The speed of sound in any chemical element in the fluid phase has one temperature-dependent value. In the solid phase, different types of sound wave may be propagated, each with its own speed: among these types of wave are longitudinal (as in fluids), transversal, and (along a surface or plate) extensional.[1]
longitudinal, m/s | transversal, m/s | extensional, m/s | notes | |
---|---|---|---|---|
3 Li lithium | ||||
use | 6000 | 20 °C | ||
WEL | 6000 | |||
4 Be beryllium | ||||
use | 12890 | 8880 | 12870 | room temperature |
CRC | 12890 | 8880 | 12870 | |
WEL | 13000 | |||
5 B boron | ||||
use | 16200 | 20 °C | ||
WEL | 16200 | |||
6 C carbon | ||||
use | ||||
WEL | 18350 | |||
11 Na sodium | ||||
use | 3200 | 20 °C | ||
WEL | 3200 | |||
12 Mg magnesium | ||||
use | 5770 | 3050 | 4940 | room temperature, annealed |
CRC | 5770 | 3050 | 4940 | annealed |
WEL | 4602 | |||
13 Al aluminium | ||||
use | 6420 | 3040 | 5000 | room temperature, rolled |
CRC | 6420 | 3040 | 5000 | rolled |
WEL | 5100 | |||
14 Si silicon | ||||
use | 8433 | 5843 | ||
Cij | 8433 | 5843 | from C11=165.64 GPa, C44=79.51 GPa, ro1=2.329 g/cm3[2] | |
WEL | 2200 | 20 °C - note: probably wrong (see talk) | ||
19 K potassium | ||||
use | 2000 | 20 °C | ||
WEL | 2000 | |||
20 Ca calcium | ||||
use | 3810 | 20 °C | ||
WEL | 3810 | |||
22 Ti titanium | ||||
use | 6070 | 3125 | 5090 | room temperature |
CRC | 6070 | 3125 | 5090 | |
WEL | 4140 | |||
23 V vanadium | ||||
use | 4560 | 20 °C | ||
WEL | 4560 | |||
24 Cr chromium | ||||
use | 6608 | 4005 | 5940 | 20 °C |
WEL | 5940 | |||
25 Mn manganese | ||||
use | 5150 | 20 °C | ||
WEL | 5150 | |||
26 Fe iron | ||||
use | 5950 | 3240 | 5120 | room temperature, electrolytic |
CRC | 4994 | 2809 | 4480 | cast |
CRC | 5950 | 3240 | 5120 | electrolytic |
CRC | 5960 | 3240 | 5200 | Armco |
WEL | 4910 | |||
27 Co cobalt | ||||
use | 4720 | 20 °C | ||
WEL | 4720 | |||
28 Ni nickel | ||||
use | 6040 | 3000 | 4900 | room temperature |
CRC | 6040 | 3000 | 4900 | |
WEL | 4970 | |||
29 Cu copper | ||||
use | 4760 | 2325 | 3810 | room temperature, annealed |
CRC | 4760 | 2325 | 3810 | annealed |
CRC | 5010 | 2270 | 3750 | rolled |
WEL | 3570 | |||
30 Zn zinc | ||||
use | 4210 | 2440 | 3850 | room temperature, rolled |
CRC | 4210 | 2440 | 3850 | rolled |
WEL | 3700 | |||
31 Ga gallium | ||||
use | 2740 | 20 °C | ||
WEL | 2740 | |||
32 Ge germanium | ||||
use | 5400 | 20 °C | ||
WEL | 5400 | |||
34 Se selenium | ||||
use | 3350 | 20 °C | ||
WEL | 3350 | |||
37 Rb rubidium | ||||
use | 1300 | 20 °C | ||
WEL | 1300 | |||
39 Y yttrium | ||||
use | 3300 | 20 °C | ||
WEL | 3300 | |||
40 Zr zirconium | ||||
