle Active JP6274574B2 (en)