TECHNICAL DATA SHEET

USP-EAGLE(GP 200-62)62%
Rigid, non-thixotropic, non-accelerated orthophthalic unsaturated polyester.
Delivery form : 62 % in (Styrene)

Specification:
Test Standard Unit Method
Non-volatiles 60-64 % ISO 3251
Viscosity, 25°C (Gardner-Holdt) Approx. I -- ASTM D1545
Viscosity, 25°C (Brookfield)* 200 - 300 mPa.s or cP ISO 2555
Acid value 25 max. mg KOH/g ISO 2114
Appearance Clear ------------ ------------
Gel time 22 - 28 Minutes
Using 0.25% Cobalt 6% +
Cure time 35 – 45 Minutes
1.5% MEKP 50% on 100
Peak Exothermic 150 - 180 °C grams of resin at 25°C

*Spindle 3 & RPM 60


Performance:
• Rigid films. • Non-accelerated.
• Good curing properties. • Non-thixotropic.
• Light color. • Medium viscosity.
Application:

• Glass fiber laminates for general-purpose applications.

Properties of cured cast resin at 25 °C


Test Test method Result
• Tensile strength (MPa) ISO/R 527 / ASTM D 638 Min. 65
• Tensile modulus (MPa) ISO/R 527 / ASTM D 638 Min. 3500
• Elongation at break ISO/R 527 / ASTM D 638 Min. 2.0
• Flexural strength (MPa) ISO 178 / ASTM D 790 Min 145
• Flexural modulus (MPa) ISO 178 / ASTM D 790 Min. 3500
• Barcol hardness ASTM D 2583 Min. 40
Compatibility:
USP-EAGLE (GP 200-62)62% should only be diluted with styrene monomer.
For cleaning of equipment (brushes etc.) Acetone is recommended
Compatibility with other resins:
The compatibility of USP-EAGLE (GP 200-62)62% with another resin should be checked prior to mixing production quantities.

Disclaimer: The use of unsaturated polyester resin can be dangerous if not used properly. Eagle Chemicals assumes no responsibility or liability for any damages whatsoever,
including but not limited to direct, indirect, incidental, consequential, or punitive damages, arising out of or in any way connected with the use or misuse of this product.
The user assumes all risks and liability associated with the use of this product. The user should read and understand all warnings and instructions before using this product.
Specifically, the properties of unsaturated polyester resins can be affected by temperature and formulation ingredients, such as dispersing agent, filler quality, and inhibitor
percent in styrene monomers. This can result in different results depending on the specific application, and the user should be aware of these risks before using the product.
In addition, unsaturated polyester resins are susceptible to gelling, which can occur when the resin is exposed to high temperatures or when the formulation ingredients are not
compatible. Gelling can make the resin unusable, and it can also be dangerous if it occurs during the storage process. So, we recommend the customer do a storage stability test
based on his own formulation at different temperatures to ensure product stability.

Review no:1/2023 Issue date:Oct,2023 Page 1/2


TECHNICAL DATA SHEET
USP-EAGLE(GP 200-62)62%
Rigid, non-thixotropic, non-accelerated orthophthalic unsaturated polyester.
Delivery form : 62 % in (Styrene)

Storage:

USP-EAGLE (GP 200-62)62% should be stored indoors in the original, unopened, and undamaged containers in a dry place
at storage temperatures between 5°C to 30°C. Exposure to sunlight should be avoided.

Stability:

Under the above-mentioned storage condition, the stability of USP-EAGLE (GP 200-62)62% will be 6 months ex-work.

The stability of USP-EAGLE (GP 200-62)62% pre-accelerated version will be 3 months only.

Disclaimer: The use of unsaturated polyester resin can be dangerous if not used properly. Eagle Chemicals assumes no responsibility or liability for any damages whatsoever,
including but not limited to direct, indirect, incidental, consequential, or punitive damages, arising out of or in any way connected with the use or misuse of this product.
The user assumes all risks and liability associated with the use of this product. The user should read and understand all warnings and instructions before using this product.
Specifically, the properties of unsaturated polyester resins can be affected by temperature and formulation ingredients, such as dispersing agent, filler quality, and inhibitor
percent in styrene monomers. This can result in different results depending on the specific application, and the user should be aware of these risks before using the product.
In addition, unsaturated polyester resins are susceptible to gelling, which can occur when the resin is exposed to high temperatures or when the formulation ingredients are not
compatible. Gelling can make the resin unusable, and it can also be dangerous if it occurs during the storage process. So, we recommend the customer do a storage stability test
based on his own formulation at different temperatures to ensure product stability.

Review no:1/2023 Issue date:Oct,2023 Page 2/2