- Prior art keywords
- sealed membrane
- lid
- pulling
- piece
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Landscapes
- Closures For Containers (AREA)
Abstract
The invention discloses a cover easy to tear and a manufacturing method thereof. The cover easy to tear comprises a cover body provided with an object taking hole, a sealing film and a gummed layer, wherein the sealing film is provided with a sealing film body and a pull sheet, and the gummed layer is arranged on the pull sheet or the sealing film body and used for adhering the pull sheet to the sealing film body. The manufacturing method of the cover easy to tear comprises the steps that a gloss oil layer is formed on the outer surface of aluminum foil and subjected to drying treatment; a heat-seal layer is formed on the inner surface of the aluminum foil; a cursor is printed on the outer surface of the aluminum foil or the gloss oil layer; a gummed area is determined according to the position of the cursor and the gummed layer is formed; the aluminum foil is cut into a shape of the required sealing film, and the gummed layer is located on the pull sheet and/or the sealing film body; the cover body is covered with the sealing film, and the object taking hole of the cover body is sealed; the pull sheet is turned over onto the sealing film body; and the pull sheet adheres to the sealing film body through the gummed layer. The cover easy to tear and the manufacturing method thereof solve the technical problem that a sealing film cracks easily due to a pull sheet and sealing film connection mode in the prior art and have the advantage that the sealing film is not prone to cracks through combination of the pull sheet and the sealing film.
Description
Technical field
The invention belongs to pot type packing technique field, particularly a kind of Easy tearing lid and manufacture method thereof.
Background technology
The lid of current packing tin for foodstuff normally adopts iron sheet or aluminium skin to make, and encloses line of weakness at tank body one, by pulling the draw ring on lid to be torn along line of weakness by lid, thus can take out the article in tank interior.The lid of this structure, tears the larger power of needs when opening from indentation, and it is very inconvenient to open; And indentation place is sharper keen, the easy scratching fingers when taking out the article inside tank body.For this reason, at pot type packaging field, there is the Easy tearing lid made with aluminum foil sealing film, although this Easy tearing lid is torn than being easier to, easily there is the situation that pulling-on piece outwards tilts when but aluminum foil sealing film main body is fitted on lid, to cause pulling-on piece accidental in manufacturing line or follow-up intermediate links, or aluminum foil sealing film is surprisingly torn, thus cause the sealing effectiveness of Easy tearing lid to tank body poor, the problem such as easily cause the article in tank contaminated or unrestrained.
In order to overcome above-mentioned defect, the Easy tearing lid that a kind of aluminum foil sealing film is made has been there is in prior art, pulling-on piece arranges lug boss/recess, the corresponding setting recess/lug boss that fasten corresponding to the lug boss/recess on pulling-on piece in aluminum foil sealing film main body, by the riveted between lug boss and recess, realize pulling-on piece and turn down combination that is rear and aluminum foil sealing film main body.Although this mode can avoid pulling-on piece outwards to tilt and pulling-on piece outwards tilts the problems such as caused sealing effectiveness difference, but the structure of this lug boss/recess, just can must make by mould being pressed on aluminum foil sealing film main body and pulling-on piece, and mould is to the compacting of aluminum foil sealing film, easily cause aluminum foil sealing film to crack even to break, aluminum foil sealing film is caused damage, is unfavorable for the carrying out of subsequent technique; In addition, in the riveted and the process that is separated of lug boss and recess, also can damage aluminium foil because stress concentrates.
Summary of the invention
For this reason, technical matters to be solved by this invention is to overcome existing mode pulling-on piece and sealed membrane are riveted together, easily cause sealed membrane to crack even to break, to the hurtful defect of sealed membrane, thus the Easy tearing lid and manufacture method thereof that provide the combination of a kind of pulling-on piece and sealed membrane not easily to cause sealed membrane to crack even to break.
For solving the problems of the technologies described above, a kind of Easy tearing lid of the present invention, comprises
Lid, is provided with and gets thing hole;
Sealed membrane, comprise sealed membrane body and the pulling-on piece being arranged on sealed membrane body edges place, get described in sealed membrane body seal cover cap is contained on thing hole, pulling-on piece can be folded on described sealed membrane body under external force;
Also comprise rubberised layer, described rubberised layer is arranged on described pulling-on piece and/or described sealed membrane body, bonding with described sealed membrane body for the pulling-on piece that will be folded on described sealed membrane body.
Described rubberised layer area occupied is less than the area of described pulling-on piece.
The shape of described rubberised layer is circular or oval or rectangle or triangle.
Described sealed membrane is disposed with gloss oil layer, aluminium foil layer and hot sealing layer from outside to inside, and described hot sealing layer is heat-sealing glue-line or PE film.
Described lid comprises metal substrate.
The outside face of described metal substrate is provided with external coating, and/or the inside face of metal substrate is provided with internal coating.
Described metal substrate is taggers tin, or Tinfree Steelor TFS, or aluminium sheet.
