Nothing Special   »   [go: up one dir, main page]

CN102665378A - Method for achieving mutual conduction of inner and outer surfaces of plastic component - Google Patents

Method for achieving mutual conduction of inner and outer surfaces of plastic component Download PDF

Info

Publication number
CN102665378A
CN102665378A CN2012101555821A CN201210155582A CN102665378A CN 102665378 A CN102665378 A CN 102665378A CN 2012101555821 A CN2012101555821 A CN 2012101555821A CN 201210155582 A CN201210155582 A CN 201210155582A CN 102665378 A CN102665378 A CN 102665378A
Authority
CN
China
Prior art keywords
plastic parts
hole
technology
aperture
filler
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012101555821A
Other languages
Chinese (zh)
Other versions
CN102665378B (en
Inventor
陈德智
蒋海英
郑兵
李立忠
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Shanghai Amphenol Airwave Communication Electronics Co Ltd
Original Assignee
Shanghai Amphenol Airwave Communication Electronics Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Shanghai Amphenol Airwave Communication Electronics Co Ltd filed Critical Shanghai Amphenol Airwave Communication Electronics Co Ltd
Priority to CN201210155582.1A priority Critical patent/CN102665378B/en
Publication of CN102665378A publication Critical patent/CN102665378A/en
Application granted granted Critical
Publication of CN102665378B publication Critical patent/CN102665378B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses a method for achieving mutual conduction of inner and outer surfaces of a plastic component. The method comprises the following steps of: drilling a through hole at a preset position of the plastic component by using laser; and activating and depositing a metal layer in a specific area to achieve the electric conduction of the inner and outer surfaces of the plastic component. Because the aperture of the through hole is very small, a filler is not required to be filled in the through hole, and the outer surface of the plastic component can be directly coated with a coating layer. Due to the small aperture, the through hole can be directly covered by the coating layer. The through hole is applied to the field, and because the minimum aperture of the through hole can reach 0.02mm, the filler is not required to be filled in the through hole; and therefore, the cost is saved and traces left on the outer surface when the filler is not completely removed and the surface is not well leveled are avoided. The method can be also applied to a production technique for fabricating a mobile terminal antenna onto a shell.

