Abstract

3D printing offers great potential for developing complex flexure mechanisms. Recently, thickness-correction factors (TCFs) were introduced to correct the thickness and stiffness deviations of powder-based metal 3D printed flexure hinges during design and analysis. However, the reasons for the different TCFs obtained in each study are not clear, resulting in a limited value of these TCFs for future design and fabrication. Herein, the influence of the porous layer of 3D printed flexure hinges on the hinge thickness is investigated. Samples of parallelogram flexure mechanisms (PFMs) were 3D printed using selective laser melting (SLM) and 316L stainless steel powder. A 3D manufacturing error analysis was completed for each PFM sample via 3D scanning, surface roughness measurement and morphological observation. The thickness of the porous layer of the flexure hinge was independent of the designed hinge thickness and remained close to the average powder particle diameter. The effective hinge thickness could be estimated by subtracting twice the value of the porous layer thickness from the designed value. Guidelines based on finite element analysis and stiffness experiments are proposed. The limitations of the presented method for evaluating the effective hinge thickness of flexure hinges 3D printed via SLM are also discussed.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Subscribe and save

Springer+ Basic
$34.99 /Month
  • Get 10 units per month
  • Download Article/Chapter or eBook
  • 1 Unit = 1 Article or 1 Chapter
  • Cancel anytime
Subscribe now

Buy Now

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Fig. 1
Fig. 2
Fig. 3
Fig. 4
Fig. 5
Fig. 6
Fig. 7
Fig. 8
Fig. 9
Fig. 10
Fig. 11

Similar content being viewed by others

References

Download references

Acknowledgements

This work was supported by the Scientific Research Foundation of Shantou University (No: NTF18002), National Key R&D Program of China (No: 2018YFB1701701) and Science and Technology Planning Project of Guangdong Province (No: 2017A050501061).

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Huaxian Wei.

Additional information

Publisher's Note

Springer Nature remains neutral with regard to jurisdictional claims in published maps and institutional affiliations.

Rights and permissions

Reprints and permissions

About this article

Check for updates. Verify currency and authenticity via CrossMark

Cite this article

Wei, H., Shirinzadeh, B., Niu, X. et al. Study of the hinge thickness deviation for a 316L parallelogram flexure mechanism fabricated via selective laser melting. J Intell Manuf 32, 1411–1420 (2021). https://doi.org/10.1007/s10845-020-01621-x

Download citation

  • Received:

  • Accepted:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s10845-020-01621-x

Keywords

Navigation