The manufacture method of a kind of Easy tearing lid of the present invention, comprises following steps:
The outside face of aluminium foil is formed gloss oil layer;
The inside face of aluminium foil forms hot sealing layer;
The outside face or gloss oil layer of aluminium foil print out cursor;
Glue bearing areas is determined in position according to cursor, forms rubberised layer in glue bearing areas;
Aluminium foil is cut into the shape of required sealed membrane, described sealed membrane comprises sealed membrane body and is arranged on the pulling-on piece at sealed membrane body edges place, and described rubberised layer is positioned on described pulling-on piece and/or described sealed membrane body;
Described sealed membrane seal cover cap is contained in getting on the lid in thing hole, and gets thing hole described in sealing;
Pulling-on piece is folded on described sealed membrane body;
Described pulling-on piece is bondd by described rubberised layer and described sealed membrane body.
Described rubberised layer area occupied is less than the area of described pulling-on piece.
Described hot sealing layer adopts heat-seal adhesive to be formed, and when adopting heat-seal adhesive to form described hot sealing layer, first heat-seal adhesive is coated on the inside face of described aluminium foil, then carries out drying process, to form hot sealing layer.
The described inside face first heat-seal adhesive being coated in described aluminium foil is formed in the step of hot sealing layer, and application rate is no more than 50 ms/min; In withering step, baking temperature is 100-250 DEG C.
PE film is adopted to form described hot sealing layer, when adopting PE film to form described hot sealing layer, first at the inside face application of adhesive of described aluminium foil, carry out drying process again, then the hot pressing of PE film being compounded in described aluminium foil scribbles in the one side of adhesives, again the aluminium foil being compounded with PE film is placed on curing chamber and carries out slaking, to form hot sealing layer.
In the step of drying process, by the aluminium foil being coated with adhesives with the speed being no more than 50 ms/min without a break successively through 50-60 DEG C, 60-70 DEG C, 70-80 DEG C three sections of baking ovens;
The hot pressing of PE film be compounded in the step that described aluminium foil scribbles in the one side of adhesives, hot pressing temperature is 50-70 DEG C;
Carry out in the step of slaking the aluminium foil being compounded with PE film being placed on curing chamber, the temperature of curing chamber is 50-55 DEG C, curing time >=72h.
The outside face of aluminium foil is formed in the step of gloss oil layer, upper ray velocity is no more than 50 ms/min, and carries out drying process in upper photoreduction process, and the temperature of dry process is 100-250 DEG C.
The manufacture method of a kind of Easy tearing lid of the present invention, also comprises the step forming described lid, is specially:
Subpunch swaging becomes lid element body;
By downward for the outer rim of described lid element body rounding limit, make the outer rim of described lid element body forms groove;
Injecting glue in described groove;
Become to get thing hole in lid element body upper punch swaging;
The process of rounding limit is carried out to described thing hole of getting.
Be contained in described sealed membrane seal cover cap with getting on the lid in thing hole, and getting in the step in thing hole described in sealing, adopt the mode of heat-sealing, the sealing temperatures of heat-sealing is 180-250 DEG C, and sealing time is 1-2 second.
Described sealed membrane seal cover cap to be contained in getting on the lid in thing hole, and before getting the step in thing hole described in sealing, first to carry out sealing between sealed membrane and described lid and locating.
After being folded to by pulling-on piece on described sealed membrane body, embossed is carried out to described sealed membrane main body and described pulling-on piece.
Technique scheme of the present invention has the following advantages compared to existing technology:
(1) Easy tearing lid of the present invention, by arranging rubberised layer on described pulling-on piece and/or described sealed membrane body, by bonding with described sealed membrane body for the pulling-on piece be folded on described sealed membrane body, realize the combination of described pulling-on piece and described sealed membrane body, arranging in rubberised layer and bonding process, described sealed membrane body and described pulling-on piece not easily crack, and not easily break, described sealed membrane body and described pulling-on piece effectively can be kept not to suffer damage, ensure normally to use.
(2) Easy tearing lid of the present invention, described rubberised layer area occupied is less than the area of described pulling-on piece.When described pulling-on piece is bonded together by rubberised layer and described sealed membrane body, pulling force can be applied by the region at described pulling-on piece without rubberised layer, pull open described pulling-on piece, that removes between described pulling-on piece with described sealed membrane body is bonding, and then convenient by pulling described pulling-on piece that described sealed membrane is peeled off described lid.
(3) manufacture method of Easy tearing lid of the present invention, by printing out cursor on the outside face of aluminium foil, glue bearing areas is determined in position according to cursor, rubberised layer is formed in glue bearing areas, then pulling-on piece is folded on described sealed membrane body, described pulling-on piece is bondd by described rubberised layer and described sealed membrane body, realize the combination of described pulling-on piece and described sealed membrane body, arranging in rubberised layer and bonding process, described sealed membrane body and described pulling-on piece not easily crack, not easily break, described sealed membrane body and described pulling-on piece can be effectively kept not to suffer damage, ensure normal use.
(4) manufacture method of Easy tearing lid of the present invention, can make the outer rim of lid smooth on the outer rim downward rounding limit of described lid element body, reduce and damage user; In described groove, injecting glue can make described lid having good sealing effectiveness with during tank body involution; Described thing hole of getting is carried out to the process of rounding limit can to get the peritreme in thing hole smooth, comes to harm when avoiding user to get thing.
(5) manufacture method of Easy tearing lid of the present invention, is contained in described sealed membrane seal cover cap with getting on the lid in thing hole, and before getting the step in thing hole described in sealing, first carries out sealing between sealed membrane and described lid and locates.First can position before described sealed membrane and described lid are carried out heat sealing like this, ensure the accuracy of involution.
