Snippet
In this study, the susceptibility to stress corrosion cracking (SCC) of laser-welded NiTi wires in Hanks' solution at 37.5° C was studied by the slow strain-rate test (SSRT) at open-circuit potential and at different applied anodic potentials. The weldment shows high susceptibility …
- 238000005260 corrosion 0 title abstract description 87
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22F—CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
- C22F1/00—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
- C22F1/10—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of nickel or cobalt or alloys based thereon
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C19/00—Alloys based on nickel or cobalt
- C22C19/03—Alloys based on nickel or cobalt based on nickel
- C22C19/05—Alloys based on nickel or cobalt based on nickel with chromium
- C22C19/051—Alloys based on nickel or cobalt based on nickel with chromium and Mo or W
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C19/00—Alloys based on nickel or cobalt
- C22C19/07—Alloys based on nickel or cobalt based on cobalt
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Chan et al. | Susceptibility to stress corrosion cracking of NiTi laser weldment in Hanks’ solution | |
Oliveira et al. | Dissimilar laser welding of superelastic NiTi and CuAlMn shape memory alloys | |
Mehrpouya et al. | Laser welding of NiTi shape memory alloy: A review | |
Quazi et al. | Current research and development status of dissimilar materials laser welding of titanium and its alloys | |
Zoeram et al. | Laser welding of Ti–6Al–4V to Nitinol | |
Oliveira et al. | Laser welding of Cu-Al-Be shape memory alloys: Microstructure and mechanical properties | |
Miranda et al. | Fiber laser welding of NiTi to Ti-6Al-4V | |
Zhou et al. | Surface and property characterization of laser polished Ti6Al4V | |
Park et al. | Corrosion behavior of biodegradable Mg-based alloys via femtosecond laser surface melting | |
Saravanan et al. | Pulsed Nd: YAG laser welding and subsequent post-weld heat treatment on super duplex stainless steel | |
Mehrpouya et al. | Laser welding of NiTi shape memory sheets using a diode laser | |
Damodaram et al. | Effect of post-weld heat treatments on microstructure and mechanical properties of friction welded alloy 718 joints | |
JP6245805B2 (en) | Shape memory material processing method and shape memory material processing apparatus | |
Yan et al. | Corrosion behavior of a laser-welded NiTi shape memory alloy | |
Zeng et al. | The role of microstructure on corrosion fatigue behavior of thick-plate Ti–6Al–4V joint via vacuum electron beam welding | |
Deepan Bharathi Kannan et al. | A review of similar and dissimilar micro-joining of nitinol | |
Mirshekari et al. | Effect of post weld heat treatment on mechanical and corrosion behaviors of NiTi and stainless steel laser-welded wires | |
Dong et al. | Microstructural characterization of laser micro-welded Nitinol wires | |
Li et al. | Impact of microstructure evolution on the corrosion behaviour of the Ti–6Al–4V alloy welded joint using high-frequency pulse wave laser | |
Razavi | Laser beam welding of Waspaloy: characterization and corrosion behavior evaluation | |
Chakraborty et al. | A comparative study of surface characterization and corrosion performance properties of laser surface modified biomedical grade nitinol | |
Chan et al. | Susceptibility to environmentally induced cracking of laser-welded NiTi wires in Hanks’ solution at open-circuit potential | |
Chan et al. | Parameter Optimization for Laser Welding of NiTi Wires by the Taguchi Method. | |
Shamsolhodaei et al. | Superelasticity preservation in dissimilar joint of NiTi shape memory alloy to biomedical PtIr | |
Mirshekari et al. | Microstructure, cyclic deformation and corrosion behavior of laser welded NiTi shape memory wires |