CN203284488U - 一种铝合金阳极氧化装置 - Google Patents
一种铝合金阳极氧化装置 Download PDFInfo
- Publication number
- CN203284488U CN203284488U CN2013202775335U CN201320277533U CN203284488U CN 203284488 U CN203284488 U CN 203284488U CN 2013202775335 U CN2013202775335 U CN 2013202775335U CN 201320277533 U CN201320277533 U CN 201320277533U CN 203284488 U CN203284488 U CN 203284488U
- Authority
- CN
- China
- Prior art keywords
- conductive
- aluminium alloy
- anode
- aluminum alloy
- cell body
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Abstract
本实用新型公开了一种铝合金阳极氧化装置,包括电解槽体、电解液、阴极导电装置、阳极导电装置和挂具,所述阴极导电装置采用铅板,所述阳极导电装置包括软连接、铜座、导电铜板和冷却水管。本实用新型的优点是阴极导电装置采用铅板,不易被电解液腐蚀,减少了材料的浪费;阳极导电装置采用软连接,导电铜座上增加导电铜板,导电性能更好,电流稳定从而使铝合金表面形成的氧化膜质量效果更好;通过冷却水管的冷却,导电铜板产生的热量能够及时散掉一部分,减少了电烧蚀带来的材料浪费。
Description
技术领域
本实用新型属于铝合金加工技术领域,特别涉及一种铝合金阳极氧化装置。
背景技术
铝合金建筑型材是当今门窗和幕墙主要的结构材料,在世界范围内广泛应用。铝合金挤压型材(未经表面处理)外观单一,并且在潮湿大气中容易腐蚀,因而很难满足建筑材料高装饰性和强耐侯性的要求,为了提高装饰效果、增强抗腐蚀性及延长使用寿命,铝型材一般都要进行表面处理。因此,表面处理是铝合金建筑型材生产的一道必不可少且极为重要的工序, 在工业上越来越广泛地采用阳极氧化的方法,在铝合金表面形成致密的氧化膜,以显著改善铝合金的耐腐蚀性、耐磨性和装饰性能。
目前铝合金阳极氧化处理是利用电化学方法,在适当电解液中,以铝合金合金零件为阳极,以不锈钢、铝等金属为阴极,电解液经常为酸性溶液,经过长时间的浸泡,不锈钢和铝等金属会与酸性溶液发生反应,造成材料的浪费;铝合金氧化过程中需要的电流很大,设备经会产生很大的热量, 极易产生电烧蚀,损坏导电装置,从而影响电流的稳定性,导致铝合金表面形成的氧化膜质量不良。
本实用新型要解决的技术问题是提供一种带有不易腐蚀的阴极板、导电性能良好、能够减少电烧蚀的铝合金阳极氧化装置。
发明内容
为解决上述现有铝合金阳极氧化处理过程中材料浪费、导电性能差,电烧蚀的问题,本实用新型采用如下技术方案:
本实用新型提供一种铝合金阳极氧化装置,包括电解槽体、电解液、阴极导电装置、阳极导电装置和挂具,所述阴极导电装置和阳极导电装置设置在电解槽体上,所述电解液设置在电解槽体内,所述挂具横跨于电解槽体上。
作为对本实用新型的改进,所述阴极导电装置为铅板。
作为对本实用新型的进一步改进,所述阳极导电装置包括软连接、铜座、导电铜板和冷却水管,所述软连接采用铜板螺栓拼接与弹簧连接,所述导电铜板置于铜座上,所述冷却水管与铜座连接。
本实用新型的有益效果在于:本实用新型阴极板采用铅板,不易被电解液腐蚀,减少了材料的浪费;阳极装置采用软连接,高度可调节,同时铜座上增加导电铜板,导电性能更好,电流稳定,从而使铝合金表面形成的氧化膜质量效果更好;通过冷却水管的冷却,导电铜板产生的热量能够适当散掉,减少了材料被烧坏带来的损失。
附图说明
图1为本实用新型一种实施例的结构示意图。
图2为本实用新型阳极导电装置的局部结构示意图。
具体实施方式
下面结合附图详细说明本实用新型的优选实施例。
请参阅图1,一种铝合金阳极氧化装置,包括电解槽体1、电解液2、阴极导电装置3、阳极导电装置4和挂具5,所述阴极导电装置3和阳极导电装置4设置在电解槽体1上,所述电解液2设置在电解槽体1内,所述挂具5横跨于电解槽体1上。电解槽体1形状为方形,一次加工能放置更多的铝材,电解液采用硫酸,因为它具有适用于铝及大部分铝合金的阳极氧化处理,处理电压较低,耗电少;处理过程不必改变电压周期;硫酸电解时,释放大量的热量,无需加装加热设备,这不仅减少了企业投入,且硫酸对人身的危害较铬酸小,货源广,价格低等优点。
本实用新型中,阴极导电装置3采用铅板,铅板的电位低,在硫酸中不易腐蚀,从而减少了材料的浪费,提高了企业的经济效益。
请参阅图2,所述阳极导电装置包括软连接41、铜座42、导电铜板43和冷却水管44,所述软连接采用铜板螺栓拼接与弹簧装置,所述导电铜板43置于铜座42上,所述冷却水管44与铜座42连接。通过螺栓拼接与弹簧装置的配合使铜座42与导电铜板43,导电铜板43与挂具5紧密接触,有利于电流稳定,得到质量较好的铝合金阳极氧化膜。阳极氧化过程中电流比较大,铜座42与导电铜板43接触部位产生的热量比较大,所述冷却水管44通有循环冷却水,起到了降温的作用,减少了电烧蚀带来的材料损坏。
Claims (3)
1.一种铝合金阳极氧化装置,其特征在于:包括电解槽体(1)、电解液(2)、阴极导电装置(3)、阳极导电装置(4)和挂具(5),所述阴极导电装置(3)和阳极导电装置(4)设置在电解槽体(1)上,所述电解液(2)设置在电解槽体(1)内,所述挂具(5)横跨于电解槽体(1)上。
2.根据权利要求1所述的一种铝合金阳极氧化装置,其特征在于:所述阴极导电装置(2)为铅板。
3.根据权利要求1所述的一种铝合金阳极氧化装置,其特征在于:所述阳极导电装置(4)包括软连接(41)、铜座(42)、导电铜板(43)和冷却水管(44),所述软连接(41)采用铜板螺栓拼接与弹簧连接,所述导电铜板(43)置于铜座(42)上,所述冷却水管(44)与铜座(42)连接。