(6) manufacture method of Easy tearing lid of the present invention, after being folded to by pulling-on piece on described sealed membrane body, carries out embossed to described sealed membrane main body and described pulling-on piece.Embossed can make the outward appearance of described sealed membrane more attractive in appearance, enhances described sealing film strength simultaneously.
Accompanying drawing explanation
In order to make content of the present invention be more likely to be clearly understood, below according to a particular embodiment of the invention and by reference to the accompanying drawings, the present invention is further detailed explanation, wherein
Fig. 1 is the Easy tearing lid of embodiment 1, pulling-on piece not with the view of sealed membrane bulk adhesive;
Fig. 2 is the view of the Easy tearing lid of embodiment 1, pulling-on piece and sealed membrane bulk adhesive;
Fig. 3 is in the manufacture method of the Easy tearing lid of embodiment 2, the position relationship schematic diagram of cursor and rubberised layer.
In figure, Reference numeral is expressed as: 1-lid, and 11-gets thing hole, 2-sealed membrane, 21-sealed membrane body, 22-pulling-on piece, 3-rubberised layer, 4-cursor.
Detailed description of the invention
Below with reference to accompanying drawing, following examples are used to be further elaborated the present invention.
Embodiment 1
Consult Fig. 1 and Fig. 2, a kind of Easy tearing lid of the present invention, comprises
Lid 1, is provided with and gets thing hole 11;
Sealed membrane 2, comprise sealed membrane body 21 and the pulling-on piece 22 being arranged on sealed membrane body 21 edge, get described in sealed membrane body 21 seal cover cap is contained on thing hole 11, pulling-on piece 22 can be folded on described sealed membrane body 21 under external force;
Also comprise rubberised layer 3, described rubberised layer 3 is arranged on described pulling-on piece 22 and/or described sealed membrane body 21, bonding with described sealed membrane body 21 for the pulling-on piece 22 that will be folded on described sealed membrane body 21.In described rubberised layer, the concrete form of glue can be multiple, such as, can be heat-seal adhesive, also can be hot melt adhesive.
Easy tearing lid of the present invention applies to mount cover on tank body, to realize sealing to tank body and unlatching.In the storage or transportation of tank body, by described rubberised layer 3, described pulling-on piece 22 is bonded on described sealed membrane body 21, thus described pulling-on piece 22 can not outwards be tilted, make described pulling-on piece 22 difficult drop-off, described sealed membrane body 21 not easily occurs by the situation of surprisingly tearing, and ensure that tank body is at the sealing effectiveness stored or in transportation; When needing the article in edible or use tank body, by applying pulling force on described pulling-on piece 22, described pulling-on piece 22 is separated with described sealed membrane body 21, and pass through pulling-on piece 22 described in outside pull-up further, make described sealed membrane peel off described lid 1, thus the article inside tank body can be taken out.
Easy tearing lid of the present invention, by arranging rubberised layer 3 on described pulling-on piece 22 and/or described sealed membrane body 21, by bonding with described sealed membrane body 21 for the pulling-on piece 22 be folded on described sealed membrane body 21, realize the combination of described pulling-on piece 22 and described sealed membrane body 21, arranging in rubberised layer 3 and bonding process, described sealed membrane body 21 and described pulling-on piece 22 not easily crack, not easily break, described sealed membrane body 21 and described pulling-on piece 22 effectively can be kept not to suffer damage, ensure normally to use.
Described rubberised layer 3 area occupied is less than the area of described pulling-on piece 22.When described pulling-on piece 22 is bonded together with described sealed membrane body 21 by rubberised layer 3, pulling force can be applied by the region at described pulling-on piece 22 without rubberised layer 3, pull open described pulling-on piece 22, that removes between described pulling-on piece 22 with described sealed membrane body 21 is bonding, and then convenient by pulling described pulling-on piece 22 that described sealed membrane 2 is peeled off described lid 1.In addition, the shape of described rubberised layer 3 can be circular, and also can be oval, square, triangle etc., can select according to demand flexibly, simple and practical, and the shape of the preferred described rubberised layer of the present embodiment is circular.
Described sealed membrane 2 is disposed with gloss oil layer, aluminium foil layer and hot sealing layer from outside to inside, and described hot sealing layer is heat-sealing glue-line or PE film.Wherein, when described Easy tearing lid mounts cover after on tank body, described hot sealing layer and described inner tank wall surround the inner space of described tank body.
Described pulling-on piece 22 is one-body molded with described sealed membrane body 21.
Described sealed membrane body 21 and described pulling-on piece 22 are provided with embossing.Embossing can make the outward appearance of described sealed membrane 2 more attractive in appearance, enhances the intensity of described sealed membrane 2 simultaneously.
Described lid 1 comprises metal substrate, and the concrete form of described metal substrate can be multiple, such as, can be taggers tin, or Tinfree Steelor TFS, or aluminium sheet.Wherein sheet steel refers to that thickness is not more than the steel plate of 3 millimeters.The preferred described metal substrate of the present embodiment is taggers tin.
Further, external coating can also be set at the outside face of described metal substrate, or internal coating is set at the inside face of described metal substrate, also external coating can be set for the outside face of described metal substrate, internal coating be set at the inside face of described metal substrate simultaneously.
