Wang et al., 1988 - Google Patents
Study on Improving the Thermo-Fatigue Resistance of HM 3 SteelWang et al., 1988
- Document ID
- 16214616435271942515
- Author
- Wang L
- Li P
- Publication year
- Publication venue
- Heat Treat. Met.(China)
External Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C21—METALLURGY OF IRON
- C21D—MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHER TREATMENTS
- C21D1/00—General methods or devices for heat treatments, e.g. annealing, hardening, quenching, tempering
- C21D1/06—Surface hardening
- C21D1/09—Surface hardening by direct application of electrical or wave energy; by particle radiation
- C21D1/10—Surface hardening by direct application of electrical or wave energy; by particle radiation by electric induction
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2232971A1 (en) | Method for treating wood at the glass transition temperature thereof | |
Wang et al. | Study on Improving the Thermo-Fatigue Resistance of HM 3 Steel | |
Kern | Distortion and Cracking. III.--How to Control Cracking | |
Radcliffe | Gas Quenching in Vacuum Furnaces--a Review of Fundamentals | |
Huang | Tempering Equations for 50 Types of Common Steels | |
Wang et al. | Influence of Quenching Temperature and Grain Size on Hardenability of 27 SiMnB Steel | |
Su | Control of Effective Case Depth for Carburized Parts | |
Li | Study on the High Temperature Thermomechanical Treating Process of 45 Steel | |
Shen | The Toughness and Toughening of Steel 35 Cr 3 W 2 V | |
Lou et al. | Study on the Relationship Among Heating Temperature, Soaking Time, and Carbonitrided Depth | |
Nakonieczny et al. | On possibility to form fatigue properties of 4140 steel by nitriding and high-temperature tempering | |
Wu et al. | The Intercritical Heat Treatment During Continuous Heating for the Medium-Manganese Cast-Steels | |
Cheng et al. | Analysis of Quenching Cracks of Machine Tool-Piston Under Supersonic Frequency Induction Hardening | |
Li | The Design and Application of Quenching Bath for Circulating Spray Quenching | |
Lu et al. | Boro-Carbonitriding for Improving the Nature of Boriding Layer | |
Wilhelmi et al. | Nitriding by Pulsed Glow Discharge | |
Haga | Heat Treat Basics: Increasing Hardness or Strength; Processing Tool Steels | |
Kloos | Strength and Wear Properties of Inductive Surface Hardened Components | |
Leban | Important Points of Heat Treating Technology Taking Into Account Material Properties | |
Listemann | Martempering and Isothermal Bainitic Hardening for Low Distortion Heat Treatment in Modern Vacuum Furnaces | |
UA19205A (en) | StarWriterMETHOD FOR THERMAL TREATMENT OF RAPID STEEL | |
Xu | Intercritical Quenching of the 40 CrSi Steel Piston Crown | |
Matsumoto | Advice on Heat Treatment of Machine Steels | |
Young | Solving Quenching Cracking of 45 Steel | |
Tonini et al. | Vacuum Heat Treating: Practical Guidelines for Best Results |