The effect of processing parameters (rotation speed and traverse speed) on the corrosion behaviour of friction stir processed high strength precipitation hardenable AA 2219-T87 alloy was investigated. The results indicate that the rotation speed has a major influence in …
- 238000005260 corrosion 0 title abstract description 65
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C1/00—Making alloys
- C22C1/02—Making alloys by melting
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C21/00—Alloys based on aluminium
- C22C21/06—Alloys based on aluminium with magnesium as the next major constituent
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C21/00—Alloys based on aluminium
- C22C21/10—Alloys based on aluminium with zinc as the next major constituent
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22F—CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
- C22F1/00—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
- C22F1/04—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of aluminium or alloys based thereon
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22F—CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
- C22F1/00—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
- C22F1/10—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of nickel or cobalt or alloys based thereon
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C19/00—Alloys based on nickel or cobalt
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C14/00—Alloys based on titanium
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C38/00—Ferrous alloys, e.g. steel alloys
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C23/00—Alloys based on magnesium
- C22C23/02—Alloys based on magnesium with aluminium as the next major constituent
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Surekha et al. | Effect of processing parameters on the corrosion behaviour of friction stir processed AA 2219 aluminum alloy | |
Surekha et al. | Microstructural characterization and corrosion behavior of multipass friction stir processed AA2219 aluminium alloy | |
Kumar et al. | Microstructure, mechanical and corrosion behavior of high strength AA7075 aluminium alloy friction stir welds–Effect of post weld heat treatment | |
Gharavi et al. | Corrosion behavior of Al6061 alloy weldment produced by friction stir welding process | |
Deng et al. | Effects of Sc and Zr microalloying additions and aging time at 120 C on the corrosion behaviour of an Al–Zn–Mg alloy | |
Wadeson et al. | Corrosion behaviour of friction stir welded AA7108 T79 aluminium alloy | |
Jiang et al. | Microstructure evolution and mechanical properties of 2060 Al-Li alloy via friction stir additive manufacturing | |
Dong et al. | Effects of Cu content on microstructure and properties of super-high-strength Al-9.3 Zn-2.4 Mg-xCu-Zr alloy | |
El-Danaf et al. | Microstructure and mechanical properties of friction stir welded 6082 AA in as welded and post weld heat treated conditions | |
Wang et al. | Corrosion behavior of spray formed 7055 aluminum alloy joint welded by underwater friction stir welding | |
El-Menshawy et al. | Effect of aging time at low aging temperatures on the corrosion of aluminum alloy 6061 | |
Selvamani | Microstructure and stress corrosion behaviour of CMT welded AA6061 T-6 aluminium alloy joints | |
Surekha et al. | Comparison of corrosion behaviour of friction stir processed and laser melted AA 2219 aluminium alloy | |
Nascimento et al. | Microstructural modification and ductility enhancement of surfaces modified by FSP in aluminium alloys | |
Peng et al. | Synergetic effects of Sc and Zr microalloying and heat treatment on mechanical properties and exfoliation corrosion behavior of Al-Mg-Mn alloys | |
Zhang et al. | Comparison of microstructure and mechanical properties of TIG and laser welding joints of a new Al–Zn–Mg–Cu alloy | |
Gharavi et al. | Corrosion evaluation of friction stir welded lap joints of AA6061-T6 aluminum alloy | |
Sajadifar et al. | On the effect of quenching on postweld heat treatment of friction-stir-welded aluminum 7075 alloy | |
Liu et al. | Effects of heterogeneity and coarse secondary phases on mechanical properties of 7050-T7451 aluminum alloy friction stir welding joint | |
Sun et al. | Effect of Sc content on microstructure and properties of Al-Zn-Mg-Cu-Zr alloy | |
Xu et al. | Microstructure evolution and stress corrosion cracking sensitivity of friction stir welded high strength AA7085 joint | |
Mehri et al. | The effects of friction stir welding on microstructure and formability of 7075-T6 sheet | |
Zhang et al. | Microstructure characteristics and corrosion behavior of refill friction stir spot welded 7050 aluminum alloy | |
Cao et al. | Effects of Cu addition on the microstructure and properties of the Al–Mn–Fe–Si alloy | |
Satyanarayana et al. | Microstructure, mechanical properties and corrosion behavior of friction stir processed AA2014 alloy |