Embodiment 2
The present embodiment provides a kind of manufacture method of Easy tearing lid, comprises following steps:
S1: print out cursor 4 on the outside face of aluminium foil;
S2: glue bearing areas is determined in the position according to cursor 4, forms rubberised layer 3 in glue bearing areas;
S3: form gloss oil layer on the outside face of aluminium foil, gloss oil layer does not hide cursor 4; If gloss oil layer is transparence, gloss oil layer also can hide cursor 4;
S4: form hot sealing layer on the inside face of aluminium foil; Described hot sealing layer adopts heat-seal adhesive to be formed, and when adopting heat-seal adhesive to form described hot sealing layer, first heat-seal adhesive is coated on the inside face of described aluminium foil, then carries out drying process, to form hot sealing layer;
S5: shape aluminium foil being cut into required sealed membrane 2, described sealed membrane 2 comprises sealed membrane body 21 and is arranged on the pulling-on piece 22 of sealed membrane body 21 edge, and described rubberised layer 3 is positioned on described pulling-on piece 22 and described sealed membrane body 21;
S6: described sealed membrane 2 seal cover cap is contained in getting on the lid 1 in thing hole 11, and get thing hole 11 described in sealing;
S7: pulling-on piece 22 is folded on described sealed membrane body 21;
S8: described pulling-on piece 22 is bondd with described sealed membrane body 21 by described rubberised layer 3.
Wherein, step S6 also can be arranged after step s8.
The manufacture method of described Easy tearing lid of the present invention, by printing out cursor 4 on the outside face of aluminium foil, glue bearing areas is determined in position according to cursor 4, rubberised layer 3 is formed in glue bearing areas, then pulling-on piece 22 is folded on described sealed membrane body 21, described pulling-on piece 22 is bondd with described sealed membrane body 21 by described rubberised layer 3, realize the combination of described pulling-on piece 22 and described sealed membrane body 21, arranging in rubberised layer 3 and bonding process, described sealed membrane body 21 and described pulling-on piece 22 not easily crack, not easily break, described sealed membrane body 21 and described pulling-on piece 22 can be effectively kept not to suffer damage, ensure normal use.
In step s3, the outside face of aluminium foil is formed in the step of gloss oil layer, upper ray velocity is 50 ms/min, and baking temperature is 250 DEG C.
In step s 4 which, in the step on the described inside face first heat-seal adhesive being coated in described aluminium foil, application rate is 40 ms/min; In withering step, baking temperature is 100 DEG C.
In step s 5, described rubberised layer 3 also only can be positioned at described pulling-on piece 22 and described sealed membrane body 21 on one of them.
In step s 5, described rubberised layer 3 area occupied is less than the area of described pulling-on piece 22.
Before step S6, first carry out sealing between sealed membrane 2 and described lid 1 and locate.First can position before described sealed membrane 2 is carried out heat sealing with described lid 1 like this, ensure the accuracy of involution.
In step s 6, adopt the mode of heat-sealing, the sealing temperatures of heat-sealing is 180 DEG C, and sealing time is 2 seconds.
After step S7, embossed is carried out to described sealed membrane body 21 and described pulling-on piece 22.Embossed can make the outward appearance of described sealed membrane 2 more attractive in appearance, enhances the intensity of described sealed membrane 2 simultaneously.
The manufacture method of Easy tearing lid provided by the present invention, also comprises the step forming described lid 1, is specially:
Subpunch swaging becomes lid element body;
By downward for the outer rim of described lid element body rounding limit, make the outer rim of described lid element body forms groove;
Injecting glue in described groove;
Become to get thing hole 11 in lid element body upper punch swaging;
The process of rounding limit is carried out to described thing hole 11 of getting.
Lid formation method of the present invention, can make the outer rim of lid smooth on the outer rim downward rounding limit of described lid element body, reduce and damage user; In described groove, injecting glue can make described lid 1 having good sealing effectiveness with during tank body involution; Described thing hole 11 of getting is carried out to the process of rounding limit can to get the peritreme in thing hole smooth, comes to harm when avoiding user to get thing.
The forming step of described lid 1 was carried out before step S6.
Embodiment 3
The present embodiment provides a kind of manufacture method of Easy tearing lid, comprises following steps:
S1: print out cursor 4 on the outside face of aluminium foil;
S2: glue bearing areas is determined in the position according to cursor 4, forms rubberised layer 3 in glue bearing areas;
S3: form gloss oil layer on the outside face of aluminium foil;
S4: form hot sealing layer on the inside face of aluminium foil; Described hot sealing layer adopts PE film to form described hot sealing layer, when adopting PE film to form described hot sealing layer, first at the inside face application of adhesive of described aluminium foil, carry out drying process again, then the hot pressing of PE film being compounded in described aluminium foil scribbles in the one side of adhesives, again the aluminium foil being compounded with PE film is placed on curing chamber and carries out slaking, to form hot sealing layer;
S5: shape aluminium foil being cut into required sealed membrane 2, described sealed membrane 2 comprises sealed membrane body 21 and is arranged on the pulling-on piece 22 of sealed membrane body 21 edge, and described rubberised layer 3 is positioned on described pulling-on piece 22 and described sealed membrane body 21;
S6: described sealed membrane 2 seal cover cap is contained in getting on the lid 1 in thing hole 11, and get thing hole 11 described in sealing;
S7: pulling-on piece 22 is folded on described sealed membrane body 21;
S8: described pulling-on piece 22 is bondd with described sealed membrane body 21 by described rubberised layer 3.
