Nothing Special   »   [go: up one dir, main page]

CN107163797A - High-temperature resistant coating for vertical and horizontal basin - Google Patents

High-temperature resistant coating for vertical and horizontal basin Download PDF

Info

Publication number
CN107163797A
CN107163797A CN201710493186.2A CN201710493186A CN107163797A CN 107163797 A CN107163797 A CN 107163797A CN 201710493186 A CN201710493186 A CN 201710493186A CN 107163797 A CN107163797 A CN 107163797A
Authority
CN
China
Prior art keywords
vertical
temperature resistant
resistant coating
horizontal basin
defoamer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710493186.2A
Other languages
Chinese (zh)
Inventor
柏建荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Taicang Youlian Drying And Grinding Equipment Co Ltd
Original Assignee
Taicang Youlian Drying And Grinding Equipment Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Taicang Youlian Drying And Grinding Equipment Co Ltd filed Critical Taicang Youlian Drying And Grinding Equipment Co Ltd
Priority to CN201710493186.2A priority Critical patent/CN107163797A/en
Publication of CN107163797A publication Critical patent/CN107163797A/en
Pending legal-status Critical Current

Abstract

The present invention discloses a kind of high-temperature resistant coating for vertical and horizontal basin, comprises the following steps:The liquid materials such as water, dispersant, defoamer, preservative, silicone modified polyester resin, epoxy resin, amino resins are put into dispersion tank first, stir, coloring pigment and extender pigment are put into successively under stirring, and accelerated scattered 20 40 minutes;Emulsion is put into paint mixing tank, after being let down with 35 times of water, add the auxiliary agents such as thickener, PH conditioning agents, antifreezing agent, coalescents, defoamer, stirring 15 minutes, to substantially uniformity, the high-temperature resistant coating for vertical and horizontal basin is obtained, the present invention provides a kind of high-temperature resistant coating for vertical and horizontal basin, with having excellent heat resistance, adhesive force and acid proof advantage.

