CN104803389A CN201510138510.XA CN201510138510A CN104803389A CN 104803389 A CN104803389 A CN 104803389A CN 201510138510 A CN201510138510 A CN 201510138510A CN 104803389 A CN104803389 A CN 104803389A
Authority
CN
China
Prior art keywords
diatomite
drying
water
rinsing
active agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510138510.XA
Other languages
Chinese (zh)
Inventor
刘来生
刘岩
刘文生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Liaoning Zhong Yuan High-Tech Co Ltd
Original Assignee
Liaoning Zhong Yuan High-Tech Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Liaoning Zhong Yuan High-Tech Co Ltd filed Critical Liaoning Zhong Yuan High-Tech Co Ltd
Priority to CN201510138510.XA priority Critical patent/CN104803389A/en
Publication of CN104803389A publication Critical patent/CN104803389A/en
Pending legal-status Critical Current

Links

Landscapes

  • Separation Of Solids By Using Liquids Or Pneumatic Power (AREA)

Abstract

The invention provides a purification method of diatomite. The method comprises procedures of raw ore crushing, screening, pulping, separation, rinsing, centrifugal spin-drying and drying. The diatomite prepared with the method is high in grade, pure and wide in application range and contains few impurities, and the method is applicable to production of the pure diatomite.

Description

A kind of Purification of Diatomite method
Technical field
The present invention is to provide a kind of Purification of Diatomite method of building materials and chemical industry and food processing field.
Background technology
Diatomite is diatom fossils weathered material in time immemorial, is widely used at building materials and chemical industry and food processing field.Usual diatomite is earthy discrete particles, deposits existence in mineral deposit mode, mineralizing process it, be mixed with the mineral materials such as sandstone, montmorillonite and illite, exist as impurity.Obtain clean diatomite, just need to remove the impurity be mixed with in diatomite.The method of usual employing hand picking, or the method that water conservancy is separated, but also can be mixed with impurity in the diatomite processed, therefore from grade, desirable technical requirements and quality can not be reached.
Summary of the invention
In order to by diatomite purifying, the present invention proposes a kind of Purification of Diatomite method.The method is by raw ore pulverizing, screening, slurrying, separation, rinsing, centrifuge dripping and baking operation.Solve the technical problem of Purification of Diatomite.
The scheme that technical solution problem of the present invention adopts is:
1, raw ore is pulverized: be crushed into Powdered by pulverizer by diatomite original ore.
2, sieve: pulverous diatomite is sieved through vibratory screening apparatus, abandons macrobead, form diatomite powder mix.
3, slurrying: be placed in pond by diatomite powder mix, adds water 5 times, is added with the hydrochloric acid of 1%, stirs simultaneously in water, after stirring, leaves standstill 30 minutes.
4, be separated: incline and upper strata bentonite slurry, take out middle level diatomite mud, abandon lower sediment thing.
5, rinsing: after separation circuit completes, continues in pond, add the water containing tensio-active agent, tensio-active agent add-on 1%, after stirring, settlement treatment 30 minutes.
6, centrifuge dripping: the diatom soil paste through rinsing is joined in whizzer, throws away attached water.
7, drying: the diatomite through drying is put in dryer, drying, then taking out from dryer, pack after naturally cooling, become finished product purified silicious earth.
Positively effect, the diatomite prepared by the inventive method is of high grade, and impurity is few, pure, wide application.Suitable to producing the application of pure diatomite.
Embodiment
1, raw ore is pulverized: be crushed into Powdered by pulverizer by diatomite original ore.
2, sieve: pulverous diatomite is sieved through vibratory screening apparatus, abandons macrobead, form diatomite powder mix.
3, slurrying: be placed in pond by diatomite powder mix, adds water 5 times, is added with the hydrochloric acid of 1%, stirs simultaneously in water, after stirring, leaves standstill 30 minutes.
4, be separated: incline and upper strata bentonite slurry, take out middle level diatomite mud, abandon lower sediment thing.
5, rinsing: after separation circuit completes, continues in pond, add the water containing tensio-active agent, tensio-active agent add-on 1%, after stirring, settlement treatment 30 minutes.
6, centrifuge dripping: the diatom soil paste through rinsing is joined in whizzer, throws away attached water.
7, drying: the diatomite through drying is put in dryer, drying, then taking out from dryer, pack after naturally cooling, become finished product purified silicious earth.
Know-why:
In pulping process, add hydrochloric acid water, the neutralization of alkaline matter can be conducive to, make impurity be easy to be separated.
In rinsing process, add tensio-active agent, diatomite can be made to clean, be conducive to being separated.
Because diatomite is different from other impurity proportion, so disperseed in water by the diatomite containing impurity, easily produce layering, thus discard impurity, retain diatomite layer slurry, be conducive to the physical sepn of diatomite and impurity.
Diatomite quality through purifying is clean, and color is pure white, good dispersity, is beneficial to application.