Wherein, step S6 also can be arranged after step s8.
In step s3, the outside face of aluminium foil is formed in the step of gloss oil layer, upper ray velocity is 45 ms/min, and baking temperature is 200 DEG C.
In step s 4 which,
In the step of drying process, by be coated with adhesives aluminium foil with the speed of 40 ms/min without a break successively through 50 DEG C, 60 DEG C, 70 DEG C three sections of baking ovens;
The hot pressing of PE film be compounded in the step that described aluminium foil scribbles in the one side of adhesives, hot pressing temperature is 50 DEG C;
Carry out in the step of slaking the aluminium foil being compounded with PE film being placed on curing chamber, the temperature of curing chamber is 50 DEG C, and the curing time is 96h.
In step s 5, described rubberised layer 3 also only can be positioned at described pulling-on piece 22 and described sealed membrane body 21 on one of them.
In step s 5, described rubberised layer 3 area occupied is less than the area of described pulling-on piece 22.
Before step S6, first carry out sealing between sealed membrane 2 and described lid 1 and locate.
In step s 6, adopt the mode of heat-sealing, the sealing temperatures of heat-sealing is 200 DEG C, and sealing time is 1.5 seconds.
After step S7, embossed is carried out to described sealed membrane body 21 and described pulling-on piece 22.
The manufacture method of Easy tearing lid provided by the present invention, also comprises the step forming described lid 1, is specially:
Subpunch swaging becomes lid element body;
By downward for the outer rim of described lid element body rounding limit, make the outer rim of described lid element body forms groove;
Injecting glue in described groove;
Become to get thing hole 11 in lid element body upper punch swaging;
The process of rounding limit is carried out to described thing hole 11 of getting.
The forming step of described lid 1 was carried out before step S6.
Embodiment 4
The present embodiment provides a kind of manufacture method of Easy tearing lid, comprises following steps:
S1: form gloss oil layer on the outside face of aluminium foil;
S2: form hot sealing layer on the inside face of aluminium foil; Described hot sealing layer adopts heat-seal adhesive to be formed, and when adopting heat-seal adhesive to form described hot sealing layer, first heat-seal adhesive is coated on the inside face of described aluminium foil, then carries out drying process, to form hot sealing layer;
S3: print out cursor 4 on the outside face of aluminium foil;
S4: glue bearing areas is determined in the position according to cursor 4, forms rubberised layer 3 in glue bearing areas;
S5: shape aluminium foil being cut into required sealed membrane 2, described sealed membrane 2 comprises sealed membrane body 21 and is arranged on the pulling-on piece 22 of sealed membrane body 21 edge, and described rubberised layer 3 is positioned on described pulling-on piece 22 and described sealed membrane body 21;
S6: described sealed membrane 2 seal cover cap is contained in getting on the lid 1 in thing hole 11, and get thing hole 11 described in sealing;
S7: pulling-on piece 22 is folded on described sealed membrane body 21;
S8: described pulling-on piece 22 is bondd with described sealed membrane body 21 by described rubberised layer 3.
Wherein, step S6 also can be arranged after step s8.
In step sl, the outside face of aluminium foil is formed in the step of gloss oil layer, upper ray velocity is 40 ms/min, and baking temperature is 150 DEG C.
In step s 2, in the step on the described inside face first heat-seal adhesive being coated in described aluminium foil, application rate is 50 ms/min; In withering step, baking temperature is 250 DEG C.Described baking temperature also can be 200 DEG C.
In step s 5, described rubberised layer 3 also only can be positioned at described pulling-on piece 22 and described sealed membrane body 21 on one of them.
In step s 5, described rubberised layer 3 area occupied is less than the area of described pulling-on piece 22.
Before step S6, first carry out sealing between sealed membrane 2 and described lid 1 and locate.
In step s 6, adopt the mode of heat-sealing, the sealing temperatures of heat-sealing is 220 DEG C, and sealing time is 1 second.
After step S7, embossed is carried out to described sealed membrane body 21 and described pulling-on piece 22.
The manufacture method of Easy tearing lid provided by the present invention, also comprises the step forming described lid 1, is specially:
Subpunch swaging becomes lid element body;
By downward for the outer rim of described lid element body rounding limit, make the outer rim of described lid element body forms groove;
Injecting glue in described groove;
Become to get thing hole 11 in lid element body upper punch swaging;
The process of rounding limit is carried out to described thing hole 11 of getting.
The forming step of described lid 1 was carried out before step S6.
