CN103275772A - Environmentally-friendly fuel oil saving material and preparation method thereof - Google Patents
Environmentally-friendly fuel oil saving material and preparation method thereof Download PDFInfo
- Publication number
- CN103275772A CN103275772A CN2013101914180A CN201310191418A CN103275772A CN 103275772 A CN103275772 A CN 103275772A CN 2013101914180 A CN2013101914180 A CN 2013101914180A CN 201310191418 A CN201310191418 A CN 201310191418A CN 103275772 A CN103275772 A CN 103275772A
- Authority
- CN
- China
- Prior art keywords
- fuel oil
- saving material
- friendly fuel
- environment friendly
- rare earth
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to an environmentally-friendly fuel oil saving material and a preparation method thereof. The environmentally-friendly fuel oil saving material comprises the following components in percentage by weight: 30-40 percent of rock glaciers, 25-35 percent of tourmaline, 20-25 percent of silica, 5-10 percent of kaolin and 3-5 percent of rare earth oxide. The rare-earth oxide is a mixture comprising lanthanum oxide, cerium oxide, yttrium oxide and neodymium oxide. The preparation method of the environmentally-friendly fuel oil saving material comprises the following steps of: 1, grinding all the raw materials into fine powder with the diameter of 10mu m-15mu m and uniformly mixing the fine powder; and 2, adding water into the fine powder, stirring and drying, and sintering at 1050-1100 DEG C for about 1 hour to prepare small balls with the diameter of 10mm-12mm. Tests prove that the environmentally-friendly fuel oil saving material is directly submerged in fuel oil, and after five hours, the fuel saving rate can reach 14-26 percent.
Description
Technical field
The invention belongs to environment-friendly type fuel-economizing admixture class, be specifically related to a kind of environment friendly fuel material and preparation method thereof.
Background technology
Along with fast development and the living standards of the people of modern society improve constantly, the demand of the energy is continued to increase, especially the consumption of petrol and diesel oil increases day by day.Simultaneously, people are also more and more higher to environmental quality requirement, particularly to the promising concern of the discharging of pollutent in the atmosphere.Because the fossil class energy belongs to Nonrenewable energy resources, the service efficiency, the minimizing air pollution emission that therefore improve existing fuel oil are significant.
Existing fuel-saving technique is mainly the oil-saving agent that adds solubility to fuel oil, and the additive of this class polycomponent synthetic is consumed simultaneously with fuel oil in use.Wherein in the part economizing additive owing to contain metal-salt, after burning, can form residue, thereby cause the increase infringement engine of mechanical friction.Owing to contain elements such as halogen family and nitrogen, sulphur, phosphorus, when burning, can cause the pollution aspect the obnoxious flavoures such as hydrogen iodide, hydrogen fluoride, nitrogen peroxide, and the three wastes in the production process of economizing additive are also more serious in the another kind of economizing additive.In addition, also has a class based on the application of the physics fuel-saving technique of tourmalinite (Tourmaline), wherein the Chinese patent publication number is that " Verdelite fuel-economizing material and the tourmalinite material fuel-economizing product " of CN101225783A related to the goods that utilize tourmalinite and other materials to make all kinds of oil fuel pipes, realizes energy-saving function; Number be in the utility model patent " tourmaline ceramic automobile fuel-economizing device " of CN202659380U at Granted publication, related to the fuel-economizing device that utilizes tourmalinite to make.Their preparation and use are all comparatively complicated, also need change the original pipeline of automobile or circuit, increase unpredictability.
Summary of the invention
1, technical problem to be solved:
Existing fuel economizing technology increases the solubility oil-saving agent, but contains residue, can damage engine, uses the physics fuel-saving technique of tourmalinite, and preparation preparation and use are all comparatively complicated, also needs the original pipeline of automobile or circuit are changed.
2, technical scheme:
In order to overcome the above problems, the invention provides a kind of environment friendly fuel oil-saving material, its raw material is formed and weight percent is: ice apron 30~40%, Tourmaline stone 25~35%, silica 20~25%, kaolin 5~10%, rare earth oxide 3~5%.
Described rare earth oxide is the mixture of lanthanum trioxide, cerium oxide, yttrium oxide and Neodymium trioxide.
A kind of preparation method of environment friendly fuel oil-saving material may further comprise the steps: the first step: various raw materials are ground to form fine powder and the evenly mixing that diameter is 10 μ m~50 μ m; Second step: make the bead that diameter is 10mm~12mm about 1 hour at 1050 ℃~1100 ℃ following sintering after adding water stirring and drying.
3, beneficial effect:
It is that it directly is dipped in the fuel oil that environment friendly fuel oil-saving material provided by the invention is used, and after 5 hours, rate of economizing gasoline can reach 14~26%.