Description

Realize the method for plastic parts inner surface and the mutual conducting of outer surface
Technical field
The present invention is applied to the electronic equipment manufacturing, portable terminal, multimedia equipment field; Can be applied to antenna and other use LDS and other with metal attached to the field of plastic parts spare surface as connection line or decorative effect.
Background technology
At present based on carry out on the plastic parts LDS (the direct moulding of LASER DIRECT STRUCTURE laser, or be called laser direct forming) or LSP (LASER SELECTIVE PLATING laser is selected plating) or other directly or between be connected on the technology of plating on the plastic parts.
With LDS is example, uses the LDS technology of three-dimensional laser system can the cad data of Antenna Design be transferred on the model antenna holder, perhaps directly transfers on the device structure, for example the portable terminal lid.Adopt follow-up lacquer spraying technique to decorate to antenna surface.The LDS technology adopts laser beam at the resinous complex three-dimensional piece surface initiative of LDS antenna pattern.This technological key advantage comprises can change design fast, and can on three-dimensional surface, formulate antenna structure.It is integrated that the LDS technology also allows the user to carry out higher levels of product, reduces parts and reduce cost.
The mutual conducting of plastic parts inner surface and outer surface if desired, its technology are perforates on plastic parts, and then carry out surface active and deposit going up metal level.For example mobile terminal antenna is a lot of now uses LDS or LSP technology to be made on the shell, and antenna is connected to inside from the outside just need via hole.In order to guarantee outward appearance and sealing property, often need use filler that the hole is blocked up, use coating to improve outward appearance then.Technology filler commonly used has glue at present, can be instant drying adhesive, AB glue, and UV glue or caulk compound are with the hole shutoff.
The method of concrete realization plastic parts inner surface and the mutual conducting of outer surface is shown in Figure 1A to Fig. 1 E:
Step 1: utilize mould on plastic rubber bracket, to carry out perforate, the aperture is generally greater than 0.5MM, and it is bigger that the hole on the plastic parts often will be opened; The mould upper and lower mould can be run into so here; Can influence die life if the hole is too small, and be easy to generate overlap, cause that thus fraction defective raises.
Step 2: laser activation and depositing metal layers in the specific region.Under the general situation, be in the hole, carry out laser activation around the hole, and deposition goes up metal level.Realize the effect of inner surface and the mutual conducting of outer surface through metal level.
Step 3: use the filler filling vias, in general, filler has glue, can be instant drying adhesive, AB glue, and UV glue or caulk compound are with the hole shutoff.
Step 4: on the customer-oriented one side of plastic parts, the filler of protrusion is removed, so that this surface energy is smooth.
Step 5: the one side after this is smooth covers and goes up coating.
Though above-mentioned process can realize the effect of plastic parts inner surface and the mutual conducting of outer surface, possibly there is following defective:
At first: it is bigger that the hole on the plastic parts often will be opened, and for example greater than 0.50, because the mould upper and lower mould can be run into here, can influence die life if the hole is too small, and be easy to generate overlap.And these through holes can influence sealing property, advance dust easily like portable terminal, and influence outward appearance.
Secondly: like the needs plug-hole; Then because that the hole often is difficult to very greatly to accomplish to cooperate with face on every side is fine; Such as in step 4, removing the clean or excessive filler of removing of filler; On coating, can leave a trace and cause bad order, especially on the coating of high glaze, usually the bad order rate is high.
Once more: the filler that plug-hole needs can increase cost of material, and production process is long, and unfavorable to environment.
Summary of the invention
First purpose of the present invention is to provide a kind of method that realizes plastic parts inner surface and the mutual conducting of outer surface, to solve the technical problem that need come filler opening with filler with the mould punching in the prior art.
Second purpose of the present invention is to provide a kind of mobile terminal antenna to be produced on the technology of shell, to solve the technical problem that need come filler opening with filler with the mould punching in the prior art.
A kind of method that realizes plastic parts inner surface and the mutual conducting of outer surface may further comprise the steps:
On the predefined position of plastic parts, beat via;
Activation and depositing metal layers in the specific region realize that through metal level plastic parts inner surface and outer surface conduct;
Said specific region comprises the plastic parts inner surface and the outer surface region of hole inwall and intercommunicating pore inwall at least.
Do not use the filler filler opening in the said via.
Preferably, the direct applying coating of one of the inner surface of said working of plastics and outer surface or inner surface and outer surface.
Preferably, the aperture is at the 0.02-0.50 millimeter;
Preferably, the method for beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
A kind of mobile terminal antenna is produced on the technology on the housing, may further comprise the steps:
Mobile terminal antenna uses the technology comprise LDS and LSP, direct plated metal on housing, and make antenna be connected to enclosure interior from outside through via, wherein via further comprises:
Beating via on the predefined position on the housing, the aperture is at 0.02-0.50MM;
Activation and depositing metal layers in the specific region realize that through metal plastic parts inner surface and outer surface conduct and do not use the filler plug-hole, and said specific region comprises the plastic parts inner surface and the outer surface region of hole inwall and intercommunicating pore inwall at least.
This technology also is included in inner surface and the outer surface or the direct applying coating of one of inner surface and outer surface of shell.
This technology also comprises: the method for beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
A kind of technology of mobile terminal shell may further comprise the steps:
On predefined position on the housing, beat and be used for the via that the multimedia equipment acoustic cavity loses heart, the aperture is at 0.02-0.50MM;
The method of beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
Compared with prior art, the present invention has the following advantages:
A kind of method that realizes plastic parts inner surface and the mutual conducting of outer surface may further comprise the steps: on the predefined position of plastic parts, beat via, the aperture of via is at 0.02-0.50MM; Activation and depositing metal layers in the specific region are realized conducting of plastic parts inner surface and outer surface through metal level; Said specific region comprises at least, the inner surface of the plastic parts of the inwall of via and connection via inwall and the zone of outer surface.And, because the via aperture is very little, need not use the filler filler opening in the hole of said via, can be at the direct applying coating of the outer surface of plastic parts, thereby these vias since the aperture is very little can coated direct covering; The present invention will beat via application this area and come; Because beating via aperture minimum can reach 0.02 millimeter; So need not use filler to fill via, not only save cost, and it is clean and surfacingization is bad at the left vestige of outer surface to have avoided removing filler.The present invention can also be applied to the method and a kind of mobile terminal antenna is produced in the production technology on the shell; Be that mobile terminal antenna uses LDS or LSP technology to be made on the shell, and make antenna be connected to enclosure from housing exterior through above via step.
On predefined position on the housing, beat and be used for the via that the multimedia equipment acoustic cavity loses heart, the aperture is at 0.02-0.50MM.Because the via aperture is very little, it is disappointing that this design can reach, and balance sound chamber inner and outer air pressure because the hole is very little, can also reach the requirement that does not influence acoustical behavior.
Description of drawings
Figure 1A to Fig. 1 E is respectively the block diagram that realizes plastic parts inner surface and the mutual conducting of outer surface in the prior art;
Fig. 2 A to Fig. 2 C realizes a kind of performing step figure of plastic parts inner surface and the mutual conducting of outer surface for the present invention.
Embodiment
See also Fig. 2 A-Fig. 2 C method that realizes plastic parts inner surface and the mutual conducting of outer surface, may further comprise the steps:
On the predefined position of plastic parts, beat via, the aperture is in the 0.02-0.5MM scope, and preferably, the aperture is about 0.05-0.3; The method of beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
Activation and depositing metal layers 12 in the specific region realize that through metal level 12 plastic parts inner surface and outer surface conduct and do not use the filler plug-hole, and said specific region comprises the plastic parts inner surface and the outer surface region of hole inwall and intercommunicating pore inwall at least.
The hole is generally taper shape, and the little other end of an end is big.This instance also is included in the surface-coated of the one side at least coating 13 of plastic parts.The via aperture is very little, need not use the filler plug-hole in the hole of said via, can be at the direct applying coating 13 of the outer surface of plastic parts, and these vias are because the aperture is very little of all right coated direct covering; The present invention will beat via application this area and come; Because beating via aperture minimum can reach 0.02 millimeter; So need not use filler to fill via, not only save cost, and it is clean and surfacingization is bad at the left vestige of outer surface to have avoided removing filler.
A kind of mobile terminal antenna is produced on the technology of shell, may further comprise the steps:
Mobile terminal antenna uses LDS or LSP technology to be made on the production technology of shell, and makes antenna be connected to enclosure from housing exterior through via hole, and wherein via hole further comprises:
On the predefined position of shell, beat via, the aperture is 0.02-0.50MM (preferably, 0.05-0.3mm can be adopted in the aperture); Activation and depositing metal layers or plating in the specific region realize that through metal plastic parts inner surface and outer surface conduct and do not use the filler filler opening., said specific region comprises the plastic parts inner surface and the outer surface region of hole inwall and intercommunicating pore inwall at least.And, in the surface-coated coating (can be the high glaze layer) of one side at least of shell.Laser is got outer surface from the inboard of shell.On plastic parts, punch, the aperture can be selected arbitrarily, as 0.3,0.1, even can arrive 0.02. and beat behind the hole according to the technological operation of plated metal on the different plastic parts, and last plated metal is for example changed plating or plated metal in piece surface comprises aperture.Give an example, like LDS technology, concrete steps are injection mo(u)ldings, beat via, and the laser activation figure is changed copper facing, and nickel or gold are last as needing lacquered surface directly to spray paint.
A kind of technology of mobile terminal shell may further comprise the steps:
On predefined position on the housing, beat and be used for the via that the multimedia equipment acoustic cavity loses heart, the aperture is at 0.02-0.50MM;
The method of beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
More than the disclosed several specific embodiments that are merely the application, but the application is not limited thereto, any those skilled in the art can think variation, all should drop in the application's the protection range.