Embodiment 5
The present embodiment provides a kind of manufacture method of Easy tearing lid, comprises following steps:
S1: form gloss oil layer on the outside face of aluminium foil;
S2: form hot sealing layer on the inside face of aluminium foil; Described hot sealing layer adopts PE film to form described hot sealing layer, when adopting PE film to form described hot sealing layer, first at the inside face application of adhesive of described aluminium foil, carry out drying process again, then the hot pressing of PE film being compounded in described aluminium foil scribbles in the one side of adhesives, again the aluminium foil being compounded with PE film is placed on curing chamber and carries out slaking, to form hot sealing layer;
S3: print out cursor 4 on the outside face of aluminium foil;
S4: glue bearing areas is determined in the position according to cursor 4, forms rubberised layer 3 in glue bearing areas;
S5: shape aluminium foil being cut into required sealed membrane 2, described sealed membrane 2 comprises sealed membrane body 21 and is arranged on the pulling-on piece 22 of sealed membrane body 21 edge, and described rubberised layer 3 is positioned on described pulling-on piece 22 and described sealed membrane body 21;
S6: described sealed membrane 2 seal cover cap is contained in getting on the lid 1 in thing hole 11, and get thing hole 11 described in sealing;
S7: pulling-on piece 22 is folded on described sealed membrane body 21;
S8: described pulling-on piece 22 is bondd with described sealed membrane body 21 by described rubberised layer 3.
Wherein, step S6 also can be arranged after step s8.
In step sl, the outside face of aluminium foil is formed in the step of gloss oil layer, upper ray velocity is 35 ms/min, and baking temperature is 250 DEG C.
In step s 2,
In the step of drying process, by be coated with adhesives aluminium foil with the speed of 50 ms/min without a break successively through 60 DEG C, 70 DEG C, 80 DEG C three sections of baking ovens; The temperature of described three sections of baking ovens also can be followed successively by 55 DEG C, 65 DEG C, 75 DEG C;
The hot pressing of PE film be compounded in the step that described aluminium foil scribbles in the one side of adhesives, hot pressing temperature is 70 DEG C; Described hot pressing temperature also can be 60 DEG C;
Carry out in the step of slaking the aluminium foil being compounded with PE film being placed on curing chamber, the temperature of curing chamber is 55 DEG C, and the curing time is 72h.The temperature of described curing chamber also can be 52 DEG C.
In step s 5, described rubberised layer 3 also only can be positioned at described pulling-on piece 22 and described sealed membrane body 21 on one of them.
In step s 5, described rubberised layer 3 area occupied is less than the area of described pulling-on piece 22.
Before step S6, first carry out sealing between sealed membrane 2 and described lid 1 and locate.
In step s 6, adopt the mode of heat-sealing, the sealing temperatures of heat-sealing is 250 DEG C, and sealing time is 1 second.
After step S7, embossed is carried out to described sealed membrane body 21 and described pulling-on piece 22.
The manufacture method of Easy tearing lid provided by the present invention, also comprises the step forming described lid 1, is specially:
Subpunch swaging becomes lid element body;
By downward for the outer rim of described lid element body rounding limit, make the outer rim of described lid element body forms groove;
Injecting glue in described groove;
Become to get thing hole 11 in lid element body upper punch swaging;
The process of rounding limit is carried out to described thing hole 11 of getting.
The forming step of described lid 1 was carried out before step S6.
Obviously, above-described embodiment is only for clearly example being described, and the restriction not to embodiment.For those of ordinary skill in the field, can also make other changes in different forms on the basis of the above description.Here exhaustive without the need to also giving all embodiments.And thus the apparent change of extending out or variation be still among the protection domain of the invention.
Claims (18)
1. an Easy tearing lid, comprises
Lid (1), is provided with and gets thing hole (11);
Sealed membrane (2), comprise sealed membrane body (21) and be arranged on the pulling-on piece (22) of sealed membrane body (21) edge, get on thing hole (11) described in sealed membrane body (21) seal cover cap is contained in, pulling-on piece (22) can be folded on described sealed membrane body (21) under external force;
It is characterized in that:
Also comprise rubberised layer (3), described rubberised layer (3) is arranged on described pulling-on piece (22) and/or described sealed membrane body (21), bonding with described sealed membrane body (21) for the pulling-on piece (22) that will be folded on described sealed membrane body (21).
2. Easy tearing lid according to claim 1, is characterized in that: described rubberised layer (3) area occupied is less than the area of described pulling-on piece (22).
3. Easy tearing lid according to claim 2, is characterized in that: the shape of described rubberised layer (3) is circular or oval or rectangle or triangle.
4. the Easy tearing lid according to any one of claim 1-3, is characterized in that: described sealed membrane (2) is disposed with gloss oil layer, aluminium foil layer and hot sealing layer from outside to inside, and described hot sealing layer is heat-sealing glue-line or PE film.
5. the Easy tearing lid according to any one of claim 1-4, is characterized in that: described lid (1) comprises metal substrate.
6. Easy tearing lid according to claim 5, is characterized in that: the outside face of described metal substrate is provided with external coating, and/or the inside face of metal substrate is provided with internal coating.
7. the Easy tearing lid according to claim 5 or 6, is characterized in that: described metal substrate is taggers tin, or Tinfree Steelor TFS, or aluminium sheet.