Description

High-temperature resistant coating for vertical and horizontal basin
Technical field
The present invention relates to a kind of high-temperature resistant coating for vertical and horizontal basin.
Background technology
Use equipment under some hot environments, such as:The blast pipe of automobile, motorcycle, chimney etc., due to being chronically at height In warm rugged environment, the service life reduction of equipment is caused, therefore it need to be protected.Conventional method is sprayed coating.And Traditional anticorrosive coating is due to non-refractory, and the life-span is shorter under the high temperature conditions, and containing a large amount of metallic compounds, it is not only dirty Environment is contaminated, and it is harmful to human body.Therefore how to prepare a kind of fire resistant anticorrosive paint be those skilled in the art always The problem of making great efforts to solve.
The content of the invention
The present invention provide it is a kind of have excellent heat resistance, adhesive force and acid resistance advantage for vertical and horizontal basin High-temperature resistant coating.
The technical scheme is that:A kind of high-temperature resistant coating for vertical and horizontal basin, comprises the following steps:First will The liquid materials such as water, dispersant, defoamer, preservative, silicone modified polyester resin, epoxy resin, amino resins input point Dissipate in tank, stir, put into coloring pigment and extender pigment successively under stirring, and accelerate scattered 20-40 minutes; Emulsion is put into paint mixing tank, after being let down with 3-5 times of water, thickener, PH conditioning agents, antifreezing agent, coalescents, froth breaking is added The auxiliary agents such as agent, stir 15 minutes, to substantially uniformity, obtain the high-temperature resistant coating for vertical and horizontal basin.
In a preferred embodiment of the present invention, the speed of agitator should be controlled in 200-400r/min.
In a preferred embodiment of the present invention, the overall component of each composition of the liquid material accounts for 30%, dispersant for water and accounted for 2%th, defoamer, which accounts for 3%, preservative and accounts for 5%, silicone modified polyester resin and account for 30%, epoxy resin and account for 15%, amino resins, accounts for 15%.
A kind of high-temperature resistant coating for vertical and horizontal basin of the present invention, with having excellent heat resistance, adhesive force and resistance to Acid advantage.
Embodiment
Presently preferred embodiments of the present invention is described in detail below so that advantages and features of the invention can be easier to by It will be appreciated by those skilled in the art that apparent clearly being defined so as to be made to protection scope of the present invention.
Wherein, comprise the following steps:First by water, dispersant, defoamer, preservative, silicone modified polyester resin, ring In the liquid materials such as oxygen tree fat, amino resins input dispersion tank, stir, by coloring pigment and constitution face under stirring Material is put into successively, and is accelerated scattered 20-40 minutes;Emulsion is put into paint mixing tank, after being let down with 3-5 times of water, thickening is added The auxiliary agents such as agent, PH conditioning agents, antifreezing agent, coalescents, defoamer, are stirred 15 minutes, to substantially uniformity, obtain being used for vertical crouch The high-temperature resistant coating of formula basin.
Further illustrate, the speed of agitator should be controlled in 200-400r/min, each composition of liquid material totally divides Measure to account for 30%, dispersant for water and account for 2%, defoamer and account for 3%, preservative and account for 5%, silicone modified polyester resin and account for 30%, epoxy resin Account for 15%, amino resins and account for 15%.
Further illustrating, the high-temperature resistant coating requirement for vertical and horizontal basin is heatproof high temperature, and heatproof will reach 1700 DEG C, using pyrosol, water-based inorganic self-curing heat-resisting paint, its physical property, chemical property and performance reach state Border advanced level.The base-material and filler of the coating are constituted by heat-resisting, non-ignitable inorganic matter.Contain a large amount of OH active groups in base-material Group, it with filler in active component and steel active surface fast reaction, generate the inorganic polymer of three-dimensional structure.Wherein have The high-temperature resistant coating for vertical and horizontal basin of machine series(High-temperature plastic)Mostly using organosilicon as carrier, its maximum temperature is general No more than 400 degrees Celsius, it will be carbonized or soften more than this temperature, and inorganic serial high-temperature-resistant adhesive is all At least 1000 degrees Celsius of high temperature, wherein inorganic zinc silicate high temperature resistant E06-500 can be born, widely used, shallow layer can rise To good anti-oxidation corrosion-resistant effect, thick coating can not only play good anti-oxidation corrosion-resistant effect, can also play To heat insulation and preservation effect.Metallurgical furnace, quartz heating-pipe plating can be widely used in as coating materials such as ceramics, glass, metals In vain, coal-burning power plant's pulverized coal preparation system anti-impact corrosive wear coated coating, automobile engine spark plug ceramic coating anti-carbon deposition, steel mark Many industrial circles such as knowledge, safety glass LOGO marks, pyroceram ink, Aero-Space.Cold spraying is in glass, pottery The body surfaces such as porcelain, metal, low temperature drying or normal temperature self-drying, the adhesive force with surface are very good, hard wear resistant damage resistant, no Cracking, function admirable.The present invention provides a kind of high-temperature resistant coating for vertical and horizontal basin, with there is excellent heat resistance, attached Put forth effort and acid proof advantage.
The embodiment of the present invention, but protection scope of the present invention is not limited thereto, it is any to be familiar with this area Technical staff disclosed herein technical scope in, the change or replacement that can be expected without creative work should all be contained Cover within protection scope of the present invention.Therefore, the protection model that protection scope of the present invention should be limited with claims Enclose and be defined.

Claims (3)

1. a kind of high-temperature resistant coating for vertical and horizontal basin, it is characterised in that:Comprise the following steps:First by water, dispersant, In the liquid materials such as defoamer, preservative, silicone modified polyester resin, epoxy resin, amino resins input dispersion tank, stirring Uniformly, coloring pigment and extender pigment are put into successively under stirring, and accelerated scattered 20-40 minutes;In paint mixing tank Emulsion is put into, after being let down with 3-5 times of water, the auxiliary agents such as thickener, PH conditioning agents, antifreezing agent, coalescents, defoamer are added, Stirring 15 minutes, to substantially uniformity, obtains the high-temperature resistant coating for vertical and horizontal basin.
2. the high-temperature resistant coating according to claim 1 for vertical and horizontal basin, it is characterised in that:The speed of agitator should Control is in 200-400r/min.
3. the high-temperature resistant coating according to claim 1 for vertical and horizontal basin, it is characterised in that:The liquid material is each Composition totality component is that water accounts for 30%, dispersant and accounts for 2%, defoamer and account for 3%, preservative and account for 5%, silicone modified polyester resin and accounts for 30%th, epoxy resin accounts for 15%, amino resins and accounts for 15%.
CN201710493186.2A 2017-06-26 2017-06-26 High-temperature resistant coating for vertical and horizontal basin Pending CN107163797A (en)