use | 3800 | 20 °C | ||
WEL | 3800 | |||
41 Nb niobium | ||||
use | 3480 | 20 °C | ||
WEL | 3480 | |||
42 Mo molybdenum | ||||
use | 6250 | 3350 | 5400 | room temperature |
CRC | 6250 | 3350 | 5400 | |
WEL | 6190 | |||
44 Ru ruthenium | ||||
use | 5970 | 20 °C | ||
WEL | 5970 | |||
45 Rh rhodium | ||||
use | 4700 | 20 °C | ||
WEL | 4700 | |||
46 Pd palladium | ||||
use | 3070 | 20 °C | ||
WEL | 3070 | |||
47 Ag silver | ||||
use | 3650 | 1610 | 2680 | room temperature |
CRC | 3650 | 1610 | 2680 | |
WEL | 2600 | |||
48 Cd cadmium | ||||
use | 2310 | 20 °C | ||
WEL | 2310 | |||
49 In indium | ||||
use | 1215 | 20 °C | ||
WEL | 1215 | |||
50 Sn tin | ||||
use | 3320 | 1670 | 2730 | room temperature, rolled |
CRC | 3320 | 1670 | 2730 | rolled |
WEL | 2500 | |||
51 Sb antimony | ||||
use | 3420 | 20 °C | ||
WEL | 3420 | |||
52 Te tellurium | ||||
use | 2610 | 20 °C | ||
WEL | 2610 | |||
56 Ba barium | ||||
use | 1620 | 20 °C | ||
WEL | 1620 | |||
57 La lanthanum | ||||
use | 2475 | 20 °C | ||
WEL | 2475 | |||
58 Ce cerium | ||||
use | 2100 | 20 °C | ||
WEL | 2100 | |||
59 Pr praseodymium | ||||
use | 2280 | 20 °C | ||
WEL | 2280 | |||
60 Nd neodymium | ||||
use | 2330 | 20 °C | ||
WEL | 2330 | |||
62 Sm samarium | ||||
use | 2130 | 20 °C | ||
WEL | 2130 | |||
64 Gd gadolinium | ||||
use | 2680 | 20 °C | ||
WEL | 2680 | |||
65 Tb terbium | ||||
use | 2620 | 20 °C | ||
WEL | 2620 | |||
66 Dy dysprosium | ||||
use | 2710 | 20 °C | ||
WEL | 2710 | |||
67 Ho holmium | ||||
use | 2760 | 20 °C | ||
WEL | 2760 | |||
68 Er erbium | ||||
use | 2830 | 20 °C | ||
WEL | 2830 | |||
70 Yb ytterbium | ||||
use | 1590 | 20 °C | ||
WEL | 1590 | |||
72 Hf hafnium | ||||
use | 3010 | 20 °C | ||
WEL | 3010 | |||
73 Ta tantalum | ||||
use | 3400 | 20 °C | ||
WEL | 3400 | |||
74 W tungsten | ||||
use | 5220 | 2890 | 4620 | room temperature, annealed |
CRC | 5220 | 2890 | 4620 | annealed |
CRC | 5410 | 2640 | 4320 | drawn |
WEL | 5174 | |||
75 Re rhenium | ||||
use | 4700 | 20 °C | ||
WEL | 4700 | |||
76 Os osmium | ||||
use | 4940 | 20 °C | ||
WEL | 4940 | |||
77 Ir iridium | ||||
use | 4825 | 20 °C | ||
WEL | 4825 | |||
78 Pt platinum | ||||
use | 3830 | 1680 | 2800 | room temperature. Calculated using Wikipedia reported values for density (21450 kg/m3), Young's Modulus (167 GPa), and Poisson's ratio (0.38) |
CRC | 3260 | 1730 | 2800 | CRC cites American Institute of Physics Handbook (AIPH) table 3f-2 for this value, but in AIPH table 2f-6 there are elastic constants reported that yield 3700,1570, 2620 |
WEL | 2680 | |||
AIPH | 3700 | 1570 | 2620 | Table 2f-6. Calculated from Young's modulus of 147 GPa (lower than commonly accepted for Platinum), Poisson's ratio of 0.39, density of 21370 kg/m3 |
