Shui et al., 2023 - Google Patents
Corrosion mechanism and fatigue behavior of aluminum alloy with high silicon contentShui et al., 2023
- Document ID
- 668805030894133166
- Author
- Shui Y
- Liu J
- Huang W
- Zhao N
- Ren P
- Zhao C
- Publication year
- Publication venue
- Materials Chemistry and Physics
External Links
Snippet
The corrosion and corrosion-assisted fatigue life degradation behaviors of Al–8Si alloy is investigated. The test results show that galvanic cells are formed in the inter-dendrites due to high Si concentration, leading to pitting corrosion. The Al 2 Cu phase and the Si-rich phase …
- 238000005260 corrosion 0 title abstract description 223
Classifications
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22F—CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
- C22F1/00—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
- C22F1/04—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of aluminium or alloys based thereon
- C22F1/053—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of aluminium or alloys based thereon of alloys with zinc as the next major constituent
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22F—CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS
- C22F1/00—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working
- C22F1/10—Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working of nickel or cobalt or alloys based thereon
-
- C—CHEMISTRY; METALLURGY
- C22—METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
- C22C—ALLOYS
- C22C21/00—Alloys based on aluminium
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25D—PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25D5/00—Electroplating characterised by the process; Pretreatment or after-treatment of work-pieces
- C25D5/48—After-treatment of electroplated surfaces
Similar Documents
Publication | Publication Date | Title |
---|---|---|
Svenningsen et al. | Effect of low copper content and heat treatment on intergranular corrosion of model AlMgSi alloys | |
Kumar et al. | Microstructure, mechanical and corrosion behavior of high strength AA7075 aluminium alloy friction stir welds–Effect of post weld heat treatment | |
Liu et al. | Mechanism of low exfoliation corrosion resistance due to slow quenching in high strength aluminium alloy | |
ZHOU et al. | Influence of thermomechanical treatments on localized corrosion susceptibility and propagation mechanism of AA2099 Al–Li alloy | |
Svenningsen et al. | Effect of high temperature heat treatment on intergranular corrosion of AlMgSi (Cu) model alloy | |
Peng et al. | Synergetic effects of Sc and Zr microalloying and heat treatment on mechanical properties and exfoliation corrosion behavior of Al-Mg-Mn alloys | |
Xuehong et al. | Effect of interrupted ageing treatment on the mechanical properties and intergranular corrosion behavior of Al-Mg-Si alloys | |
Sun et al. | Microstructure, corrosion behaviour and thermal stability of AA 7150 after ultrasonic shot peening | |
Guo et al. | Evolution of microstructure, mechanical properties and corrosion behavior of Al-4Mg-2Zn-0.3 Ag (wt.%) alloy processed by T6 or thermomechanical treatment | |
Sun et al. | Effect of Sc content on microstructure and properties of Al-Zn-Mg-Cu-Zr alloy | |
Charalampidou et al. | Corrosion-induced mechanical properties degradation of Al-Cu-Li (2198-T351) aluminium alloy and the role of side-surface cracks | |
Liu et al. | Correlation between artificial aging and intergranular corrosion sensitivity of a new Al‐Cu‐Li alloy sheet | |
He et al. | Effect of Sn on microstructure and corrosion behaviors of Al-Mg-Si alloys | |
Zou et al. | Detailed characterizations of microstructure evolution, corrosion behavior and mechanical properties of refill friction stir spot welded 2219 aluminum alloy | |
Wang et al. | Effects of pre-stretching and aging treatments on microstructure, mechanical properties, and corrosion behavior of spray-formed Al-Li alloy 2195 | |
Araujo et al. | Microstructural, electrochemical and localized corrosion characterization of the AA2198-T851 alloy | |
Shui et al. | Corrosion mechanism and fatigue behavior of aluminum alloy with high silicon content | |
Lei et al. | Effects of solid solution temperature on the microstructure and properties of 6013 aluminum alloy | |
Wang et al. | Corrosion of Al-3.5 Cu-1.5 Mg–1Si alloy prepared by selective laser melting and heat treatment | |
Liu et al. | Effect of minor Ge addition on microstructure and localized corrosion behavior of Al-Zn-Mg alloy sheet | |
Duan et al. | Intergranular corrosion behavior of extruded 6005A alloy profile with different microstructures | |
ZHANG et al. | Effect of Cu content on intergranular corrosion and exfoliation corrosion susceptibility of Al− Zn− Mg−(Cu) alloys | |
Liang et al. | Corrosion behavior of Al-6.8 Zn-2.2 Mg-Sc-Zr alloy with high resistance to intergranular corrosion | |
Chen et al. | The effect of heat treatment on the microstructure and electrochemical corrosion behavior of multilayer AA6061 alloy fabricated by additive friction stir deposition | |
Wen et al. | The initial corrosion behavior of Al–Cu–Li bicrystals: effect of misorientation and precipitates |