Claims (9)

1. a method that realizes plastic parts inner surface and the mutual conducting of outer surface is characterized in that, may further comprise the steps:
On the predefined position of plastic parts, beat via;
Activation and depositing metal layers in the specific region realize that through metal level plastic parts inner surface and outer surface conduct;
Said specific region comprises the plastic parts inner surface and the outer surface region of hole inwall and intercommunicating pore inwall at least.
2. the method for claim 1 is characterized in that, also comprises, one of the inner surface of said working of plastics and outer surface or inner surface and outer surface be applying coating directly.
3. the method for claim 1 is characterized in that, the via aperture is at the 0.02-0.50 millimeter.
4. the method for claim 1 is characterized in that, the method for beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
5. a mobile terminal antenna is produced on the technology on the housing, it is characterized in that, may further comprise the steps:
Mobile terminal antenna uses the technology comprise LDS and LSP, direct plated metal on housing, and make antenna be connected to enclosure interior from outside through via, wherein via further comprises:
Beating via on the predefined position on the housing, the aperture is at 0.02-0.50MM;
Activation and depositing metal layers in the specific region realize that through metal plastic parts inner surface and outer surface conduct, and said specific region comprises the plastic parts inner surface and the outer surface region of hole inwall and intercommunicating pore inwall at least.
6. technology as claimed in claim 5 is characterized in that, also is included in inner surface and the outer surface or the direct applying coating of one of inner surface and outer surface of shell.
7. technology as claimed in claim 5 is characterized in that the method for beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
8. the technology of a mobile terminal shell is characterized in that, may further comprise the steps:
On predefined position on the housing, beat and be used for the via that the multimedia equipment acoustic cavity loses heart, the aperture is at 0.02-0.50MM.
9. technology as claimed in claim 8 is characterized in that the method for beating via comprises laser drilling, ultrasonic drilling, mechanical punching wherein at least a.
CN201210155582.1A 2012-05-18 2012-05-18 Realize the method for plastic parts inner surface and the mutual conducting of outer surface Active CN102665378B (en)