79 Au gold | ||||
use | 3240 | 1200 | 2030 | room temperature, hard-drawn |
CRC | 3240 | 1200 | 2030 | hard-drawn |
WEL | 1740 | |||
81 Tl thallium | ||||
use | 818 | 20 °C | ||
WEL | 818 | |||
82 Pb lead | ||||
use | 2160 | 700 | 1190 | room temperature, annealed |
CRC | 2160 | 700 | 1190 | annealed |
CRC | 1960 | 690 | 1210 | rolled |
WEL | 1260 | |||
83 Bi bismuth | ||||
use | 1790 | 20 °C | ||
WEL | 1790 | |||
90 Th thorium | ||||
use | 2490 | 20 °C | ||
WEL | 2490 | |||
92 U uranium | ||||
use | 3155 | 20 °C | ||
WEL | 3155 | |||
94 Pu plutonium | ||||
use | 2260 | 20 °C | ||
WEL | 2260 |
m/s | notes | |
---|---|---|
1 H hydrogen (gas) | ||
use | 1310 | 27 °C |
CRC | 1310 | 27 °C |
WEL | 1270 | |
Zuckerwar | 1270 | 20 °C, 1 atm |
CRC | 890 | deuterium, 0 °C |
1 H hydrogen (liquid) | ||
use | 1101 | −252.9 °C |
CRC | 1101 | −252.9 °C |
2 He helium (gas) | ||
use | 965 | 0 °C |
CRC | 965 | 0 °C |
Zuckerwar | 1007 | 20 °C, 1 atm |
WEL | 970 | |
2 He helium (liquid) | ||
use | 180 | −268.9 °C |
CRC | 180 | −268.9 °C |
7 N nitrogen (gas) | ||
use | 353 | 27 °C |
CRC | 353 | 27 °C |
Zuckerwar | 349 | 20 °C, 1 atm |
WEL | 333.6 | |
7 N nitrogen (liquid) | ||
use | 939 | −195.8 °C |
CRC | 939 | −195.8 °C |
8 O oxygen (gas) | ||
use | 330 | 27 °C |
CRC | 330 | 27 °C |
Zuckerwar | 326 | 20 °C, 1 atm |
WEL | 317.5 | |
8 O oxygen (liquid) | ||
use | 906 | −183.0 °C |
CRC | 906 | −183.0 °C |
10 Ne neon (gas) | ||
use | 435 | 0 °C |
CRC | 435 | 0 °C |
WEL | 936 (presumably for liquid?) | |
17 Cl chlorine (gas) | ||
use | 206 | 0 °C |
CRC | 206 | 0 °C |
WEL | 206 | |
18 Ar argon (gas) | ||
use | 323 | 27 °C |
CRC | 323 | 27 °C |
Zuckerwar | 319 | 20 °C, 1 atm |
WEL | 319 | |
18 Ar argon (liquid) | ||
use | 813 | −185.9 °C |
CRC | 813 | −185.9 °C |
36 Kr krypton (gas) | ||
use | 221 | 20 °C |
Zuckerwar | 221 | 20 °C, 1 atm |
talk | 220 ± 1, prelim. experimental value | 23 °C, 101.3 kPa |
36 Kr krypton (liquid) | ||
use | 1120 | |
88RAB | 1120 | |
WEL | 1120 | |
54 Xe xenon (gas) | ||
use | 178 | 20 °C, 1 atm |
Zuckerwar | 178 | 20 °C, 1 atm |
54 Xe xenon (liquid) | ||
use | 1090 | |
88RAB | 1090 | |
WEL | 1090 | |
80 Hg mercury (liquid) | ||
use | 1451.4 | 20 °C |
CR2 | 1460.8 | 0 °C |
CR2 | 1451.4 | 20 °C |
CRC | 1450 | 25 °C |
WEL | 1407 |
Seamless Wikipedia browsing. On steroids.
Every time you click a link to Wikipedia, Wiktionary or Wikiquote in your browser's search results, it will show the modern Wikiwand interface.
Wikiwand extension is a five stars, simple, with minimum permission required to keep your browsing private, safe and transparent.