8. a manufacture method for Easy tearing lid, is characterized in that: comprise following steps:
The outside face of aluminium foil is formed gloss oil layer;
The inside face of aluminium foil forms hot sealing layer;
The outside face or gloss oil layer of aluminium foil print out cursor (4);
Glue bearing areas is determined in position according to cursor (4), forms rubberised layer (3) in glue bearing areas;
Aluminium foil is cut into the shape of required sealed membrane (2), described sealed membrane (2) comprises sealed membrane body (21) and is arranged on the pulling-on piece (22) of sealed membrane body (21) edge, and described rubberised layer (3) is positioned on described pulling-on piece (22) and/or described sealed membrane body (21);
Described sealed membrane (2) seal cover cap is contained in on the lid getting thing hole (11) (1), and gets thing hole (11) described in sealing;
Pulling-on piece (22) is folded on described sealed membrane body (21);
Described pulling-on piece (22) is bondd by described rubberised layer (3) and described sealed membrane body (21).
9. the manufacture method of Easy tearing lid according to claim 8, is characterized in that: described rubberised layer (3) area occupied is less than the area of described pulling-on piece (22).
10. the manufacture method of Easy tearing lid according to claim 8 or claim 9, it is characterized in that: described hot sealing layer adopts heat-seal adhesive to be formed, and when adopting heat-seal adhesive to form described hot sealing layer, first heat-seal adhesive is coated on the inside face of described aluminium foil, carry out drying process again, to form hot sealing layer.
The manufacture method of 11. Easy tearing lids according to claim 10, is characterized in that: formed in the step of hot sealing layer on the described inside face first heat-seal adhesive being coated in described aluminium foil, application rate is no more than 50 ms/min; In withering step, baking temperature is 100-250 DEG C.
The manufacture method of 12. Easy tearing lids according to claim 8 or claim 9, it is characterized in that: adopt PE film to form described hot sealing layer, when adopting PE film to form described hot sealing layer, first at the inside face application of adhesive of described aluminium foil, carry out drying process again, then the hot pressing of PE film is compounded in described aluminium foil to scribble in the one side of adhesives, then the aluminium foil being compounded with PE film is placed on curing chamber carries out slaking, to form hot sealing layer.
The manufacture method of 13. Easy tearing lids according to claim 12, is characterized in that:
In the step of drying process, by the aluminium foil being coated with adhesives with the speed being no more than 50 ms/min without a break successively through 50-60 DEG C, 60-70 DEG C, 70-80 DEG C three sections of baking ovens;
The hot pressing of PE film be compounded in the step that described aluminium foil scribbles in the one side of adhesives, hot pressing temperature is 50-70 DEG C;
Carry out in the step of slaking the aluminium foil being compounded with PE film being placed on curing chamber, the temperature of curing chamber is 50-55 DEG C, curing time >=72h.
The manufacture method of 14. Easy tearing lids according to Claim 8 according to any one of-13, it is characterized in that: formed in the step of gloss oil layer on the outside face of aluminium foil, upper ray velocity is no more than 50 ms/min, and carries out drying process in upper photoreduction process, and the temperature of dry process is 100-250 DEG C.
The manufacture method of 15. Easy tearing lids according to Claim 8 according to any one of-14, is characterized in that: also comprise the step forming described lid (1), be specially:
Subpunch swaging becomes lid element body;
By downward for the outer rim of described lid element body rounding limit, make the outer rim of described lid element body forms groove;
Injecting glue in described groove;
Become to get thing hole (11) in lid element body upper punch swaging;
The process of rounding limit is carried out to described thing hole (11) of getting.
The manufacture method of 16. Easy tearing lids according to Claim 8 according to any one of-15, it is characterized in that: described sealed membrane (2) seal cover cap is being contained in on the lid getting thing hole (1), and get in the step of thing hole (11) described in sealing, adopt the mode of heat-sealing, the sealing temperatures of heat-sealing is 180-250 DEG C, and sealing time is 1-2 second.
The manufacture method of 17. Easy tearing lids according to Claim 8 according to any one of-16, it is characterized in that: described sealed membrane (2) seal cover cap is contained in on the lid getting thing hole (11) (1), and before getting the step of thing hole (11) described in sealing, first carry out sealing between sealed membrane (2) and described lid (1) and locate.
The manufacture method of 18. Easy tearing lids according to Claim 8 according to any one of-17, it is characterized in that: after pulling-on piece (22) being folded to described sealed membrane body (21) and being upper, embossed is carried out to described sealed membrane body (21) and described pulling-on piece (22).