Claims (1)

1. a Purification of Diatomite method, raw ore is pulverized: be crushed into Powdered by pulverizer by diatomite original ore; Screening: sieved through vibratory screening apparatus by pulverous diatomite, abandon macrobead, forms diatomite powder mix; It is characterized in that:
Through operation:
Slurrying: be placed in pond by diatomite powder mix, adds water 5 times, is added with the hydrochloric acid of 1%, stirs simultaneously in water, after stirring, leaves standstill 30 minutes;
Be separated: incline and upper strata bentonite slurry, take out middle level diatomite mud, abandon lower sediment thing;
Rinsing: after separation circuit completes, continues in pond, add the water containing tensio-active agent, tensio-active agent add-on 1%, after stirring, settlement treatment 30 minutes;
Centrifuge dripping: the diatom soil paste through rinsing is joined in whizzer, throws away attached water;
Drying: the diatomite through drying is put in dryer, drying, then taking out from dryer, pack after naturally cooling, become finished product purified silicious earth.
CN201510138510.XA 2015-03-27 2015-03-27 Purification method of diatomite Pending CN104803389A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201510138510.XA CN104803389A (en) 2015-03-27 2015-03-27 Purification method of diatomite

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201510138510.XA CN104803389A (en) 2015-03-27 2015-03-27 Purification method of diatomite

Publications (1)

Publication Number Publication Date
CN104803389A true CN104803389A (en) 2015-07-29

Family

ID=53688663

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201510138510.XA Pending CN104803389A (en) 2015-03-27 2015-03-27 Purification method of diatomite

Country Status (1)

Country Link
CN (1) CN104803389A (en)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106975563A (en) * 2017-05-17 2017-07-25 上海圣地亚水务发展有限公司 Diatom ore deposit unhurried current normal temperature of washing the sand selects algae method
CN109192352A (en) * 2018-09-14 2019-01-11 天津理工大学 A method of improving curing type copper conductor slurry electrical property
CN109536738A (en) * 2018-12-14 2019-03-29 湘潭大学 A kind of method of lead bullion cream removal of impurities
CN114570212A (en) * 2022-03-16 2022-06-03 苏州盛虹环保科技有限公司 Preparation and application method of membrane pollution inhibitor for membrane bioreactor

Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1044233A (en) * 1988-09-30 1990-08-01 广西化工研究所 The method for preparing filter aid with diatomite
US7448564B2 (en) * 2005-08-04 2008-11-11 New Dimension Crushers, Llc Portable apparatus for crushing rock and other hard material and related method

Patent Citations (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1044233A (en) * 1988-09-30 1990-08-01 广西化工研究所 The method for preparing filter aid with diatomite
US7448564B2 (en) * 2005-08-04 2008-11-11 New Dimension Crushers, Llc Portable apparatus for crushing rock and other hard material and related method

Non-Patent Citations (1)

* Cited by examiner, † Cited by third party
Title
袁鹏: "硅藻土的提纯及其表面羟基、酸位研究", 《中国优秀博士论文数据库》 *

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106975563A (en) * 2017-05-17 2017-07-25 上海圣地亚水务发展有限公司 Diatom ore deposit unhurried current normal temperature of washing the sand selects algae method
CN106975563B (en) * 2017-05-17 2019-09-27 上海圣地亚水务发展有限公司 Diatom mine unhurried current room temperature of washing the sand selects algae method
CN109192352A (en) * 2018-09-14 2019-01-11 天津理工大学 A method of improving curing type copper conductor slurry electrical property
CN109536738A (en) * 2018-12-14 2019-03-29 湘潭大学 A kind of method of lead bullion cream removal of impurities
CN114570212A (en) * 2022-03-16 2022-06-03 苏州盛虹环保科技有限公司 Preparation and application method of membrane pollution inhibitor for membrane bioreactor

Similar Documents

Publication Publication Date Title
CN106000622B (en) A kind of color of quartzite production glass sand-magnetic separation joint dressing method
CN102205972B (en) Modification method of attapulgite
CN104925823B (en) A kind of purifying technique of hematite-type potassium feldspar emery dust
CN104803389A (en) Purification method of diatomite
CN104261361A (en) Washing and direct flotation method of low-grade refractory argillaceous phosphorite
CN111994938B (en) Method for preparing calcium sulfate whisker from calcium carbide slag modified phosphogypsum
CN107805043B (en) Method for preparing kaolin for medium-high grade ceramics from fine tailings and poor-quality kaolin
CN109250725A (en) It is a kind of to refine montmorillonite production technology using bentonite
CN102127568A (en) Method for removing impurities from cassava raw material
CN106542534A (en) A kind of method of impurity natrium in de-sodium agent removing afwillite
CN104973605A (en) Purification method of crude diatomite
CN102515881B (en) Process for preparing potash magnesium sulphate fertilizer by muddy potassium mixed salt mineral
CN110357572A (en) A kind of kaolin intelligence wet powder-making method for ceramic raw material
CN104844021B (en) The preparation method and device of lime cream
CN108910905A (en) A kind of the ultrasound centrifugation purification and sodium base method of low-grade bentonite
CN205099372U (en) Powder desalinization of soil by flooding or leaching apparatus for producing
CN103011230B (en) Low-cost method for preparing nano calcium sulfate
CN106745014A (en) A kind of method of purification of low taste sepiolite
CN103373844A (en) Method for comprehensive utilization of resources in exploitation of weathered granite mine
CN101817533B (en) Preparation method of electronic-level crystalline silicon powder
CN110357470B (en) Process method for removing blue illite particles in quartz sand through high-pressure acid leaching
CN107934970A (en) One kind purifies diatomaceous method from raw ore
CN108069539A (en) A kind of method that waste mud recycles in Production of Ceramics
KR20190115873A (en) Manufacturing method of alkarine mineral water
CN106492995A (en) A kind of preparation method of barite mineral collector

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
EXSB Decision made by sipo to initiate substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication

Application publication date: 20150729

RJ01 Rejection of invention patent application after publication