Embodiment
The present invention is described in detail below in conjunction with embodiment.
Embodiment one
Raw material is formed and weight percent is: ice apron 30%, Tourmaline stone 35%, silica 25%, kaolin 7%, rare earth oxide 3%.
Embodiment two
Raw material is formed and weight percent is: ice apron 35%, Tourmaline stone 30%, silica 25%, kaolin 7%, rare earth oxide 3%.
Embodiment three
Raw material is formed and weight percent is: ice apron 40%, Tourmaline stone 25%, silica 25%, kaolin 7%, rare earth oxide 3%.
Embodiment four
Raw material is formed and weight percent is: ice apron 35%, Tourmaline stone 35%, silica 20%, kaolin 7%, rare earth oxide 3%.
Embodiment five
Raw material is formed and weight percent is: ice apron 40%, Tourmaline stone 30%, silica 20%, kaolin 7%, rare earth oxide 3%.
Embodiment six
Raw material is formed and weight percent is: ice apron 38%, Tourmaline stone 27%, silica 25%, kaolin 7%, rare earth oxide 3%.
Fuel oil of the present invention is preferably gasoline or diesel oil.
Environment friendly fuel oil-saving material of the present invention is applied in the fuel oil, by adding 1g in every 1000g fuel oil.
Environment friendly fuel oil-saving material of the present invention is applied in the fuel oil, can place fuel container for a long time, when oil-saving effect obviously descends, its taking-up can be reused after calcination
Form and the preparation method by the raw material of above six embodiment, prepare corresponding environmental protection fuel economizing material and test:
Be divided into test group and control group, the oil-saving material that six embodiment of the present invention are prepared is by adding 1g and soaking 5 hours in every 1000g fuel oil, and the control group fuel oil does not add any material.
Carry out the full load platform with 188F type petrol motor and No. 93 gasoline and drive test, rate of economizing gasoline and the exhaust emissions amount behind the oil-saving material used in detection, and each test repeats 10 times, and the averaging of income result is as follows:
From above data as can be seen: it is that it directly is dipped in the fuel oil that environment friendly fuel oil-saving material provided by the invention is used, and after 5 hours, rate of economizing gasoline can reach 14~26%.
Claims (10)
1. environment friendly fuel oil-saving material is characterized in that: it is formed and weight percent is: ice apron 30~40%, Tourmaline stone 25~35%, silica 20~25%, kaolin 5~10%, rare earth oxide 3~5%.
2. environment friendly fuel oil-saving material as claimed in claim 1, it is characterized in that: described rare earth oxide is the mixture of lanthanum trioxide, cerium oxide, yttrium oxide and Neodymium trioxide.
3. environment friendly fuel oil-saving material as claimed in claim 1 or 2, it is characterized in that: fuel oil is gasoline or diesel oil.
4. environment friendly fuel oil-saving material as claimed in claim 1 or 2 is characterized in that: it is formed and weight percent is: ice apron 30%, Tourmaline stone 35%, silica 25%, kaolin 7%, rare earth oxide 3%.
5. environment friendly fuel oil-saving material as claimed in claim 1 or 2: it is characterized in that: it is formed and weight percent is: ice apron 35%, Tourmaline stone 30%, silica 25%, kaolin 7%, rare earth oxide 3%.
6. environment friendly fuel oil-saving material as claimed in claim 1 or 2: it is characterized in that: it is formed and weight percent is: ice apron 40%, Tourmaline stone 25%, silica 25%, kaolin 7%, rare earth oxide 3%.
7. environment friendly fuel oil-saving material as claimed in claim 1 or 2: it is characterized in that: it is formed and weight percent is: ice apron 35%, Tourmaline stone 35%, silica 20%, kaolin 7%, rare earth oxide 3%.
8. environment friendly fuel oil-saving material as claimed in claim 1 or 2: it is characterized in that: it is formed and weight percent is: ice apron 40%, Tourmaline stone 30%, silica 20%, kaolin 7%, rare earth oxide 3%.
9. environment friendly fuel oil-saving material as claimed in claim 1 or 2: it is characterized in that: it is formed and weight percent is: ice apron 38%, Tourmaline stone 27%, silica 25%, kaolin 7%, rare earth oxide 3%.
10. the preparation method of an environment friendly fuel oil-saving material may further comprise the steps: the first step: various raw materials are ground to form fine powder and the evenly mixing that diameter is 10 μ m~50 μ m; Second step: make the bead that diameter is 10mm~12mm about 1 hour at 1050 ℃~1100 ℃ following sintering after adding water stirring and drying.