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201510496768.7A CN105173384A (en) | 2015-08-13 | 2015-08-13 | Cover easy to tear and manufacturing method thereof |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN201510496768.7A CN105173384A (en) | 2015-08-13 | 2015-08-13 | Cover easy to tear and manufacturing method thereof |
Publications (1)
Publication Number | Publication Date |
---|---|
CN105173384A true CN105173384A (en) | 2015-12-23 |
Family
ID=54895959
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CN201510496768.7A Pending CN105173384A (en) | 2015-08-13 | 2015-08-13 | Cover easy to tear and manufacturing method thereof |
Country Status (1)
Country | Link |
---|---|
CN (1) | CN105173384A (en) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN106180462A (en) * | 2016-07-15 | 2016-12-07 | 东莞市满贯包装有限公司 | Preparation method of large-diameter packaging tin and product thereof |
CN107416337A (en) * | 2017-07-25 | 2017-12-01 | 奥瑞金包装股份有限公司 | The processing method of Easy tearing lid |
CN108058908A (en) * | 2016-11-08 | 2018-05-22 | 内蒙古伊利实业集团股份有限公司 | A kind of packing jar sealing cover |
CN109018600A (en) * | 2018-10-18 | 2018-12-18 | 湖州金洁实业有限公司 | A kind of high temperature resistant aluminium foil Easy tearing lid |
CN110436050A (en) * | 2019-08-28 | 2019-11-12 | 浙江金石包装有限公司 | A kind of Easy tearing lid |
Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101665174A (en) * | 2009-10-21 | 2010-03-10 | 浙江金石包装有限公司 | Hot melt adhesive aluminum foil sealing film and manufacturing method thereof |
KR101207759B1 (en) * | 2005-10-19 | 2012-12-03 | 도요 세이칸 가부시키가이샤 | Easy open lid |
CN103274121A (en) * | 2013-06-07 | 2013-09-04 | 浙江金石包装有限公司 | Easy-to-tear aluminum foil cover and preparation method thereof |
CN204548749U (en) * | 2014-12-09 | 2015-08-12 | 广州番禺美特包装有限公司 | A kind of pulling-on piece bonded type Easy tearing lid structure |
CN204979718U (en) * | 2015-08-13 | 2016-01-20 | 浙江金石包装有限公司 | Cap easy to tear |
-
2015
- 2015-08-13 CN CN201510496768.7A patent/CN105173384A/en active Pending
Patent Citations (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
KR101207759B1 (en) * | 2005-10-19 | 2012-12-03 | 도요 세이칸 가부시키가이샤 | Easy open lid |
CN101665174A (en) * | 2009-10-21 | 2010-03-10 | 浙江金石包装有限公司 | Hot melt adhesive aluminum foil sealing film and manufacturing method thereof |
CN103274121A (en) * | 2013-06-07 | 2013-09-04 | 浙江金石包装有限公司 | Easy-to-tear aluminum foil cover and preparation method thereof |
CN204548749U (en) * | 2014-12-09 | 2015-08-12 | 广州番禺美特包装有限公司 | A kind of pulling-on piece bonded type Easy tearing lid structure |
CN204979718U (en) * | 2015-08-13 | 2016-01-20 | 浙江金石包装有限公司 | Cap easy to tear |
Cited By (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN106180462A (en) * | 2016-07-15 | 2016-12-07 | 东莞市满贯包装有限公司 | Preparation method of large-diameter packaging tin and product thereof |
CN106180462B (en) * | 2016-07-15 | 2018-06-01 | 东莞市满贯包装有限公司 | Preparation method of large-diameter packaging tin and product thereof |
CN108058908A (en) * | 2016-11-08 | 2018-05-22 | 内蒙古伊利实业集团股份有限公司 | A kind of packing jar sealing cover |
CN107416337A (en) * | 2017-07-25 | 2017-12-01 | 奥瑞金包装股份有限公司 | The processing method of Easy tearing lid |
CN107416337B (en) * | 2017-07-25 | 2020-04-14 | 奥瑞金科技股份有限公司 | Processing method of easy-to-tear cover |
CN109018600A (en) * | 2018-10-18 | 2018-12-18 | 湖州金洁实业有限公司 | A kind of high temperature resistant aluminium foil Easy tearing lid |
CN110436050A (en) * | 2019-08-28 | 2019-11-12 | 浙江金石包装有限公司 | A kind of Easy tearing lid |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN105173384A (en) | Cover easy to tear and manufacturing method thereof | |
JP6406553B2 (en) | Container sealed body with excellent heat resistance, openability and airtightness | |
US11124332B2 (en) | Ring-peel-seal liner | |
AU2018254160B2 (en) | Two-side adherable high-frequency induction heating container sealing member, compact cosmetic container having tamper function with same applied thereto, and flip cap container having temper function with same applied thereto | |
TW201823117A (en) | Easy-to-tear can for film covering foods | |
CN204979718U (en) | Cap easy to tear | |
JP6463058B2 (en) | Resealable sealed container | |
RU2018119312A (en) | RE-SEALED CONTAINER CONTAINING INSERT AND METHOD OF MANUFACTURE | |
CA3102898A1 (en) | Metallic can end | |
JP2000191021A (en) | Inner seal | |
US20200180835A1 (en) | Lidded container | |
JP6299257B2 (en) | Opening mechanism of easily openable containers | |
TWM592823U (en) | Container sealing film | |
CN221164116U (en) | Sealing gasket with hidden aluminum foil layer and pull lugs | |
EP1938951A2 (en) | Food container | |
KR20140134129A (en) | Laminate structure for container sealing | |
CN214524981U (en) | But PP drenches membrane paper container for microwave | |
JP5845031B2 (en) | Manufacturing method of heat seal can | |
JP2016088622A (en) | Can top and can including the same | |
JP5008501B2 (en) | Blister pack manufacturing method | |
JPS6025390Y2 (en) | tape seal lid | |
JPH01167073A (en) | Hermetically sealed container and its manufacturing | |
JP4727289B2 (en) | Cup-shaped container with a sealing member bonded | |
JPS6242897Y2 (en) | ||
JPS6144989Y2 (en) |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
C06 | Publication | ||
PB01 | Publication | ||
C10 | Entry into substantive examination | ||
SE01 | Entry into force of request for substantive examination | ||
RJ01 | Rejection of invention patent application after publication |
Application publication date: 20151223 |
|
RJ01 | Rejection of invention patent application after publication |