JP2011238862A - 太陽電池用封止膜及びこれを用いた太陽電池 - Google Patents
太陽電池用封止膜及びこれを用いた太陽電池 Download PDFInfo
- Publication number
- JP2011238862A JP2011238862A JP2010110767A JP2010110767A JP2011238862A JP 2011238862 A JP2011238862 A JP 2011238862A JP 2010110767 A JP2010110767 A JP 2010110767A JP 2010110767 A JP2010110767 A JP 2010110767A JP 2011238862 A JP2011238862 A JP 2011238862A
- Authority
- JP
- Japan
- Prior art keywords
- solar cell
- mass
- sealing film
- vinyl acetate
- ethylene
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
【解決手段】エチレン−酢酸ビニル共重合体、架橋剤及び紫外線吸収剤を含む太陽電池用封止膜であって、前記架橋剤は2,5−ジメチル−2,5−ジ(t−ブチルパーオキシ)ヘキサンであり、前記エチレン−酢酸ビニル共重合体100質量部に対して0.1〜1.2質量部含み、前記紫外線吸収剤は2−ヒドロキシ−4−n−オクトキシベンゾフェノンであり、前記エチレン−酢酸ビニル共重合体100質量部に対して0.02〜0.28質量部含むことを特徴とする太陽電池用封止膜。
【選択図】図1
Description
(1)前記2,5−ジメチル−2,5−ジ(t−ブチルパーオキシ)ヘキサンの含有量が0.3〜0.9質量部である。
(2)前記2−ヒドロキシ−4−n−オクトキシベンゾフェノンの含有量が0.02〜0.2質量部である。
(3)前記エチレン−酢酸ビニル共重合体の酢酸ビニル含有量が、前記エチレン−酢酸ビニル共重合体の質量を基準として、20〜35質量%である。
本発明に使用する架橋剤Aは、下記式(I)
本発明に使用する紫外線吸収剤Aは、下記式(II)
エチレン−酢酸ビニル共重合体(EVAとも言う)を主成分とすることで、安価であり、透明性及び柔軟性に優れる太陽電池用封止膜を形成することができる。
さらに、架橋硬化前の太陽電池用封止膜は、架橋助剤を含んでいることが好ましい。前記架橋助剤は、エチレン−酢酸ビニル共重合体の架橋密度を向上させ、封止膜の接着性及び耐久性を向上させることができる。
本発明の太陽電池用封止膜には、更に接着力を高める目的で、シランカップリング剤を含むことが好ましい。シランカップリング剤としては、γ−メタクリロキシプロピルトリメトキシシラン、γ−クロロプロピルメトキシシラン、ビニルエトキシシラン、ビニルトリス(β−メトキシエトキシ)シラン、ビニルトリアセトキシシラン、γ−グリシドキシプロピルトリメトキシシラン、γ−グリシドキシプロピルトリエトキシシラン、β−(3,4−エポキシシクロヘキシル)エチルトリメトキシシラン、ビニルトリクロロシラン、γ−メルカプトプロピルトリメトキシシラン、γ−アミノプロピルトリエトキシシラン、N−β−(アミノエチル)−γ−アミノプロピルトリメトキシシラン等を挙げることができる。特に、γ−メタクリロキシプロピルトリメトキシシランが好ましい。これらシランカップリング剤は、単独で使用しても、又は2種以上組み合わせて使用しても良い。また、シランカップリング剤の含有量は、エチレン−酢酸ビニル共重合体100質量部に対して0.01〜5質量部であることが好ましく、特に0.1〜2質量部が好ましい。
本発明の太陽電池用封止膜は、膜の種々の物性(機械的強度、透明性等の光学的特性、耐熱性、耐光性、架橋速度等)の改良あるいは調整、特に機械的強度の改良のため、必要に応じて、可塑剤、アクリロキシ基含有化合物、メタクリロキシ基含有化合物及び/又はエポキシ基含有化合物などの各種添加剤をさらに含んでいてもよい。
表1及び2に示す配合で各材料をロールミルに供給し、70℃において混練して太陽電池用封止膜組成物を調製した。前記太陽電池用封止膜組成物を、70℃においてカレンダ成形し、放冷後、太陽電池用封止膜(厚さ0.6mm)を作製した。
(1)黄色度
白色ガラス(厚さ3mm)/上記太陽電池用封止膜(厚さ0.6mm)/白色ガラス(厚さ3mm)の順で積層し、得られた積層体を真空ラミネーターにて、100℃の温度で10分間仮圧着した後、オーブンに入れ、温度155℃の条件で45分架橋させた。この積層体について、紫外線照射200時間後の黄色度(YI)を、カラーメーター(HZ−2、スガ試験機株式会社製)を用いて、JIS−K−7105(1981)に準拠して測定した。
接着力は180°ピール試験(JIS K 6854、1994年)により評価した。フロートガラス(3mm厚)/上記太陽電池用封止膜(0.6mm厚)/離形PETフィルム(75μm厚)の順で積層し、得られた積層体を真空ラミネーターにて、100℃の温度で10分間仮圧着した後、オーブンに入れ、温度155℃の条件で45分架橋させた。これを、図2に示すように、ガラス板21と太陽電池用封止膜23との間の一部を剥離して、太陽電池用封止膜23を180°折り返して引張試験機(島津製作所社製、オートグラフ)を用いて引張速度100mm/分時の引き剥がし力をガラス接着力(N/cm)として測定した。
実施例1〜10において架橋剤Aと紫外線吸収剤Aを表1に示すように、種々の添加量で配合した太陽電池用封止膜は、黄色度、ガラス接着力共に良好であった。特に、架橋剤Aを0.3〜0.9質量部、紫外線吸収剤Aを0.02〜0.2質量部配合した実施例3〜5及び7,8は黄色度が低く且つ接着性も良好であることが認められた。
12 裏面側保護部材
13A 表面側封止膜
13B 裏面側封止膜
14 太陽電池用セル
21 ガラス板
23 太陽電池用封止膜
Claims (5)
- エチレン−酢酸ビニル共重合体、架橋剤及び紫外線吸収剤を含む太陽電池用封止膜であって、
前記架橋剤は2,5−ジメチル−2,5−ジ(t−ブチルパーオキシ)ヘキサンであり、前記エチレン−酢酸ビニル共重合体100質量部に対して0.1〜1.2質量部含み、
前記紫外線吸収剤は2−ヒドロキシ−4−n−オクトキシベンゾフェノンであり、前記エチレン−酢酸ビニル共重合体100質量部に対して0.02〜0.28質量部含むことを特徴とする太陽電池用封止膜。 - 前記2,5−ジメチル−2,5−ジ(t−ブチルパーオキシ)ヘキサンの含有量が0.3〜0.9質量部である請求項1に記載の太陽電池用封止膜。
- 前記2−ヒドロキシ−4−n−オクトキシベンゾフェノンの含有量が0.02〜0.2質量部である請求項1又は2に記載の太陽電池用封止膜。
- 前記エチレン−酢酸ビニル共重合体の酢酸ビニル含有量が、前記エチレン−酢酸ビニル共重合体の質量を基準として、20〜35質量%である請求項1〜3の何れか1項に記載の太陽電池用封止膜。
- 請求項1〜4の何れか1項に記載の太陽電池用封止膜を用いたことを特徴とする太陽電池。